Title: Pavement Concrete Thickness Study

Author(s): Tim Manherz

Publication: Web Session

Volume: ws_S22_Manherz.pdf

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 3/28/2022

Abstract:
Discusses factors that affect the elevation of the top and bottom surfaces. Compares differences in level, sloped and warped slab-on-grade paving. Presents data collection methodology for slab-on-grade thickness for parking lot projects collected for ACI 330.