Non‐Proprietary Ultra‐High Performance Concrete for Precast Bridge Decks Field Joints

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Non‐Proprietary Ultra‐High Performance Concrete for Precast Bridge Decks Field Joints

Author(s): Moustafa

Publication: Web Session

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 10/17/2021

Abstract:
Using full‐depth precast deck panels and deck bulb tee girders (DBTs) is one of the most popular and reliable solutions nowadays for accelerated bridge construction (ABC). Precast panels and DBTs usually require to be connected on‐site using robust materials such as ultra‐high performance concrete (UHPC) for the field joints. The unparalleled mechanical properties of UHPC mixes have gained material popularity for ABC connections. The objective of this study is to leverage readily developed non‐proprietary UHPC mixes, but using local materials available in the western United States, and proof‐test it in precast deck panels transverse field joints and DBTs longitudinal field joints. The presentation provides an overview of a comprehensive experimental program where four full‐scale specimens of two representative bridge deck systems with UHPC field joints were tested under static vertical loading. The structural behavior of all specimens was evaluated in terms of load and deflection capacities as well as the field joint performance.