Title: Corrosion Propagation in Cracked and Uncracked Prestressed Piles

Author(s): Mohammad A. Khawaja, Kwangsuk Suh, Venkat Bhethanabotla, and Rajan Sen

Publication: Materials Journal

Volume: 119

Issue: 5

Appears on pages(s): 103-118

Keywords: corrosion propagation; engineering practice; oxygen permeation; prestressed concrete; service life; similitude; uncracked.

DOI: 10.14359/51735950

Date: 9/1/2022

Abstract:
This paper presents results from a comprehensive, cradle-to-grave study in which electrochemical measurements (corrosion potential and corrosion rate), crack progression, and gravimetric metal loss were recorded for one-third-scale Class V prestressed specimens exposed for over 3 years to a simulated outdoor marine environment. These data were used to isolate the effect of cracking on the corrosion rate and determine the appropriate oxygen permeation coefficient values that were used to quantify the differences in corrosion propagation between the cracked and uncracked states. The permeation coefficient in cracked sections was found to be more than 20 times larger than that in uncracked ones. It was also higher than that for reinforced concrete specimens under comparable wetting-and-drying saltwater exposure. The findings predict that comparable (Class V) full-size prestressed pile specimens will crack within 3 years of the destruction of the passive layer (depassivation).

Related References:

1. Neville, A. M., Properties of Concrete, fifth edition, Pearson Education Limited, London, UK, 2011.

2. ACI Committee 224, “Control of Cracking in Concrete Structures (ACI 224R-01) (Reapproved 2008),” American Concrete Institute, Farmington Hills, MI, 2001, 46 pp.

3. ACI Committee 222, “Guide to Design and Construction Practices to Mitigate Corrosion of Reinforcement in Concrete Structures (ACI 222.3R-11),” American Concrete Institute, Farmington Hills, MI, 2011, 28 pp.

4. Tuutti, K., “Corrosion of Steel in Concrete,” Swedish Cement and Concrete Research Institute, Stockholm, Sweden, 1982, 473 pp.

5. Bertolini, L.; Elsener, B.; Pedeferri, P.; and Polder, R., Corrosion of Steel in Concrete: Prevention, Diagnosis, Repair, Wiley-VCH Verlag GmbH & Co. KGaA, Weinheim, Germany, 2004.

6. Jamali, A.; Angst, U.; Adey, B.; and Elsener, B., “Modeling of Corrosion-Induced Concrete Cover Cracking: A Critical Analysis,” Construction and Building Materials, V. 42, May 2013, pp. 225-237. doi: 10.1016/j.conbuildmat.2013.01.019

7. Crank, J., The Mathematics of Diffusion, second edition, Brunel University Uxbridge, Oxford University Press, Oxford, UK, 1975, 421 pp.

8. Käthler, C. B.; Angst, U. M.; Hornbostel, K.; and Elsener, B., “Critical Analysis of Experiments on Reinforcing Bar Corrosion in Cracked Concrete,” ACI Materials Journal, V. 117, No. 3, May 2020, pp. 145-154.

9. Ali, M. S.; Ji, C.; and Mirza, M. S., “Durable Design of Reinforced Concrete Elements against Corrosion,” Construction and Building Materials, V. 93, Sept. 2015, pp. 317-325. doi: 10.1016/j.conbuildmat.2015.05.011

10. Cui, Z., and Alipour, A., “Concrete Cover Cracking and Service Life Prediction of Reinforced Concrete Structures in Corrosive Environments,” Construction and Building Materials, V. 159, Jan. 2018, pp. 652-671. doi: 10.1016/j.conbuildmat.2017.03.224

11. Suh, K., “Underwater FRP Repair of Corrosion Damaged Prestressed Piles,” PhD dissertation, Department of Civil and Environmental Engineering, University of South Florida, Tampa, FL, 2006, 231 pp.

12. Suh, K.; Mullins, G.; Sen, R.; and Winters, D., “Effectiveness of Fiber-Reinforced Polymer in Reducing Corrosion in Marine Environment,” ACI Structural Journal, V. 104, No. 1, Jan.-Feb. 2007, pp. 76-83.

13. Khawaja, M. A.; Sen, R.; and Bhethanabotla, V., “Predictive Framework for FRP-Concrete Corrosion Repair,” Journal of Composites for Construction, ASCE, V. 24, No. 6, Dec. 2020, p. 04020068. doi: 10.1061/(ASCE)CC.1943-5614.0001082

14. Khoe, C.; Sen, R.; and Bhethanabotla, V. R., “Oxygen Permeability of FRP-Concrete Repair Systems,” Journal of Composites for Construction, ASCE, V. 16, No. 3, June 2012, pp. 277-285. doi: 10.1061/(ASCE)CC.1943-5614.0000257

15. Broomfield, J. P., Corrosion of Steel in Concrete: Understanding, Investigation and Repair, E&FN Spon, London, UK, 1997, 296 pp.

16. Lorentz, T., and French, C., “Corrosion of Reinforcing Steel in Concrete: Effects of Materials, Mix Composition, and Cracking,” ACI Materials Journal, V. 92, No. 2, Mar.-Apr. 1995, pp. 181-190.

17. Mohammed, T. U.; Otsuki, N.; and Hamada, H., “Corrosion of Steel Bars in Cracked Concrete under Marine Environment,” Journal of Materials in Civil Engineering, ASCE, V. 15, No. 5, Oct. 2003, pp. 460-469. doi: 10.1061/(ASCE)0899-1561(2003)15:5(460)

18. ASTM C876-15, “Standard Test Method for Corrosion Potentials of Uncoated Reinforcing Steel in Concrete,” ASTM International, West Conshohocken, PA, 2015, 8 pp.

19. ASTM G1-03, “Standard Practice for Preparing, Cleaning, and Evaluating Corrosion Test Specimens,” ASTM International, West Conshohocken, PA, 2003, 9 pp.

20. Misra, S., and Uomoto, T., “Reinforcement Corrosion under Simultaneous Diverse Exposure Conditions,” Durability of Concrete: Second International Conference – Montreal, Canada 1991, SP-126, V. M. Malhotra, ed., American Concrete Institute, Farmington Hills, MI, 1991, pp. 423-441.

21. Sagüés, A. A.; Kranc, S. C.; Presuel-Moreno, F.; Rey, D.; Torres-Acosta, A.; and Yao, L., “Corrosion Forecasting for 75-Year Durability Design of Reinforced Concrete,” Report No. BA502, University of South Florida, Tampa, FL, 2001, 175 pp.

22. Khawaja, M. A., “Corrosion Rate Prediction in FRP-Concrete Repair,” PhD dissertation, Department of Civil and Environmental Engineering, University of South Florida, Tampa, FL, 2021.

23. Khoe, C.; Chowdhury, S.; Bhethanabotla, V. R.; and Sen, R., “Measurement of Oxygen Permeability of Epoxy Polymers,” ACI Materials Journal, V. 107, No. 2, Mar.-Apr. 2010, pp. 138-146.

24. Al Azzawi, M.; Hopkins, P.; Mullins, G.; and Sen, R., “FRP–Concrete Bond after 12-Year Exposure in Tidal Waters,” Journal of Composites for Construction, ASCE, V. 22, No. 5, Oct. 2018, p. 04018031. doi: 10.1061/(ASCE)CC.1943-5614.0000864

25. Li, C. Q. “Reliability Based Service Life Prediction of Corrosion Affected Concrete Structures,” Journal of Structural Engineering, ASCE, V. 130, No. 10, Oct. 2004, pp. 1570-1578.

26. Torres-Acosta, A. A., and Sagüés, A. A., “Concrete Cracking by Localized Steel Corrosion—Geometric Effects,” ACI Materials Journal, V. 101, No. 6, Nov.-Dec. 2004, pp. 501-507.

27. Lau, K.; Sagüés, A. A.; and Powers, R. G., “Corrosion of Epoxy-Coated Rebar in Marine Bridges—Part 2: Corrosion in Cracked Concrete,” Corrosion, V. 66, No. 6, June 2010, pp. 065002-065002-16.


ALSO AVAILABLE IN:

Electronic Materials Journal