Experimental Study to Predict Bond-Slip Behavior of Corroded Reinforced Concrete Columns

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Experimental Study to Predict Bond-Slip Behavior of Corroded Reinforced Concrete Columns

Author(s): Hakan Yalciner and Atila Kumbasaroglu

Publication: Structural Journal

Volume: 119

Issue: 5

Appears on pages(s): 111-128

Keywords:

DOI: 10.14359/51734795

Date: 9/1/2022

Abstract:
To perform accurate seismic analyses of corroded reinforced concrete (RC) buildings, it is necessary to predict the bond-slip relationships to modify the moment-curvature relationships. In this study, empirical models were developed to predict the bond strength of corroded RC columns. Twenty-five RC columns were tested under combined cyclic lateral displacement excursions for three concrete strength levels—specifically, 9, 27, and 37 MPa (1305, 3915, and 5365 psi, respectively)—at two axial load ratios of 0.20 and 0.40 and at four corrosion levels. An accelerated corrosion method was applied to corrode the reinforcing bars embedded in the RC columns. The actual corrosion levels were determined by breaking the concrete and extracting all the longitudinal and transverse reinforcing bars from the RC columns. Three empirical models were developed. The first model was used to predict the development length of the corroded reinforcing bars. The second and third models were used to predict the bond strength and slip in the reinforcing bars as a function of the corrosion levels. The results indicated that previous models that predict the bond strength of corroded RC members were limited because of the theoretically considered development length of the noncorroded reinforcing bars.

Related References:

ACI Committee 318, 2002, “Building Code Requirements for Structural Concrete (ACI 318-02) and Commentary (ACI 318R-02),” American Concrete Institute, Farmington Hills, MI, 443 pp.

ACI Committee 318, 2008, “Building Code Requirements for Structural Concrete (ACI 318-08) and Commentary (ACI 318R-08),” American Concrete Institute, Farmington Hills, MI, 473 pp.

ACI Committee 318, 2019, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19),” American Concrete Institute, Farmington Hills, MI, 624 pp.

ACI Committee 408, 1979, “Suggested Development, Splice, and Standard Hook Provisions for Deformed Bars in Tension (ACI 408.1R-79),” Concrete International, V. 1, No. 7, July, pp. 44-46.

Alsiwat, J. M., and Saatcioglu, M., 1992, “Reinforcement Anchorage Slip under Monotonic Loading,” Journal of Structural Engineering, ASCE, V. 118, No. 9, pp. 2421-2438. doi: 10.1061/(ASCE)0733-9445(1992)118:9(2421)

ASTM G1-03, 2003, “Standard Practice for Preparing, Cleaning, and Evaluating Corrosion Test Specimens,” ASTM International, West Conshohocken, PA, 9 pp.

Auyeung, Y.; Balaguru, P.; and Chung, L., 2000, “Bond Behavior of Corroded Reinforcement Bars,” ACI Materials Journal, V. 97, No. 2, Mar.-Apr., pp. 214-221. doi: 10.14359/826

Azad, A. K.; Ahmad, S.; and Al-Gohi, B. H. A., 2010, “Flexural Strength of Corroded Reinforced Concrete Beams,” Magazine of Concrete Research, V. 62, No. 6, pp. 405-414. doi: 10.1680/macr.2010.62.6.405

Bhargava, K.; Ghosh, A. K.; Mori, Y.; and Ramanujam, S., 2008, “Suggested Empirical Models for Corrosion-Induced Bond Degradation in Reinforced Concrete,” Journal of Structural Engineering, ASCE, V. 134, No. 2, pp. 221-230. doi: 10.1061/(ASCE)0733-9445(2008)134:2(221)

Bicer, K.; Yalciner, H.; Balkıs, A. P.; and Kumbasaroglu, A., 2018, “Effect of Corrosion on Flexural Strength of Reinforced Concrete Beams with Polypropylene Fibers,” Construction and Building Materials, V. 185, pp. 574-588. doi: 10.1016/j.conbuildmat.2018.07.021

Cabrera, J. G., 1996, “Deterioration of Concrete due to Reinforcement Steel Corrosion,” Cement and Concrete Composites, V. 18, No. 1, pp. 47-59. doi: 10.1016/0958-9465(95) 00043-710.1016/0958-9465(95)

Çağatay, İ. H., 2005, “Experimental Evaluation of Buildings Damaged in Recent Earthquakes in Turkey,” Engineering Failure Analysis, V. 12, No. 3, pp. 440-452. doi: 10.1016/j.engfailanal.2004.02.007

Chang, J. J., 2002, “A Study of the Bond Degradation of Rebar due to Cathodic Protection Current,” Cement and Concrete Research, V. 32, No. 4, pp. 657-663. doi: 10.1016/S0008-8846(01)00740-2

Chang, J. J., 2003, “Bond Degradation due to the Desalination Process,” Construction and Building Materials, V. 17, No. 4, pp. 281-287. doi: 10.1016/S0950-0618(02)00113-7

Cheng, H.; Li, H.-N.; and Wang, D.-S., 2018, “Prediction for Lateral Deformation Capacity of Corroded Reinforced Concrete Columns,” The Structural Design of Tall and Special Buildings, V. 28, No. 1, Article No. e1560, 15 pp. doi: 10.1002/tal.1560

Chung, L.; Cho, S.-H.; Kim, J.-H. J.; and Yi, S.-T., 2004, “Correction Factor Suggestion for ACI Development Length Provisions Based on Flexural Testing of RC Slabs with Various Levels of Corroded Reinforcing Bars,” Engineering Structures, V. 26, No. 8, pp. 1013-1026. doi: 10.1016/j.engstruct.2004.01.008

Chung, L.; Kim, J.-H. J.; and Yi, S.-T., 2008, “Bond Strength Prediction for Reinforced Concrete Members with Highly Corroded Reinforcing Bars,” Cement and Concrete Composites, V. 30, No. 7, pp. 603-611. doi: 10.1016/j.cemconcomp.2008.03.006

Di Carlo, F.; Meda, A.; and Rinaldi, Z., 2017, “Numerical Evaluation of the Corrosion Influence on the Cyclic Behaviour of RC Columns,” Engineering Structures, V. 153, pp. 264-278. doi: 10.1016/j.engstruct.2017.10.020

El Maaddawy, T.; Soudki, K.; and Topper, T., 2005, “Long-Term Performance of Corrosion-Damaged Reinforced Concrete Beams,” ACI Structural Journal, V. 102, No. 5, Sept.-Oct., pp. 649-656. doi: 10.14359/14660

Fang, C.; Lundgren, K.; Chen, L.; and Zhu, C., 2004, “Corrosion Influence on Bond in Reinforced Concrete,” Cement and Concrete Research, V. 34, No. 11, pp. 2159-2167. doi: org/10.1016/j.cemconres.2004.04.00610.1016/j.cemconres.2004.04.006

FEMA 461, 2007, “Interim Testing Protocols for Determining the Seismic Performance Characteristics of Structural and Nonstructural Components,” Federal Emergency Management Agency, Washington, DC, 138 pp.

Guo, A.; Li, H.; Ba, X.; Guan, X.; and Li, H., 2015, “Experimental Investigation on the Cyclic Performance of Reinforced Concrete Piers with Chloride-Induced Corrosion in Marine Environment,” Engineering Structures, V. 105, pp. 1-11. doi: 10.1016/j.engstruct. 2015.09.03110.1016/j.engstruct

Imam, A., and Azad, A. K., 2016, “Prediction of Residual Shear Strength of Corroded Reinforced Concrete Beams,” International Journal of Advanced Structural Engineering, V. 8, No. 3, pp. 307-318. doi: 10.1007/s40091-016-0133-x

Jnaid, F., and Aboutaha, R. S., 2016, “Residual Flexural Strength of Corroded Reinforced Concrete Beams,” Engineering Structures, V. 119, pp. 198-216. doi: 10.1016/j.engstruct. 2016.04.01810.1016/j.engstruct

Joshi, J.; Arora, H. C.; and Sharma, U. K., 2015, “Structural Performance of Differently Confined and Strengthened Corroding Reinforced Concrete Columns,” Construction and Building Materials, V. 82, pp. 287-295. doi: 10.1016/j.conbuildmat.2015.02.056

Lee, H.-S.; Noguchi, T.; and Tomosawa, F., 2002, “Evaluation of the Bond Properties between Concrete and Reinforcement as a Function of the Degree of Reinforcement Corrosion,” Cement and Concrete Research, V. 32, No. 8, pp. 1313-1318. doi: 10.1016/S0008-8846(02)00783-4

Lehman, D. E., and Moehle, J. P., 2000, “Seismic Performance of Well-Confined Concrete Bridge Columns,” PEER Report 1998/01, Pacific Earthquake Engineering Research Center, University of California, Berkeley, Berkeley, CA, 316 pp.

Li, C. Q.; Zheng, J. J.; Lawanwisut, W.; and Melchers, R. E., 2007, “Concrete Delamination Caused by Steel Reinforcement Corrosion,” Journal of Materials in Civil Engineering, ASCE, V. 19, No. 7, pp. 591-600. doi: 10.1061/(ASCE)0899-1561(2007)19:7(591)

Li, D.; Wei, R.; Xing, F.; Sui, L.; Zhou, Y.; and Wang, W., 2018, “Influence of Non-Uniform Corrosion of Steel Bars on the Seismic Behavior of Reinforced Concrete Columns,” Construction and Building Materials, V. 167, pp. 20-32. doi: 10.1016/j. conbuildmat.2018.01.149

Lowes, L. N., and Altoontash, A., 2003, “Modeling Reinforced-Concrete Beam-Column Joints Subjected to Cyclic Loading,” Journal of Structural Engineering, ASCE, V. 129, No. 12, pp. 1686-1697. doi: 10.1061/(ASCE)0733-9445(2003)129:12(1686)

Ma, Y.; Che, Y.; and Gong, J., 2012, “Behavior of Corrosion Damaged Circular Reinforced Concrete Columns under Cyclic Loading,” Construction and Building Materials, V. 29, pp. 548-556. doi: 10.1016/j.conbuildmat.2011.11.002

Meda, A.; Mostosi, S.; Rinaldi, Z.; and Riva, P., 2014, “Experimental Evaluation of the Corrosion Influence on the Cyclic Behaviour of RC Columns,” Engineering Structures, V. 76, pp. 112-123. doi: 10.1016/j.engstruct.2014.06.043

Melek, M.; Wallace, J. W.; and Conte, J. P., 2003, “Experimental Assessment of Columns with Short Lap Splices Subjected to Cyclic Loads,” PEER Report 2003/04, Pacific Earthquake Engineering Research Center, University of California, Berkeley, Berkeley, CA, 192 pp.

Otani, S., and Sozen, M. A., 1972, “Behavior of Multistory Reinforced Concrete Frames During Earthquakes,” Structural Research Series No. 392, University of Illinois Engineering Experiment Station, University of Illinois at Urbana-Champaign, Urbana, IL, 551 pp.

Ou, Y.-C., and Nguyen, N. D., 2016, “Modified Axial-Shear-Flexure Interaction Approaches for Uncorroded and Corroded Reinforced Concrete Beams,” Engineering Structures, V. 128, pp. 44-54. doi: 10.1016/j.engstruct.2016.09.031

Park, R., and Paulay, T., 1975, Reinforced Concrete Structures, first edition, John Wiley & Sons, Inc., New York, NY, pp. 36-45.

Sezen, H., and Moehle, J. P., 2004, “Strength and Deformation Capacity of Reinforced Concrete Columns with Limited Ductility,” Proceedings of the 13th World Conference on Earthquake Engineering, Vancouver, BC, Canada, Paper No. 279, 15 pp.

Sezen, H., and Setzler, E. J., 2008, “Reinforcement Slip in Reinforced Concrete Columns,” ACI Structural Journal, V. 105, No. 3, May-June, pp. 280-289. doi: org/10.14359/1978710.14359/19787

Shimizu, Y.; Hirosawa, M.; and Zhou, J., 2000, “Statistical Analysis of Concrete Strength in Existing Reinforced Concrete Buildings in Japan,” Proceedings of the 12th World Conference on Earthquake Engineering, Auckland, New Zealand, Paper No. 1499, 8 pp.

Stanish, K.; Hooton, R. D.; and Pantazopoulou, S. J., 1999, “Corrosion Effects on Bond Strength in Reinforced Concrete,” ACI Structural Journal, V. 96, No. 6, Nov.-Dec., pp. 915-921.

Suffern, C.; El-Sayed, A.; and Soudki, K., 2010, “Shear Strength of Disturbed Regions with Corroded Stirrups in Reinforced Concrete Beams,” Canadian Journal of Civil Engineering, V. 37, No. 8, pp. 1045-1056. doi: 10.1139/L10-031

Tapan, M., and Aboutaha, R. S., 2011, “Effect of Steel Corrosion and Loss of Concrete Cover on Strength of Deteriorated RC Columns,” Construction and Building Materials, V. 25, No. 5, pp. 2596-2603. doi: 10.1016/j.conbuildmat.2010.12.003

Torres-Acosta, A. A.; Navarro-Gutierrez, S.; and Terán-Guillén, J., 2007, “Residual Flexure Capacity of Corroded Reinforced Concrete Beams,” Engineering Structures, V. 29, No. 6, pp. 1145-1152. doi: 10.1016/j.engstruct.2006.07.018

Vu, N. S.; Yu, B.; and Li, B., 2016, “Prediction of Strength and Drift Capacity of Corroded Reinforced Concrete Columns,” Construction and Building Materials, V. 115, pp. 304-318. doi: 10.1016/j.conbuildmat.2016.04.048

Wang, X.-H., and Liang, F.-Y., 2008, “Performance of RC Columns with Partial Length Corrosion,” Nuclear Engineering and Design, V. 238, No. 12, pp. 3194-3202. doi: 10.1016/j.nucengdes.2008.08.007

Yalciner, H., and Kumbasaroglu, A., 2020, “Experimental Evaluation and Modeling of Corroded Reinforced Concrete Columns,” ACI Structural Journal, V. 117, No. 4, July, pp. 61-76. doi: 10.14359/51721372

Yalciner, H.; Eren, O.; and Sensoy, S., 2012, “An Experimental Study on the Bond Strength between Reinforcement Bars and Concrete as a Function of Concrete Cover, Strength and Corrosion Level,” Cement and Concrete Research, V. 42, No. 5, pp. 643-655. doi: 10.1016/j.cemconres.2012.01.003

Yalciner, H.; Kumbasaroglu, A.; and Karimi, A., 2019, “Prediction of Seismic Performance Levels of Corroded Reinforced Concrete Columns as a Function of Crack Width,” Advances in Civil Engineering Materials, V. 8, No. 3, pp. 376-397. doi: 10.1520/ACEM20190035

Yalciner, H.; Kumbasaroglu, A.; El-Sayed, A. K.; Balkıs, A. P.; Dogru, E.; Turan, A. I.; Karimi, A.; Kohistani, R.; Mermit, M. F.; and Bicer, K., 2020, “Flexural Strength of Corroded Reinforced Concrete Beams,” ACI Structural Journal, V. 117, No. 1, Jan., pp. 29-41. doi: 10.14359/51720195

Yalciner, H.; Kumbasaroglu, A.; Ertuc, İ.; and Turan, A. İ., 2018, “Confinement Effect of Geo-Grid and Conventional Shear Reinforcement Bars Subjected to Corrosion,” Structures, V. 13, pp. 139-152. doi: 10.1016/j.istruc.2017.12.004

Yalciner, H.; Sensoy, S.; and Eren, O., 2015, “Seismic Performance Assessment of a Corroded 50-Year-Old Reinforced Concrete Building,” Journal of Structural Engineering, ASCE, V. 141, No. 12, p. 05015001. doi: 10.1061/(ASCE)ST.1943-541X.0001263

Yang, S.-Y.; Song, X.-B.; Jia, H.-X.; Chen, X.; and Liu, X.-L., 2016, “Experimental Research on Hysteretic Behaviors of Corroded Reinforced Concrete Columns with Different Maximum Amounts of Corrosion of Rebar,” Construction and Building Materials, V. 121, pp. 319-327. doi: 10.1016/j.conbuildmat.2016.06.002

Zhang, Y.; Bicici, E.; Sezen, H.; and Zheng, S., 2020, “Reinforcement Slip Model Considering Corrosion Effects,” Construction and Building Materials, V. 235, Article No. 117348, 14 pp. doi: 10.1016/j.conbuildmat.2019.117348

Zhao, Y.; Lin, H.; Wu, K.; and Jin, W., 2013, “Bond Behavior of Normal/Recycled Concrete and Corroded Steel Bars,” Construction and Building Materials, V. 48, pp. 348-359. doi: 10.1016/j.conbuildmat.2013.06.09