Analysis of the Effect of Three-Stage Mixing on the Properties of Concrete with Recycled Aggregates and Various Mineral Additives

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Analysis of the Effect of Three-Stage Mixing on the Properties of Concrete with Recycled Aggregates and Various Mineral Additives

Author(s): Alena Sicakova

Publication: Symposium Paper

Volume: 355

Issue:

Appears on pages(s): 455-464

Keywords: recycled concrete aggregate; cement; fly ash; recycled concrete powder; recycled aggregate concrete; three-stage mixing; compressive strength, prolonged mixing time

DOI: 10.14359/51736053

Date: 7/1/2022

Abstract:
The use of recycled concrete aggregate, as a component of the new concrete mixture, implies a thorough understanding of its basic properties, considering that they may significantly differ from the properties of natural aggregates. It is believed that its performance can be enhanced by improving the surface properties of RCA. Coating RCA grains within a triple mixing process represents one of the promising methods. This principle has been adopted by several researchers who report a significant improvement in concrete properties compared to standard mixing, especially through improved ITZ parameters. In the paper, the triple mixing process of concrete with coarse RCA was studied, while the method of applying the mineral powdery materials (cement, fly ash, and fine particles of RCA) to the pre-moistened aggregate was used. A comparison of positive/negative effects of three-stage mixing on the set of six properties of concrete, comparing standard mixing is presented. It was found that three-stage mixing has no different effect on samples prepared after prolonged mixing than on samples prepared immediately after mixing, nor on samples cured for 90 days than on samples cured 28-days. Cement as a coating material gave the best results in the presented range of testing while RCA powder showed promising potential.

Related References:

1. Soga, S., and Takagi, K., “Influence of the mixing energy on fresh concrete,” Transactions of the Japan Concrete Institute 8 (1986), pp. 73–80.

2. Mitsutaka, H. and I. Yasuro I., “A new concrete mixing method for improving bond mechanisms”. Bond in Concrete: Proceedings from the International Conference on Bond in Concrete, 1982, pp. 282-288. Ed. P. Bartos, Paisley, Scotland: Paisley College of Technology.

3. Tamimi, A. K., “Effects of a new mixing technique on the properties of the cement paste-aggregate interface,” Cement and Concrete Research 24(7), 19941pp. 299–1304.

4. Gaynor, R. D., “Avoiding uniformity problems in truck-mixed concrete,” Concrete Journal, August 2006, Pp. 570–572.

5. Pope, A. W. and Jennings, H. M., “The influence of mixing on the microstructure of the cement paste/aggregate interfacial zone and the strength of mortar,” Journal of Materials Science, Vol. 26, 1992, pp. 6452–6462.

6. Rejeb, S. K., “Improving compressive strength of concrete by a two-step mixing method,” Cement and Concrete Research, Vol. 26, no. 4, 1996, pp. 585–592.

7. Tam, V. W. Y. et al., “Microstructural analysis of recycled aggregate concrete produced from two-stage mixing approach,” Cement and Concrete Research, Vol. 35, no. 6, 2005, pp. 1195–1203.

8. Li, J., Xiao, H. and Zhou, Y. “Influence of coating recycled aggregate surface with pozzolanic powder on properties of recycled aggregate concrete,” Construction and Building Materials, 23, 2009, pp. 1287–1291.

9. Elhakam, A.A., Mohamed, A.E. and Awad, E., “Influence of self-healing, mixing method and adding silica fume on mechanical properties of recycled aggregates concrete,” Construction and Building Materials 35, 2012, pp. 421–427.

10. Ryu, J. S., “Improvement on strength and impermeability of recycled concrete made from crushed concrete coarse aggregate,” Journal of Materials Science Letters 21, 2002, pp. 1565 – 1567.

11. Uniyal, S. and Aggrawal, V., “Two-Stage Mixing Approach (TSMA) Versus Normal Mixing Approach (NMA) For Concrete in Terms of Compressive Strength and Carbonation Depth,” IJSRD - International Journal for Scientific Research & Development, Vol. 2, no. 5, 2014, pp. 721–725.

12. Tam, V. W. Y. and Tam, C.M., “Diversifying two-stage mixing approach (TSMA) for recycled aggregate concrete: TSMAs and TSMAsc,” Construction and Building Materials 22, 2008, pp. 2068–2077.

13. Jeong, H., “Processing and properties of recycled aggregate concrete,” Master of Science, University of Illinois, Urbana: 2011.

14. Lee, S. H. et al., “Influence of aggregate coated with modified sulfur on the properties of cement concrete,” Materials, Vol. 7, no. 6, 2014, pp. 4739–4754.

15. Fládr, J. and Bílý, P., “Influence of mixing procedure on mechanical properties of high-performance concrete,” Fibre Concrete 2017, IOP Conf. Series: Materials Science and Engineering, 246.

16. Preetha, R. et al., “Effect of mixing methods in behavior of fly ash concrete,” online. https://www.nbmcw.com/concrete/27659-effect-of-mixing-methods-in-behavior-of-flyash-concrete.html

17. Kong, D. et al., “Effect and mechanism of surface-coating pozzalanics materials around aggregate on properties and ITZ microstructure of recycled aggregate concrete,” Construction and Building Materials, Vol. 24, no. 5, 2010, pp. 701–708.

18. Kong, D.Y., et al., “Strengthening of the ITZ in recycled aggregate concrete,” Xi’an international conference on architecture and technology, proceedings – architecture in harmony, Xian, PRC, 2006, pp. 614-617.

19. Surya, M. et al., “Recycled aggregate concrete for transportation infrastructure,” Procedia - Social and Behavioral Sciences. Vol. 104, 2013, pp. 1158–1167.

20. Zhang. W. et al, “Effect of the optimized triple mixing method on the ITZ microstructure and performancedoi of recycled aggregate concrete,” Construction and Building Materials 203, 2019, pp. 601–607.

21. Sicakova, A. and Urban. K., “The influence of discharge time, kind of additive, and kind of aggregate on the properties of three-stage mixed concrete,” Sustainability, 10 (11), 2018, pp. 1-13.

22. CEN EN 12350-2: 2010Testing fresh concrete. Part 2 Slump test. European Committee for Standardization: Brussels, Belgium, 2016.

23. CEN EN 12390-3: 2010 Testing Hardened Concrete. Part 3: Compressive Strength of Test Specimens; European Committee for Standardization: Brussels, Belgium, 2010.

24. CEN EN 12390-6:2009 Testing Hardened Concrete. Part 6: Tensile Splitting Strength of Test Specimens; European Committee for Standardization: Brussels, Belgium, 2009.

25. CEN EN 1015-18:2003 Methods of Test for Mortar for Masonry. Part 18: Determination of Water Absorption Coefficient Due to Capillary Action of Hardened Mortar. European Committee for Standardization: Brussels, Belgium, 2003.

26. CEN EN 12390-8: 2011 Testing Hardened Concrete. Part 8: Depth of Penetration of Water under Pressure; European Committee for Standardization: Brussels, Belgium, 2011.