FRP Reinforced Concrete Around the World, Part 1

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: FRP Reinforced Concrete Around the World, Part 1

Author(s):

Publication: Concrete International

Volume: 44

Issue: 5

Appears on pages(s): 25-28

Keywords: bar, reinforcement, design, construction

DOI: 10.14359/51734736

Date: 5/1/2022

Abstract:
This two-part series discusses various activities taking place around the world to make the technology of fiber-reinforced polymer (FRP) reinforcement for concrete structures accessible to the construction industry. Part 1 focuses on initiatives for acceptance and implementation of FRP reinforcement in four countries: Brazil, Iran, Italy, and New Zealand.

Related References:

1. Cardoso, D.C.T.; Carnio, M.A.; Forti, N.C.S.; and Christ, R., “Recommended Practice IBRACON: Fiber-Reinforced Polymer (FRP) Reinforced Concrete Structures,” first edition, IBRACON, São Paulo, Brazil, 2021. (in production)

2. “Guide for the Design and Construction of Concrete Structures Reinforced with Fiber-Reinforced Polymer Bars,” CNR-DT 203/2006, CNR (National Research Council), Rome, Italy, 2007, 35 pp.

3. CAN/CSA S806-12, “Design and Construction of Building Structures with Fibre-Reinforced Polymers,” CSA Group, Toronto, ON, Canada, 2012, 198 pp.

4. ACI Committee 440, “Guide for the Design and Construction of Structural Concrete Reinforced with Fiber-Reinforced Polymer (FRP) Bars (ACI 440.1R-15),” American Concrete Institute, Farmington Hills, MI, 2015, 88 pp.

5. ASTM D7957/D7957M-17, “Standard Specification for Solid Round Glass Fiber Reinforced Polymer Bars for Concrete Reinforcement,” ASTM International, West Conshohocken, PA, 2017, 5 pp.

6. NORMA BRASILEIRA ABNT NBR 6118:2014, “Projeto de estruturas de concreto—Procedimiento (Design of Concrete Structures—Procedure),” Associação Brasileira de Normas Técnicas, Rio de Janeiro, Brazil, 2014, 256 pp. (in Portuguese)

7. He, Z., and Qiu, F., “Probabilistic Assessment on Flexural Capacity of GFRP-Reinforced Concrete Beams Designed by Guideline ACI 440.1 R-06,” Construction and Building Materials, V. 25, No. 4, 2011, pp. 1663-1670.

8. ACI Committee 440, “Guide for Test Methods for Fiber Reinforced Polymer (FRP) Composites for Reinforcing or Strengthening Concrete and Masonry Structures (ACI 440.3R-12),” American Concrete Institute, Farmington Hills, MI, 2012, 23 pp.

9. ISO 10406-1:2008, “Fibre-Reinforced Polymer (FRP) Reinforcement of Concrete—Test Methods—Part 1: FRP Bars and Grids,” International Organization for Standardization (ISO), Geneva, Switzerland, 2008, 40 pp.

10. Iranian National Building Codes Compilation Office, MMS9:2016, “Iranian National Building Code, Part 9: Reinforced Concrete Buildings Design,” Ministry of Housing and Urban Development (MHDU), Tehran, Iran, 2016.

11. fib Bulletin No. 40: “FRP Reinforcement in RC Structures,” International Federation for Structural Concrete (fib), Lausanne, Switzerland, 2007, 160 pp.

12. Aiello, M.A.; Ascione, L.; D’Antino, T.; Frassine, R.; Lignola, G.P.; Poggi, C.; and Prota, A., “Reinforced Concrete with FRP Bars: The Italian State of Technical Normative,” Structural, No. 237, Sept.-Oct. 2021, www.structuralweb.it/cms/it4-magazine.asp?pag=articoli.asp&idCopertina=105.