Post-Fire Assessment and Retrofitting of Concrete Buildings: Case Study

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Post-Fire Assessment and Retrofitting of Concrete Buildings: Case Study

Author(s): A. Gil, V. Kodur, F. Pacheco, D. Schneider, R. Christ, and B. Tutikian

Publication: Structural Journal

Volume: 119

Issue: 5

Appears on pages(s): 57-67

Keywords:

DOI: 10.14359/51734898

Date: 9/1/2022

Abstract:
Reinforced concrete structures possess good fire-resistance properties and rarely experience failure during a fire incident. However, following a fire incident, proper post-fire assessment and repair of the structure may be needed for rehabilitation of the building. This paper presents the application of the X-ray diffraction technique in the analysis of powder samples extracted from concrete members for the estimation of sectional temperatures reached in a real fire incident. Using these sectional temperatures, a simplified evaluation approach was applied for evaluating the residual capacity of structural members in a fire-damaged building. Results of the analysis showed a reduction of 30% and 27% of beam and column capacity after exposure to a fire incident, respectively. Based on the analysis, recommendations were made for rehabilitating the fire-damaged building to meet current design code specifications.

Related References:

1. Kodur, V. K. R., and Naser, M. Z., Structural Fire Engineering, McGraw Hill, New York, NY, 2020.

2. Ni, S., and Gernay, T., “Predicting Residual Deformations in a Reinforced Concrete Building Structure after a Fire Event,” Engineering Structures, V. 202, Jan. 2020, Article No. 109853. doi: 10.1016/j.engstruct.2019.109853

3. Kodur, V. K. R., and Agrawal, A., “Effect of Temperature Induced Bond Degradation on Fire Response of Reinforced Concrete Beams,” Engineering Structures, V. 142, July 2017, pp. 98-109. doi: 10.1016/j.engstruct.2017.03.022

4. Nassif, A., “Postfire Full Stress–Strain Response of Fire-Damaged Concrete,” Fire and Materials, V. 30, No. 5, 2006, pp. 323-332. doi: 10.1002/fam.911

5. Neves, I. C.; Rodrigues, J. P. C.; and Loureiro, A. P., “Mechanical Properties of Reinforcing and Prestressing Steels after Heating,” Journal of Materials in Civil Engineering, ASCE, V. 8, No. 4, 1996, pp. 189-194. doi: 10.1061/(ASCE)0899-1561(1996)8:4(189)

6. Alogla, S., and Kodur, V. K. R., “Quantifying Transient Creep Effects on Fire Response of Reinforced Concrete Columns,” Engineering Structures, V. 174, 2018, pp. 885-895. doi: 10.1016/j.engstruct.2018.07.093

7. Felicetti, R.; Gambarova, P. G.; and Meda, A., “Residual Behavior of Steel Rebars and R/C Sections after a Fire,” Construction and Building Materials, V. 23, No. 12, 2009, pp. 3546-3555. doi: 10.1016/j.conbuildmat.2009.06.050

8. Khoury, G. A., “Compressive Strength of Concrete at High Temperatures: A Reassessment,” Magazine of Concrete Research, V. 44, No. 161, 1992, pp. 291-309. doi: 10.1680/macr.1992.44.161.291

9. Garlock, M.; Paya-Zaforteza, I.; Kodur, V.; and Gu, L., “Fire Hazard in Bridges: Review, Assessment and Repair Strategies,” Engineering Structures, V. 35, Feb. 2012, pp. 89-98. doi: 10.1016/j.engstruct.2011.11.002

10. Agrawal, A., and Kodur, V. K. R., “A Novel Experimental Approach for Evaluating Residual Capacity of Fire Damaged Concrete Members,” Fire Technology, V. 56, No. 2, Mar. 2020, pp. 715-735. doi: 10.1007/s10694-019-00900-1

11. Dwaikat, M. B., and Kodur, V. K. R., “Hydrothermal Model for Predicting Fire-Induced Spalling in Concrete Structural Systems,” Fire Safety Journal, V. 44, No. 3, 2009, pp. 425-434. doi: 10.1016/j.firesaf.2008.09.001

12. Hager, I., “Colour Change in Heated Concrete,” Fire Technology, V. 50, No. 4, July 2014, pp. 945-958.

13. fib Bulletin No. 46, “Fire Design of Concrete Structures - Structural Behavior and Assessment,” Fédération internationale du béton, Lausanne, Switzerland, 2008, 214 pp.

14. PCI MNL 124, “Design for Fire Resistance of Precast/Prestressed Concrete,” Precast/Prestressed Concrete Institute, Chicago, IL, 1997.

15. Kodur, V. K. R., and Agrawal, A., “Estimating Postfire Residual Capacity of Heavily Damaged Concrete Members,” Journal of Performance of Constructed Facilities, ASCE, V. 35, No. 2, 2021, p. 04020151. doi: 10.1061/(ASCE)CF.1943-5509.0001561

16. Castellote, M.; Alonso, C.; Andrade, C.; Turrillas, X.; and Campo, J., “Composition and Microstructural Changes of Cement Pastes upon Heating, as Studied by Neutron Diffraction,” Cement and Concrete Research, V. 34, No. 9, 2004, pp. 1633-1644. doi: 10.1016/S0008-8846(03)00229-1

17. Hager, I., “Behaviour of Cement Concrete at High Temperature,” Bulletin of the Polish Academy of Sciences: Technical Sciences, V. 61, No. 1, 2013, pp. 145-154. doi: 10.2478/bpasts-2013-0013

18. fib Bulletin No. 38, “Fire Design of Concrete Structures - Materials, Structures and Modelling,” Fédération internationale du béton, Lausanne, Switzerland, 2007, 106 pp.

19. Missemer, L.; Ouedraogo, E.; Malecot, Y.; Clergue, C.; and Rogat, D., “Fire Spalling of Ultra-High Performance Concrete: From a Global Analysis to Microstructure Investigations,” Cement and Concrete Research, V. 115, Jan. 2019, pp. 207-219. doi: 10.1016/j.cemconres.2018.10.005

20. Fernandes, B.; Gil, A. M.; Bolina, F. L.; and Tutikian, B. F., “Microstructure of Concrete Subjected to Elevated Temperatures: Physico-Chemical Changes and Analysis Techniques,” Revista IBRACON de Estruturas e Materiais, V. 10, No. 4, 2017, pp. 838-863. doi: 10.1590/s1983-41952017000400004

21. Handoo, S. K.; Agarwal, S.; and Agarwal, S. K., “Physicochemical, Mineralogical, and Morphological Characteristics of Concrete Exposed to Elevated Temperatures,” Cement and Concrete Research, V. 32, No. 7, 2002, pp. 1009-1018. doi: 10.1016/S0008-8846(01)00736-0

22. Peng, G.-F., and Huang, Z.-S., “Change in Microstructure of Hardened Cement Paste Subjected to Elevated Temperatures,” Construction and Building Materials, V. 22, No. 4, 2008, pp. 593-599. doi: 10.1016/j.conbuildmat.2006.11.002

23. Kim, K. Y.; Yun, T. S.; and Park, K. P., “Evaluation of Pore Structures and Cracking in Cement Paste Exposed to Elevated Temperatures by X-Ray Computed Tomography,” Cement and Concrete Research, V. 50, Aug. 2013, pp. 34-40. doi: 10.1016/j.cemconres.2013.03.020

24. Lim, S., and Mondal, P., “Micro- and Nano-Scale Characterization to Study the Thermal Degradation of Cement-Based Materials,” Materials Characterization, V. 92, June 2014, pp. 15-25. doi: 10.1016/j.matchar.2014.02.010

25. EN 1994-1-2:2005, “Eurocode 4: Design of Composite Steel and Concrete Structures - Part 1-2: General Rules—Structural Fire Design,” European Committee for Standardization, Brussels, Belgium, 2005, 111 pp.

26. Kodur, V. K. R., and Agrawal, A., “An Approach for Evaluating Residual Capacity of Reinforced Concrete Beams Exposed to Fire,” Engineering Structures, V. 110, Mar. 2016, pp. 293-306. doi: 10.1016/j.engstruct.2015.11.047

27. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19),” American Concrete Institute, Farmington Hills, MI, 2019, 624 pp.

28. ASTM C42/C42M-20, “Standard Test Method for Obtaining and Testing Drilled Cores and Sawed Beams of Concrete,” ASTM International, West Conshohocken, PA, 2020, 7 pp.


ALSO AVAILABLE IN:

Electronic Structural Journal