Structure and Properties of Alkali-Silica Reaction Gels Treated with Lithium Nitrate

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Structure and Properties of Alkali-Silica Reaction Gels Treated with Lithium Nitrate

Author(s): Jianqiang Wei

Publication: Web Session

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 10/17/2021

Abstract:
Alkali-silica reaction (ASR) is a deleterious reaction between reactive silica in aggregates and the alkaline pore solution of concrete. The reaction forms hygroscopic ASR gels, which can absorb water, swell, and exert pressure on surrounding concrete, causing internal stresses, volume expansion, and cracking of concrete. Mixing lithium admixtures in fresh concrete has been proven as an effective ASR mitigation approach at the concrete level. However, the exact mechanism has not been fully understood. Moreover, the morphology, chemical composition and properties of ASR gels might vary with their age and forming location in concrete. To uncover the role of lithium in mitigating ASR, synthetic ASR gels containing various dosages of lithium nitrate admixture were prepared. Microstructure, composition, and crystallization of ASR gels in the presence of lithium were investigated through microscopy, spectrographic, and X-ray diffraction techniques. Physical and mechanical properties, such as water absorption, swelling and strength development, were also studied through vapor sorption, weight, static volume change and compressive strength tests, respectively. The results indicate that the gelation time of ASR gels was extended significantly. The swelling, stiffness, and strength of ASR gels were also decreased in the presence of lithium.