Title:
Production of Lightweight Aggregates by Means of Cold-Bonding Granulation Process of Municipal Solid Waste Incinerator (MSWI) Fly Ash
Author(s):
Ilenia Farina, Cinzia Salzano, Marco de Pertis, Alberto Ferraro, Francesco Colangelo, Raffaele Cioffi
Publication:
Symposium Paper
Volume:
355
Issue:
Appears on pages(s):
109-114
Keywords:
cold-bonding granulation, granulated blast furnace slag, industrial waste, lightweight artificial aggregates, marble sludge, MSWI fly-ash
DOI:
10.14359/51736017
Date:
7/1/2022
Abstract:
The recovery/recycling of solid industrial waste is a major environmental, economic and productive reality in the context of waste management activities. One of the main aspects related to the application of recovery technologies is the removal of waste from landfills and it is sufficient to observe the consequent proportional decrease in quantities of industrial waste in landfills in order to confirm the progressive development of recovery technologies related to the world of waste. Disposal and recovery/recycling aim at minimizing environmental impacts and promoting the efficient use of resources. In the current landscape of waste recycling, there are consolidated activities in constant search of technological improvements aimed at optimizing recovery efficiency. In this context, the final goal of this study is the production of lightweight artificial aggregates through the recycling of industrial solid waste, such as fly ash, blast furnace slag, and marble sludge. The results show that the aggregates produced can be classified as lightweight aggregates and are suitable for road paving.
Related References:
1. Biskri, Y., Achoura, D., Chelghoum, N., & Mouret, M., 2017. Mechanical and durability characteristics of High Performance Concrete containing steel slag and crystalized slag as aggregates. Construction and Building Materials, 150, 167-178.
2. Aslam, M., Shafigh, P., Nomeli, M. A., & Jumaat, M. Z., 2017. Manufacturing of high-strength lightweight aggregate concrete using blended coarse lightweight aggregates. Journal of building engineering, 13, 53-62.
3. Thomas, J., Thaickavil, N. N., & Wilson, P. M. (2018). Strength and durability of concrete containing recycled concrete aggregates. Journal of Building Engineering, 19, 349-365.
4. Tam, V.W.Y., Soomro, M., Evangelista, A.C.J., 2018. A review of recycled aggregate in concrete applications (2000–2017). Constr. Build. Mater. 172, 272–292. doi: 10.1016/j.conbuildmat.2018.03.240
5. Tang, P., Florea, M. V. A., & Brouwers, H. J. H. (2017). Employing cold bonded pelletization to produce lightweight aggregates from incineration fine bottom ash. Journal of cleaner production, 165, 1371-1384.
6. Tang, P., & Brouwers, H. J. H. (2017). Integral recycling of municipal solid waste incineration (MSWI) bottom ash fines (0–2 mm) and industrial powder wastes by cold-bonding pelletization. Waste Management, 62, 125-138.
7. Güneyisi, E., Gesoğlu, M., Pürsünlü, Ö., & Mermerdaş, K. (2013). Durability aspect of concretes composed of cold bonded and sintered fly ash lightweight aggregates. Composites Part B: Engineering, 53, 258-266.
8. Gesoğlu, M., Özturan, T., Güneyisi, E., 2007. Effects of fly ash properties on characteristics of cold-bonded fly ash lightweight aggregates. Constr. Build. Mater. 21, 1869–1878.
9. Frankovič, A., Bokan-Bosiljkov, V., Ducman, V., 2017. Lightweight aggregates made from fly ash using the coldbond process and their use in lightweight concrete. Materiali in tehnologije 51, 267-274.
10. Li, S., Liu, K., Sun, L., 2017. Effect of different kinds of lightweight aggregates on performance of composite insulation materials. Journal of Building Materials, 20(2), 245-250.
11. Colangelo, F., Petrillo, A., Cioffi, R., Borrelli, C., Forcina, A., 2018. Life cycle assessment of recycled concretes: A case study in southern Italy, Science of The Total Environment, 615, pp. 1506-1517.
12. Ferraro, A., Colangelo, F., Farina, I., Race, M., Cioffi, R., Cheeseman, C., Fabbricino, M., 2020. Cold-bonding process for treatment and reuse of waste materials: Technical designs and applications of pelletized products. Critical Reviews in Environmental Science and Technology, 1-35.
13. Tajra, F., Abd Elrahman, M., Chung, S.-Y., Stephan, D., 2018. Performance assessment of core-shell structured lightweight aggregate produced by cold bonding pelletization process. Constr. Build. Mater. 179, 220–231.
14. Colangelo, F., Messina, F., Cioffi, R., 2015. Recycling of MSWI fly ash by means of cementitious double step cold bonding pelletization: Technological assessment for the production of lightweight artificial aggregates. Journal of Hazardous Materials, 299, pp. 181-191.