Mix-Designs of Concretes in Durable Reinforced and Prestressed Structures of a Viaduct for a Railway Train Connecting Venice with Cortina, in Italy

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Mix-Designs of Concretes in Durable Reinforced and Prestressed Structures of a Viaduct for a Railway Train Connecting Venice with Cortina, in Italy

Author(s): Mario Collepardi, Silvia Collepardi, Roberto Troli

Publication: Symposium Paper

Volume: 355

Issue:

Appears on pages(s): 307-316

Keywords: Carbonation; Durability; Freezing-Thawing Cycles; Mix-Design; Sea-Water

DOI: 10.14359/51736036

Date: 7/1/2022

Abstract:
In this paper, the mixture designs of the concrete in durable reinforced and prestressed structures of a viaduct for a railway train connecting Venice directly with Cortina are illustrated. Three mixture designs, based on the European Norms for the 100-year durable concrete reinforced or prestressed structures of the above construction, are developed as a function of the environmental region crossed by the viaduct of this railway train. The first region of the travel connects the Santa Lucia railway station in Venice with the mainland where the reinforced and prestressed concrete structures are exposed to tidal, splash, and spray zones of the close seawater. The second region crossed by the viaduct of the railway train is the oriental Po Valley exposed to air and rain and then to the penetration of CO2 with the risk of corrosion of the metallic reinforcements. The last region crossed by the viaduct of the railway train is a large area of up to 1,500 m (4,920 ft)-high mountains and is exposed in winter seasons to freeze-thaw cycles. A pozzolanic cement type CEM II-B/V 42.5 N, with about 20% Portland cement replaced by siliceous fly ash, is recommended to ensure that the alkali-reactive aggregates, if any, are neutralized by the presence of fly ash. For structural reasons, a cube characteristic strength (fcu/ck) of 50 MPa (7,250 psi) is prescribed for all the viaducts crossing the three regions.

Related References:

1. L.Zaia, “Dolomites’s train: there is the agreement, Zaia dreams the Venice-Cortina train”, Il Gazzettino, June, 28,2019.

2. EN 206-1, “Concrete – Specification, performance, production and conformity”, December 2016.

3. Eurocode 2,”Design of concrete structures – Part 1-1: General rules and rules for buildings”, 2015.

4. EN 197-1 “Cement composition, specification and conformity criteria for common cements”, 1993.

5. M. Collepardi, “Damage by alkali silica reaction”, The New Concrete, pp.154-157, Second Edition, published by Grafiche Tintoretto, 2010.

6. M. Collepardi, S. Collepardi and R. Troli, “Cube compressive strength with cement class 42.5”, Concrete Mix Design, pg 55, Grafiche Tintoretto, 2007.

7. I. Lyse, “Tests in consistency and strength of concrete having constant water content”, Proceedings A.S.T.M. 32, pp.629-636, 1932.