Meta-Analysis of PCE Structures as Dispersants in Cementitious Materials

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Meta-Analysis of PCE Structures as Dispersants in Cementitious Materials

Author(s): Thomas Wagner, Tobias Lange, Torben Gädt

Publication: Symposium Paper

Volume: 354

Issue:

Appears on pages(s): 61-74

Keywords: cement; dispersant; meta-analysis; polycarboxylate ether; rheology; slump flow; yield stress

DOI: 10.14359/51736062

Date: 7/1/2022

Abstract:
The structure-activity relationship of dispersants in cement was explored by conducting a meta-analysis of academic publications on polycarboxylate ether (PCE). Therefore, structural data of PCE dispersants was collected from the academic literature together with the corresponding mini-slump data. The structures were summarized using the structural parameters P (the number of repeat units of the side chain), n (the number of repeat units in the backbone), and N (the number of monomers per repeat unit). It was found that the distribution of side-chain length is multimodal, reflecting the availability of commercial macromonomers based on poly(ethylene glycol) (PEG). For the mean values, it was found P = 38.5, N = 4.7, and n = 24.3. The most frequently employed charge-bearing monomers are acrylic acid, methacrylic acid, and maleic acid. The main macromonomers are either based on methoxy poly(ethylene glycol) methacrylate, isoprenyl-poly(ethylene glycol) (IPEG), methallyl-PEG, or allyl-PEG. Additionally, rheology data from mini-slump tests containing this PCE was transformed into yield stress data. In an attempt to identify the most dosage-efficient PCE structures, the yield stress data were compared with PCE structural descriptors and dosage. It was found that PCE with a P/N ratio between 6-12 and an adsorption constant between 10-100 show the highest dosage efficiency.