Self-Compacting Concrete for the Durable Reinforced Foundations of the Calatrava Bridge in Venice

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Self-Compacting Concrete for the Durable Reinforced Foundations of the Calatrava Bridge in Venice

Author(s): Mario Collepardi, Silvia Collepardi, Ettore Menegaldo and Roberto Troli

Publication: Symposium Paper

Volume: 354

Issue:

Appears on pages(s): 187-192

Keywords: durability; limestone filler; self-compacting concrete; superplasticizer; viscosity modifier

DOI: 10.14359/51736072

Date: 7/1/2022

Abstract:
The present paper describes the building of the Fourth Bridge on the Grand Canal in Venice, designed by the Architect Santiago Calatrava. In particular, this paper is devoted to the laboratory and field tests to develop the composition of a self-compacting concrete (SCC) to be placed in the congested reinforced foundations of the Calatrava Bridge. To ensure a durable service life of at least 100 years, a water-cement ratio as low as 0.45 was adopted due to the contact of the reinforced foundations with the seawater. The placement of the SCC was carried out in only a few hours of a night to reduce the interruption of the ferry traffic in the Grand Canal. The concrete was pumped from truck mixers, all located on the Rome Square side of the bank of the Grand Canal, and feeding the fresh mixture in both the reinforced spaces devoted to the foundations. The reinforced foundations are exposed to a significant load due to the heavy weight of the bridge manufactured of steel and glass, as well as to the shear stress caused by the peculiar shape of the bridge characterized by a segmental arch. Due to these factors, some cracks were observed every year on the top of the foundations. This means that in the next future some measures should be taken to block the formation of new cracks. Meanwhile, the already formed cracks have been sealed and protected by an upper coating stone in order to inhibit the ingress of the airborne swept by the wind from the close sea water causing the corrosion of the metallic reinforcements promoted by the presence of chloride ions.

Related References:

1. H. Ohamura, “Self-Compacting Concrete”, Concrete International, Vol.19., No. 7, pp. 50-54, 1997.

2. N. Miura, N. Takeda, R. Chikamatsu, S. Sogo, “Self-Compacting Concrete”, ACI SP-140, pp.163-186, 1993.

3. K. Tanaka, K. Sato, S. Watanabe, “Self-Compacting Concretes”, ACI SP-140, pp. 25-51, 1993.

4. EN 197-1 “Cement – Part 1: Composition, specifications and conformity criteria for common cements”, 2011.

5. EN 206-1, “Concrete – Specification, performance, production and conformity”, 2016.