Influence of Thickness Parameters on Performance of Interlocking Concrete Block Pavement

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Influence of Thickness Parameters on Performance of Interlocking Concrete Block Pavement

Author(s): Arjun Siva Rathan R. T., Sunitha V., and Anusudha V.

Publication: Materials Journal

Volume: 119

Issue: 6

Appears on pages(s): 65-76

Keywords: deflection; interlocking paver; numerical; optimization; plate load

DOI: 10.14359/51736002

Date: 11/1/2022

Abstract:
Interlocking concrete block pavement (ICBP) is one of the pavement types adopted worldwide. The influential parameter of ICBP is comparatively more, which includes the geometric parameters of the interlocking paver blocks such as the size, shape, thickness, strength, and laying pattern of the blocks, and the gradations of the jointing and bedding sand. Other than the wearing surface, the thickness and properties of the bedding sand, base, and subgrade also play a vital role in the deflection properties of ICBP. The objective of the present study is to analyze the influence of block thickness, base thickness, and granular layer thickness on the deflection behavior and stress distribution of ICBP. The block thicknesses used for this study are 80, 100, and 120 mm; the bedding sand thicknesses are 30, 50, and 70 mm; and the base thicknesses are 150, 300, and 450 mm. The experimental work is carried out using the laboratory plate load test to determine the deflection and stress distribution of ICBP. Numerical analysis is also employed to simulate laboratory testing. The study attempts to find the most influential factor and the optimized parametric value for attaining lower deflection using Design-Expert software. The test results conclude that the thicknesses of the block and granular layer play an imperative role among the considered parameters.

Related References:

ASTM D1196-93(1997), 1997, “Standard Test Method for Nonrepetitive Static Plate Load Tests of Soils and Flexible Pavement Components, for Use in Evaluation and Design of Airport and Highway Pavements,” ASTM International, West Conshohocken, PA, 2 pp.

Chen, C.; Yang, Q.; Leng, W.; Dong, J.; Xu, F.; Wei, L.; and Ruan, B., 2022, “Experimental Investigation of the Mechanical Properties of the Sand–Concrete Pile Interface Considering Roughness and Relative Density,” Materials (Basel), V. 15, No. 13, July, Article No. 4480. doi: 10.3390/ma15134480

Füssl, J.; Kluger-Eigl, W.; and Blab, R., 2016, “Experimental Identification and Mechanical Interpretation of the Interaction Behaviour between Concrete Paving Blocks,” International Journal of Pavement Engineering, V. 17, No. 6, pp. 478-488.

Gunatilake, D., and Mampearachchi, W. K., 2019, “Finite Element Modelling Approach to Determine Optimum Dimensions for Interlocking Concrete Blocks Used for Road Paving,” Road Materials and Pavement Design, V. 20, No. 2, pp. 280-296. doi: 10.1080/14680629.2017.1385512

IRC:SP:20-2002, 2002, “Rural Roads Manual,” Indian Roads Congress, New Delhi, India, 383 pp.

IRC:SP:63-2018, 2018, “Guidelines for the Use of Interlocking Concrete Block Pavement,” India Roads Congress, New Delhi, India, 52 pp.

IS 383:2016, 2016, “Coarse and Fine Aggregate for Concrete — Specification,” Bureau of Indian Standards, New Delhi, India, 21 pp.

IS:1498-1970 (R2007), 1970, “Classification and Identification of Soils for General Engineering Purposes,” Bureau of Indian Standards, New Delhi, India, 28 pp.

IS 15658:2006, 2006, “Precast Concrete Blocks for Paving—Specification,” Bureau of Indian Standards, New Delhi, India, 27 pp.

Jamshidi, A.; Kurumisawa, K.; White, G.; Nishizawa, T.; Igarashi, T.; Nawa, T.; and Mao, J., 2019, “State-of-the-Art of Interlocking Concrete Block Pavement Technology in Japan as a Post-Modern Pavement,” Construction and Building Materials, V. 200, Mar., pp. 713-755. doi: 10.1016/j.conbuildmat.2018.11.286

Knapton, J., 1992, “The Structural Design of Heavy Duty Concrete Block Pavements,” Workshop on Interlocking Concrete Pavements, pp. 187-198.

Knapton, J., and Barber, S. D., 1982, “UK Research into Concrete Block Pavement Design,” Concrete Works International, V. 1, No. 3, pp. 107-111.

Kuipers, G., 1992, “The Effect of Concrete Block Lock-Up on Pavement Performance,” Proceedings, Fourth International Conference on Concrete Block Paving, Auckland, New Zealand, pp. 51-59.

Lehmann, S.; Leppla, S.; and Norkus, A., 2020, “Experimental Study of the Modulus of Deformation Determined by Static and Dynamic Plate Load Tests,” The Baltic Journal of Road and Bridge Engineering, V. 15, No. 4, pp. 109-124. doi: 10.7250/bjrbe.2020-15.497

Lin, W.; Cho, Y.-H.; and Kim, I. T., 2016, “Development of Deflection Prediction Model for Concrete Block Pavement Considering the Block Shapes and Construction Patterns,” Advances in Materials Science and Engineering, V. 2016, Article No. 5126436, 9 pp. doi: 10.1155/2016/5126436

Lin, W.; Kim, D.; Ryu, S. W.; Hao, H.; Ge, Y.-E.; and Cho, Y.-H., 2018, “Evaluation of the Load Dissipation Behavior of Concrete Block Pavements with Various Block Shapes and Construction Patterns,” Journal of Materials in Civil Engineering, ASCE, V. 30, No. 2, Feb., p. 04017291. doi: 10.1061/(ASCE)MT.1943-5533.0002113

Mampearachchi, W. K., and Senadeera, A., 2014, “Determination of the Most Effective Cement Concrete Block Laying Pattern and Shape for Road Pavement Based on Field Performance,” Journal of Materials in Civil Engineering, ASCE, V. 26, No. 2, Feb., pp. 226-232. doi: 10.1061/(ASCE)MT.1943-5533.0000801

Panda, B. C., and Ghosh, A. K., 2001, “Source of Jointing Sand for Concrete Block Pavement,” Journal of Materials in Civil Engineering, ASCE, V. 13, No. 3, June, pp. 235-237. doi: 10.1061/(ASCE)0899-1561(2001)13:3(235)

Panda, B. C., and Ghosh, A. K., 2002a, “Structural Behavior of Concrete Block Paving. II: Concrete Blocks,” Journal of Transportation Engineering, ASCE, V. 128, No. 2, Mar., pp. 130-135. doi: 10.1061/(ASCE)0733-947X(2002)128:2(130)

Panda, B. C., and Ghosh, A. K., 2002b, “Structural Behavior of Concrete Block Paving. I: Sand in Bed and Joints,” Journal of Transportation Engineering, ASCE, V. 128, No. 2, Mar., pp. 123-129. doi: 10.1061/(ASCE)0733-947X(2002)128:2(130)

Rada, G. R.; Smith, D. R.; Miller, J. S.; and Witczak, M. W., 1990, “Structural Design of Concrete Block Pavements,” Journal of Transportation Engineering, ASCE, V. 116, No. 5, Sept., pp. 615-635. doi: 10.1061/(ASCE)0733-947X(1990)116:5(615)

Rathan, A. S. R. T., and Sunitha, V., 2021, “Development of Design Procedure for Interlocking Concrete Block Pavement,” International Journal of Pavement Engineering, pp. 1-15.

Rathan, A. S. R. T.; Sai, A.; and Sunitha, V., 2021a, “Mechanical and Structural Performance Evaluation of Pervious Interlocking Paver Blocks,” Construction and Building Materials, V. 292, July, Article No. 123438. doi: 10.1016/j.conbuildmat.2021.123438

Rathan, A. S. R. T.; Velayudhan, S.; Pathath, M.; Lekshmipathy, J.; and Visvanathan, A., 2021b, “Experimental and Numerical Evaluation of the Parameters Influencing the Shear-Stress Behavior of Interlocking Paver Blocks–Bedding Sand Interface Using Large-Scale Direct Shear Test,” Journal of Materials in Civil Engineering, ASCE, V. 33, No. 6, June, p. 04021104. doi: 10.1061/(ASCE)MT.1943-5533.0003724

Rathan, A. S. R. T.; Sunitha, V.; Murshida, P.; and Anusudha, V., 2022, “Influence of Bedding and Jointing Sand on the Shear Strength Characteristics of Interlocking Paver Blocks – Bedding Sand Interface,” International Journal of Pavement Engineering, V. 23, No. 7, pp. 2160-2175. doi: 10.1080/10298436.2020.1847286

Sarkar, H.; Halder, P. C.; and Ryntathiang, T. L., 2014, “Behavior of Interlocking Concrete Block Pavement over Stone Dust Grouted Subbase,” International Journal of Advanced Structures and Geotechnical Engineering, V. 03, No. 01, Jan., pp. 44-48.

Shackel, B., 1988, “The Evolution and Application of Mechanistic Design Procedures for Concrete Block Pavements,” Proceedings, Third International Conference on Concrete Block Paving, Rome, Italy, pp. 114-120.

Shafabakhsh, G.; Family, A.; and Pourzand Hossein Abad, B., 2014, “Numerical Analysis of Concrete Block Pavements and Comparison of Its Settlement with Asphalt Concrete Pavements Using Finite Element Method,” Engineering Journal, V. 18, No. 4, Oct., pp. 39-51.

Tawfik, M. M., and El-Mossallamy, Y. M., 2017, “Application of the Finite Element Method for Investigating the Dynamic Plate Loading Test,” Ain Shams Engineering Journal, V. 8, No. 1, Mar., pp. 39-49. doi: 10.1016/j.asej.2015.08.011

Wellner, F., and Gleitz, T., 1996, “Dynamic Load Bearing Tests on Block Pavements,” Proceedings, Fifth International Conference on Concrete Block Paving, Tel Aviv, Israel, pp. 317-327.