Title: Development and Testing of High/Ultra High Performance Concrete for Durable Bridge Components and Connections

Author(s): Wille

Publication: Web Session

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 10/17/2021

Abstract:
This presentation shares the development of a cost‐efficient, non‐proprietary ultra‐high performance concrete using local available materials from the New England area. Methods of investigation include spread test, compression and direct tensile tests, as well as surface resistivity, and strength development.