Effect of Corrosion on Bond Strength and Development Length of Reinforcing Bar in Epoxy-Grouted Nut Coupler

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effect of Corrosion on Bond Strength and Development Length of Reinforcing Bar in Epoxy-Grouted Nut Coupler

Author(s): Naseeruddin Haris and Sangeeta Gadve

Publication: Materials Journal

Volume: 119

Issue: 5

Appears on pages(s): 239-250

Keywords: corrosion; coupler bond strength; development length; epoxy; impressed current; nut coupler; pullout test; reinforcing bar

DOI: 10.14359/51735977

Date: 9/1/2022

Abstract:
Corrosion of steel reinforcing bars in reinforced concrete (RC) structures is a matter of concern among practicing engineers and researchers are perpetually working over it. The development length of reinforcing bars at joints of RC structural frames are more prone to severe corrosion. Due to this, the design stress that needs to be developed in reinforcing bars is largely reduced. In addition, the development lengths of reinforcing bars create congestion at frame joints. This paper is an attempt to overcome these issues. In this paper, an epoxy-grouted nut coupler system is proposed that generates the required design stress in reinforcing bars with a very short development length at end anchorages, due to which congestion of the reinforcing bar at the joints can be avoided. The experimental investigation on the effect of corrosion on bond strength and development length of reinforcing bar in this epoxy-grouted nut coupler is also carried out by performing pullout tests. Statistical models are developed to predict the bond strength between the coupler and reinforcing bar corroded to different levels. This epoxy-grouted nut coupler is an effective tool for developing required stress in reinforcing bars by reducing the actual development length of reinforcing bars in the case of new structures. It is also useful and convenient in regeneration of stress in reinforcing bars at end anchorages that has been lost in corrosion-damaged structures.

Related References:

1. Almusallam, A. A., “Effect of Degree of Corrosion on the Properties of Reinforcing Steel Bars,” Construction and Building Materials, V. 15, No. 8, 2001, pp. 361-368. doi: 10.1016/S0950-0618(01)00009-5

2. El Maaddawy, T. A., and Soudki, K. A., “Effectiveness of Impressed Current Technique to Simulate Corrosion of Steel Reinforcement in Concrete,” Journal of Materials in Civil Engineering, ASCE, V. 15, No. 1, 2003, pp. 41-47. doi: 10.1061/(ASCE)0899-1561(2003)15:1(41)

3. IS 456:2000, “Plain and Reinforced Concrete - Code of Practice,” Bureau of Indian Standards, New Delhi, India.

4. BS EN 1992-1-1:2004+A1:2014, “Eurocode 2: Design of concrete structures — Part 1-1: General rules and rules for buildings,” British Standards Institution, London, UK.

5. AS 3600:2018, “Concrete Structures,” Standards Australia, Sydney, NSW, Australia.

6. GB 50010:2010, “Code for Design of Concrete Structures,” China Architecture and Building Press, Beijing, China.

7. Zhang, X., and Li, B., “Seismic Performance of Exterior Reinforced Concrete Beam-Column Joint with Corroded Reinforcement,” Engineering Structures, V. 228, 2021, p. 111556. doi: 10.1016/j.engstruct.2020.111556

8. Bahekar, P. V., and Gadve, S. S., “Impressed Current Cathodic Protection of Rebar in Concrete Using Carbon FRP Laminate,” Construction and Building Materials, V. 156, 2017, pp. 242-251. doi: 10.1016/j.conbuildmat.2017.08.145

9. Zhang, Y.; Biçici, E.; Sezen, H.; and Zheng, S., “Reinforcement Slip Model Considering Corrosion Effects,” Construction and Building Materials, V. 235, 2020, p. 117348. doi: 10.1016/j.conbuildmat.2019.117348

10. Fernandez, I.; Bairán, J. M.; and Marí, A. R., “Corrosion Effects on the Mechanical Properties of Reinforcing Steel Bars Fatigue and σ-ε Behaviour,” Construction and Building Materials, V. 101, 2015, pp. 772-783. doi: 10.1016/j.conbuildmat.2015.10.139

11. Cheng, H.; Li, H.-N.; Biondini F. Wang, D.-S.; and Zou, Y., “Strain Penetration Effect on Cyclic Response of Corroded RC Columns,” Engineering Structures, V. 243, 2021, p. 112653. doi: 10.1016/j.engstruct.2021.112653

12. Kang, T.; Shin, M.; and Mitra, N., “Headed Reinforcement Applications for Reinforced Concrete Beam Column Connections,” Structures Congress: Don’t Mess with Structural Engineers, 2009, pp. 1505-1514.

13. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19),” American Concrete Institute, Farmington Hills, MI, 2019, 623 pp.

14. Thompson, M. K.; Ziehl, M. J.; Jirsa, J. O.; and Breen, J. E., “CCT Nodes Anchored by Headed Bars—Part 1: Behavior of Nodes,” ACI Structural Journal, V. 102, No. 6, Nov.-Dec. 2005, pp. 808-815.

15. Thompson, M. K.; Jirsa, J. O.; and Breen, J. E., “CCT Nodes Anchored by Headed Bars—Part 2: Capacity of Nodes,” ACI Structural Journal, V. 103, No. 1, Jan.-Feb. 2006, pp. 65-73.

16. Thompson, M. K.; Ledesma, A.; Jirsa, J. O.; and Breen, J. E., “Lap Splices Anchored by Headed Bars,” ACI Structural Journal, V. 103, No. 2, Mar.-Apr. 2006, pp. 271-279.

17. Shao, Y.; Darwin, D.; O’Reilly, M.; Lequesne, R. D.; Ghimire, K.; and Hano, M., “Anchorage of Conventional and High-Strength Headed Reinforcing Bars,” SM Report No. 117, University of Kansas Center for Research, Lawrence, KS, Aug. 2016, 234 pp.

18. Breña, S.; Messier, J.; and Peterfreund, S., “Behavior of Straight and T-Headed ASTM A1035/A1035M Bar Splices in Flexural Members,” ACI Structural Journal, V. 115, No. 1, Jan. 2018, pp. 79-90. doi: 10.14359/51700782

19. Einea, A.; Yamane, T.; and Tadros, M., “Grout-Filled Pipe Splices for Precast Concrete Construction,” PCI Journal, V. 40, No. 1, 1995, pp. 82-93. doi: 10.15554/pcij.01011995.82.93

20. Austin, S. A.; Lyons, R.; and Ing, M. J., “Electrochemical Behavior of Steel-Reinforced Concrete during Accelerated Corrosion Testing,” Corrosion Science, V. 60, No. 2, 2004, pp. 203-212. doi: 10.5006/1.3287722

21. Gadve, S.; Mukherjee, A.; and Malhotra, S. N., “Corrosion Protection of Fiber-Reinforced Polymer-Wrapped Reinforced Concrete,” ACI Materials Journal, V. 107, No. 4, July-Aug. 2010, pp. 349-356.

22. Haris, “Mechanical Properties of Reinforcing Steel Bars Corroded at Different Levels,” ACI Materials Journal, V. 118, No. 4, July 2021, pp. 109-120.

23. Imperatore, S.; Rinaldi, Z.; and Drago, C., “Degradation Relationships for the Mechanical Properties of Corroded Steel Rebars,” Construction and Building Materials, V. 148, 2017, pp. 219-230. doi: 10.1016/j.conbuildmat.2017.04.209

24. NZS3101-2006+A1-3, “Concrete Structures Standard Part 1: The Design of Concrete Structures,” Standards New Zealand, Sydney, NSW, Australia.

25.. IS 1786:2008, “High Strength Deformed Steel Bars and Wires for Concrete Reinforcement-Specification,” Bureau of Indian Standards, New Delhi, India, 2008.

26. Caré, S., and Raharinaivo, A., “Influence of Impressed Current on the Initiation of Damage in Reinforced Mortar Due to Corrosion of Embedded Steel,” Cement and Concrete Research, V. 37, 2007, pp. 1598-1612.

27. ASTM G1-90, “Standard Practice for Preparing, Cleaning, and Evaluating Corrosion Test Specimens,” ASTM International, West Conshohocken, PA, 1999, 20 pp.

28. BS EN 1990:2002, “Eurocode: Basis of Structural Design,” British Standards Institution, London, UK, 2002.


ALSO AVAILABLE IN:

Electronic Materials Journal