Stable Time for Concrete Gas Permeability in Natural Tidal Environment

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Stable Time for Concrete Gas Permeability in Natural Tidal Environment

Author(s): Yun Zhang, Meng Wang, Chen-Lu Fu, Yan-Hong Gao, and Yu-Rong Zhang

Publication: Materials Journal

Volume: 119

Issue: 5

Appears on pages(s): 213-226

Keywords: gas permeability coefficient; microstructure; natural tidal environment; stable time

DOI: 10.14359/51735956

Date: 9/1/2022

Abstract:
The stable time for concrete permeability is of great significance to evaluate the permeability of concrete and predict the service life of actual engineering. Based on a test with an exposure time of more than 3 years in a natural tidal environment, the gas permeability and microstructure parameters of concrete with different water-binder ratios (w/b) and admixtures including fly ash (FA), slag (SG), silica fume (SF), and basalt fiber (BF) were tracked and tested. Then, the time-dependent gas permeability and main microstructure parameters and their stable time were investigated. Finally, the relationship between stable time for the gas permeability coefficient and microstructure parameters was studied. The results show that the apparent and intrinsic gas permeability coefficients of concrete both decrease with exposure time. For ordinary concrete, the gas permeability coefficient and the corresponding stable time increase with w/b. The stable time for gas permeability coefficients of SF concrete is the shortest among admixture concrete, while that of BF concrete is the longest. The time dependent gas permeability is in keeping with the change of total porosity and contributive porosity of large capillary pores (100 to 1000 nm) with exposure time. Moreover, the change trends of stable time for gas permeability, total porosity, and contributive porosity of large capillary pores with w/b and admixture type are consistent. The stable time for the intrinsic gas permeability coefficient has a better correlation with that for contributive porosity of large capillary pores than that for total porosity. The intrinsic gas permeability coefficient stabilizes first, followed by contributive porosity of large capillary pores, which is the most important factor influencing the stable time for the intrinsic gas permeability coefficient, and total porosity stabilizes last.

Related References:

1. Basheer, L.; Kropp, J.; and Cleland, D. J., “Assessment of the Durability of Concrete from Its Permeation Properties: A Review,” Construction and Building Materials, V. 15, No. 2-3, 2001, pp. 93-103. doi: 10.1016/S0950-0618(00)00058-1

2. Demis, S., and Papadakis, V. P., “Durability Design Process of Reinforced Concrete Structures - Service Life Estimation, Problems and Perspectives,” Journal of Building Engineering, V. 26, 2019, p. 100876. doi: 10.1016/j.jobe.2019.100876

3. Dhandapani, Y.; Sakthivel, T.; Santhanam, M.; Gettu, R.; and Pillai, R. G., “Mechanical Properties and Durability Performance of Concretes with Limestone Calcined Clay Cement (LC3),” Cement and Concrete Research, V. 107, 2018, pp. 136-151. doi: 10.1016/j.cemconres.2018.02.005

4. Qian, R.; Shi, J.; Li, Y.; Chen, W.; Liu, G.; Liu, Z. Y.; She, W.; and Zhang, Y. S., “Investigation on Parameters Optimization for Gas Permeability Testing of Concrete: Inlet-Gas Pressure and Confining Pressure,” Construction and Building Materials, V. 250, 2020, p. 118901. doi: 10.1016/j.conbuildmat.2020.118901

5. Gui, Q.; Qin, M.; and Li, K., “Gas Permeability and Electrical Conductivity of Structural Concretes: Impact of Pore Structure and Pore Saturation,” Cement and Concrete Research, V. 89, 2016, pp. 109-119. doi: 10.1016/j.cemconres.2016.08.009

6. Zhang, J.; Bian, F.; Zhang, Y. R.; Fang, Z.; Fu, C.; and Guo, J., “Effect of Pore Structures on Gas Permeability and Chloride Diffusivity of Concrete,” Construction and Building Materials, V. 163, 2018, pp. 402-413. doi: 10.1016/j.conbuildmat.2017.12.111

7. Zhou, C. S.; Chen, W.; Wang, W.; and Skoczylas, F., “Indirect Assessment of Hydraulic Diffusivity and Permeability for Unsaturated Cement-Based Material from Sorptivity,” Cement and Concrete Research, V. 82, 2016, pp. 117-129. doi: 10.1016/j.cemconres.2016.01.002

8. Zhang, P.; Hou, D. S.; Liu, Q.; Liu, Z. L.; and Yu, J., “Water and Chloride Ions Migration in Porous Cementitious Materials: An Experimental and Molecular Dynamics Investigation,” Cement and Concrete Research, V. 102, 2017, pp. 161-174. doi: 10.1016/j.cemconres.2017.09.010

9. Kim, Y. Y.; Lee, K. M.; Bang, J. W.; and Kwon, S. J., “Effect of w/c Ratio on Durability and Porosity in Cement Mortar with Constant Cement Amount,” Advances in Materials Science and Engineering, V. 2014, 2014, pp. 1-11. doi: 10.1155/2014/273460

10. Zhang, J.; Guo, J.; Li, D. H.; Zhang, Y. R.; Bian, F.; and Fang, Z. F., “The Influence of Admixture on Chloride Time-Varying Diffusivity and Microstructure of Concrete by Low-Field NMR,” Ocean Engineering, V. 142, 2017, pp. 94-101. doi: 10.1016/j.oceaneng.2017.06.065

11. Hassan, K. E.; Cabrera, J. G.; and Maliehe, R. S., “The Effect of Mineral Admixtures on the Properties of High-Performance Concrete,” Cement and Concrete Composites, V. 22, No. 4, 2000, pp. 267-271. doi: 10.1016/S0958-9465(00)00031-7

12. Hamami, A. A.; Turcry, P.; and Aït-Mokhtar, A., “Influence of Mix Proportions on Microstructure and Gas Permeability of Cement Pastes and Mortars,” Cement and Concrete Research, V. 42, No. 2, 2012, pp. 490-498. doi: 10.1016/j.cemconres.2011.11.019

13. Yacoub, A.; Djerbi, A.; and Fen-Chong, T., “The Effect of the Drying Temperature on Water Porosity and Gas Permeability of Recycled Sand Mortar,” Construction and Building Materials, V. 214, 2019, pp. 677-684. doi: 10.1016/j.conbuildmat.2019.04.128

14. Real, S., and Bogas, J. A., “Oxygen Permeability of Structural Lightweight Aggregate Concrete,” Construction and Building Materials, V. 137, 2017, pp. 21-34. doi: 10.1016/j.conbuildmat.2017.01.075

15. Atmaca, N.; Abbas, M. L.; and Atmaca, A., “Effects of Nano-Silica on the Gas Permeability, Durability and Mechanical Properties of High-Strength Lightweight Concrete,” Construction and Building Materials, V. 147, 2017, pp. 17-26. doi: 10.1016/j.conbuildmat.2017.04.156

16. Sinsiri, T.; Chindaprasirt, P.; and Jaturapitakkul, C., “Influence of Fly Ash Fineness and Shape on the Porosity and Permeability of Blended Cement Pastes,” International Journal of Minerals Metallurgy and Materials, V. 17, No. 6, 2010, pp. 683-690. doi: 10.1007/s12613-010-0374-9

17. Houaria, M. B. A.; Abdelkader, M.; Marta, C.; and Abdelhafid, K., “Comparison Between the Permeability Water and Gas Permeability of the Concretes Under the Effect of Temperature,” Energy Procedia, V. 139, 2017, pp. 725-730. doi: 10.1016/j.egypro.2017.11.278

18. Van den Heede, P.; Gruyaert, E.; and de Belie, N., “Transport Properties of High-Volume Fly Ash Concrete: Capillary Water Sorption, Water Sorption Under Vacuum and Gas Permeability,” Cement and Concrete Composites, V. 32, No. 10, 2010, pp. 749-756. doi: 10.1016/j.cemconcomp.2010.08.006

19. Liu, B.; Luo, G.; and Xie, Y., “Effect of Curing Conditions on the Permeability of Concrete with High Volume Mineral Admixtures,” Construction and Building Materials, V. 167, 2018, pp. 359-371. doi: 10.1016/j.conbuildmat.2018.01.190

20. Yu, Z., and Ye, G., “The Pore Structure of Cement Paste Blended with Fly Ash,” Construction and Building Materials, V. 45, 2013, pp. 30-35. doi: 10.1016/j.conbuildmat.2013.04.012

21. Zhang, J.; Zhang, P.; Wu, J.; Feng, X. X.; Bian, F.; and Zhang, Y. R., “Time-Dependent Correlation between Micro-Structural Parameters and Gas Permeability of Concrete in A Natural Tidal Environment,” Construction and Building Materials, V. 205, 2019, pp. 475-485. doi: 10.1016/j.conbuildmat.2019.01.200

22. Das, B. B., and Kondraivendhan, B., “Implication of Pore Size Distribution Parameters on Compressive Strength, Permeability and Hydraulic Diffusivity of Concrete,” Construction and Building Materials, V. 28, No. 1, 2012, pp. 382-386. doi: 10.1016/j.conbuildmat.2011.08.055

23. Zhu, J.; Zhang, R.; Zhang, Y.; and He, F., “The Fractal Characteristics of Pore Size Distribution in Cement-Based Materials and Its Effect on Gas Permeability,” Scientific Reports, V. 9, No. 1, 2012, pp. 1-12.

24. Sakai, Y., “Correlations Between Air Permeability Coefficients and Pore Structure Indicators of Cementitious Materials,” Construction and Building Materials, V. 209, 2019, pp. 541-547. doi: 10.1016/j.conbuildmat.2019.03.068

25. Güneyisi, E.; Gesoğlu, M.; Booya, E.; and Mermerdas, K., “Strength and Permeability Properties of Self-Compacting Concrete with Cold Bonded Fly Ash Lightweight Aggregate,” Construction and Building Materials, V. 74, 2015, pp. 17-24. doi: 10.1016/j.conbuildmat.2014.10.032

26. Zhang, X. T.; Li, Z.; Ma, Q.; and Zhou, X. C., “Study on The Correlation between SHPC Pore Structure and Air Permeability,” Tehnicki Vjesnik (Strojarski Fakultet), V. 24, No. 5, 2017, pp. 1425-1430.

27. Liu, L.; He, Z.; Cai, X.; and Fu, S., “Application of Low-Field NMR to The Pore Structure of Concrete,” Applied Magnetic Resonance, V. 52, No. 1, 2021, pp. 15-31. doi: 10.1007/s00723-020-01229-7

28. Zhou, C. S.; Ren, F. Z.; Wang, Z. D.; Chen, W.; and Wang, W., “Why Permeability to Water is Anomalously Lower than That to Many Other Fluids for Cement-Based Material?” Cement and Concrete Research, V. 100, 2017, pp. 373-384. doi: 10.1016/j.cemconres.2017.08.002

29. RILEM TC 116-PCD, “Test for Gas Permeability of Concrete,” Materials and Structures, V. 32, No. 3, 1999, pp. 176-178. doi: 10.1007/BF02481511

30. Boel, V.; Audenaert, K.; and de Schutter, G., “Gas Permeability and Capillary Porosity of Self-Compacting Concrete,” Materials and Structures, V. 41, No. 7, 2008, pp. 1283-1290. doi: 10.1617/s11527-007-9326-x

31. Guo, L., “Research of Influence of Mineral Admixtures on Permeability of Concrete,” master’s thesis, Harbin Institute of Technology, Harbin, China, 2010. (in Chinese)

32. Jain, R. B., “A Recursive Version of Grubbs’ Test for Detecting Multiple Outliers in Environmental and Chemical Data,” Clinical Biochemistry, V. 43, No. 12, 2010, pp. 1030-1033. doi: 10.1016/j.clinbiochem.2010.04.071

33. Choi, Y. C.; Kim, J.; and Choi, S., “Mercury Intrusion Porosimetry Characterization of Micropore Structures of High-Strength Cement Pastes Incorporating High Volume Ground Granulated Blast-Furnace Slag,” Construction and Building Materials, V. 137, 2017, pp. 96-103. doi: 10.1016/j.conbuildmat.2017.01.076

34. Algin, Z., and Ozen, M., “The Properties of Chopped Basalt Fibre Reinforced Self-Compacting Concrete,” Construction and Building Materials, V. 186, 2018, pp. 678-685. doi: 10.1016/j.conbuildmat.2018.07.089

35. Sogbossi, H.; Verdier, J.; and Multon, S., “New Approach for the Measurement of Gas Permeability and Porosity Accessible to Gas in Vacuum and Under Pressure,” Cement and Concrete Composites, V. 103, 2019, pp. 59-70. doi: 10.1016/j.cemconcomp.2019.04.032

36. Kameche, Z. A.; Ghomari, F.; Choinska, M.; and Khelidj, A., “Assessment of Liquid Water and Gas Permeabilities of Partially Saturated Ordinary Concrete,” Construction and Building Materials, V. 65, 2014, pp. 551-565. doi: 10.1016/j.conbuildmat.2014.04.137

37. Zhang, J. Z.; Zhou, X. Y.; Zhang, Y.; Wang, M.; and Zhang, Y. R., “Stable Process of Concrete Chloride Diffusivity and Corresponding Influencing Factors Analysis,” Construction and Building Materials, V. 261, 2020, p. 119994. doi: 10.1016/j.conbuildmat.2020.119994

38. Yu, Z. Y.; Chen, Y.; Liu, P.; and Wang, W. L., “Accelerated Simulation of Chloride Ingress into Concrete under Drying-Wetting Alternation Condition Chloride Environment,” Construction and Building Materials, V. 93, 2015, pp. 205-213. doi: 10.1016/j.conbuildmat.2015.05.090

39. Khan, M. I., “Permeation of High-Performance Concrete,” Journal of Materials in Civil Engineering, ASCE, V. 15, No. 1, 2003, pp. 84-92. doi: 10.1061/(ASCE)0899-1561(2003)15:1(84)

40. Guo, Y.; Hu, X.; and Lv, J., “Experimental Study on the Resistance of Basalt Fibre-reinforced Concrete to Chloride Penetration,” Construction and Building Materials, V. 223, 2019, pp. 142-155. doi: 10.1016/j.conbuildmat.2019.06.211

41. Song, H. W.; Pack, S. W.; Nam, S. H.; Jang, J. C.; and Saraswathy, V., “Estimation of the Permeability of Silica Fume Cement Concrete,” Construction and Building Materials, V. 24, No. 3, 2010, pp. 315-321. doi: 10.1016/j.conbuildmat.2009.08.033

42. Yu, Z.; Ni, C.; Tang, M.; and Shen, X., “Relationship Between Water Permeability and Pore Structure of Portland Cement Paste Blended with Fly Ash,” Construction and Building Materials, V. 175, 2018, pp. 458-466. doi: 10.1016/j.conbuildmat.2018.04.147

43. Yokoyama, Y.; Yokoi, T.; and Ihara, J. I., “The Effects of Pore Size Distribution and Working Techniques on The Absorption and Water Content of Concrete Floor Slab Surfaces,” Construction and Building Materials, V. 50, 2014, pp. 560-566. doi: 10.1016/j.conbuildmat.2013.10.013


ALSO AVAILABLE IN:

Electronic Materials Journal