Non-Expandable Perlite Powder as Pozzolanic Addition in Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Non-Expandable Perlite Powder as Pozzolanic Addition in Concrete

Author(s): Michal Bacuvcík, Ján Mendel, and Ivan Janotka

Publication: Materials Journal

Volume: 119

Issue: 4

Appears on pages(s): 3-14

Keywords: carbonation; durability; k-value; perlite; pozzolan; utility property

DOI: 10.14359/51734681

Date: 7/1/2022

Abstract:
The main purpose of this research was to verify non-expandable powdered perlite (PP) for suitability as a Type II addition for use in concrete. The tests were carried out using CEM II/A-S 42.5 N. Pozzolanic reactivity was verified by the Frattini test. The suitability for use in concrete was assessed by considering the criteria of EN 450-1 as the limits of individual results necessary to be fulfilled for fly ash. If a standard is not issued for a pozzolan, it must be evaluated by the most closely related standard. Following this request, the k-value for PP required by EN 206+A2 and prescribed in TNI CEN/TR 16639 was determined. The k-value concept is based on the comparison of the durability performance for the relevant exposure class of a reference concrete with cement “A” against a test concrete, in which a part of cement “A” is replaced by an addition. This concept permits a defined range of combinations of cement conforming to EN 197-1 with a pozzolanic addition that may count fully toward requirements for the maximum water-cement ratio (w/c) and minimum cement content, which are specified for concrete. The TNI provides more detailed information on the principles of the equivalent performance concept and on the application of this concept in 12 European Committee for Standardization (CEN) member countries. This paper reveals the methodological and experimental procedures for the k-value determination for PP as well as the resistance to carbonation, which includes one important aspect of durability related to the exposure class XC—corrosion induced by carbonation. The novelty of this investigation consists of the presentation of the Slovak national procedure for determination of the k-value and the resistance to carbonation alongside those elaborated by Technical Committee CEN/TC 104, Concrete and Related Products. The results point to the fact that the unexpanded PP is a Type II addition suitable for use in concrete.

Related References:

1. Ramezanianpour, A. A.; Motahari Karein, S. M.; Vosoughi, P.; Pilvar, A.; Isapour, S.; and Moodi, F., “Effects of Calcined Perlite Powder as a SCM on the Strength and Permeability of Concrete,” Construction and Building Materials, V. 66, Sept. 2014, pp. 222-228. doi: 10.1016/j.conbuildmat.2014.05.086

2. Rashad, A. M., “A Synopsis about Perlite as Building Material – A Best Practice Guide for Civil Engineer,” Construction and Building Materials, V. 121, Sept. 2016, pp. 338-353. doi: 10.1016/j.conbuildmat.2016.06.001

3. Demirboğa, R.; Örüng, İ.; and Gül, R., “Effects of Expanded Perlite Aggregate and Mineral Admixtures on the Compressive Strength of Low-Density Concretes,” Cement and Concrete Research, V. 31, No. 11, Nov. 2001, pp. 1627-1632. doi: 10.1016/S0008-8846(01)00615-9

4. Türkmen, İ., and Kantarcı, A., “Effects of Expanded Perlite Aggregate and Different Curing Conditions on the Physical and Mechanical Properties of Self-Compacting Concrete,” Building and Environment, V. 42, No. 6, June 2007, pp. 2378-2383. doi: 10.1016/j.buildenv.2006.06.002

5. Sengul, O.; Azizi, S.; Karaosmanoglu, F.; and Tasdemir, M. A., “Effect of Expanded Perlite on the Mechanical Properties and Thermal Conductivity of Lightweight Concrete,” Energy and Buildings, V. 43, No. 2-3, Feb.-Mar. 2011, pp. 671-676. doi: 10.1016/j.enbuild.2010.11.008

6. ASTM C618-15, “Standard Specification for Coal Fly Ash and Raw or Calcined Natural Pozzolan for Use in Concrete,” ASTM International, West Conshohocken, PA, 2015, 5 pp.

7. EN 206+A2:2021, “Concrete – Specification, Performance, Production and Conformity,” European Committee for Standardization, Brussels, Belgium, 2017, 104 pp.

8. EN 450-1:2013, “Fly Ash for Concrete – Part 1: Definition, Specifications and Conformity Criteria,” European Committee for Standardization, Brussels, Belgium, 2013, 33 pp.

9. EN 13263-1:2005+A1:2009, “Silica Fume for Concrete – Part 1: Definitions, Requirements and Conformity Criteria,” European Committee for Standardization, Brussels, Belgium, 2009, 28 pp.

10. EN 15167-1:2007, “Ground Granulated Blast Furnace Slag for Use in Concrete, Mortar and Grout – Part 1: Definitions, Specifications and Conformity Criteria,” European Committee for Standardization, Brussels, Belgium, 2007, 24 pp.

11. SK-Technical Approval CEMPERLIT No. 17/0017, Building Testing and Research Institute (TSÚS) Bratislava, Bratislava, Slovakia, 2017.

12. TNI CEN/TR 16639:2014, “Use of k-Value Concept, Equivalent Concrete Performance Concept and Equivalent Performance of Combinations Concept,” (Approved by European Committee for Standardization on Nov. 26, 2013; issued in Mar. 2014 and applicable in Slovakia from Apr. 2015).

13. Bačuvčík, M., and Janotka, I., “Stanovenie k-hodnoty perlitu ako prímesi typu II na použitie do betónu/Bestimmung des k-Wertes von Perlit als des Zusatzstoffes Typ II für die Verwendung in Beton (translated: Determination of the k-Value of Perlite as the Addition of Type II for Use in Concrete),” Building Testing and Research Institute (TSÚS) Bratislava, Bratislava, Slovakia, 2016. (fully equivalent texts in Slovak and German)

14. Ray, A.; Sriravindrarajah, R.; Guerbois, J.-P.; Thomas, P. S.; Border, S.; Ray, H. N.; Haggman, J.; and Joyce, P., “Evaluation of Waste Perlite Fines in the Production of Construction Materials,” Journal of Thermal Analysis and Calorimetry, V. 88, No. 1, Apr. 2007, pp. 279-283. doi: 10.1007/s10973-006-8107-z

15. Karein, S. M. M.; Joshaghani, A.; Ramezanianpour, A. A.; Isapour, S.; and Karakouzian, M., “Effects of the Mechanical Milling Method on Transport Properties of Self-Compacting Concrete Containing Perlite Powder as a Supplementary Cementitious Material,” Construction and Building Materials, V. 172, May 2018, pp. 677-684. doi: 10.1016/j.conbuildmat.2018.03.205

16. Erdem, T. K.; Meral, Ç.; Tokyay, M.; and Erdoğan, T. Y., “Use of Perlite as a Pozzolanic Addition in Producing Blended Cements,” Cement and Concrete Composites, V. 29, No. 1, Jan. 2007, pp. 13-21. doi: 10.1016/j.cemconcomp.2006.07.018

17. Erdoğan, S. T., and Sağlık, A. Ü., “Early-Age Activation of Cement Pastes and Mortars Containing Ground Perlite as a Pozzolan,” Cement and Concrete Composites, V. 38, Apr. 2013, pp. 29-39. doi: 10.1016/j.cemconcomp.2013.03.004

18. Cobîrzan, N.; Balog, A.-A.; and Moşonyi, E., “Investigation of the Natural Pozzolans for Usage in Cement Industry,” Procedia Technology, V. 19, 2015, pp. 506-511.

19. Bektas, F.; Turanli, L.; and Monteiro, P. J. M., “Use of Perlite Powder to Suppress the Alkali–Silica Reaction,” Cement and Concrete Research, V. 35, No. 10, Oct. 2005, pp. 2014-2017. doi: 10.1016/j.cemconres.2004.10.029

20. Fodil, D., and Mohamed, M., “Compressive Strength and Corrosion Evaluation of Concretes Containing Pozzolana and Perlite Immersed in Aggressive Environments,” Construction and Building Materials, V. 179, Aug. 2018, pp. 25-34.

21. Chihaoui, R.; Khelafi, H.; Senhadji, Y.; and Mouli, M., “Potential Use of Natural Perlite Powder as a Pozzolanic Mineral Admixture in Portland Cement,” Journal of Adhesion Science and Technology, V. 30, No. 17, 2016, pp. 1930-1944. doi: 10.1080/01694243.2016.1171568

22. Yu, L.-H.; Ou, H.; and Lee, L.-L., “Investigation on Pozzolanic Effect of Perlite Powder in Concrete,” Cement and Concrete Research, V. 33, No. 1, Jan. 2003, pp. 73-76.

23. Chromá, M.; Rovnaníková, P.; Teplý, B.; Bergmeister, K.; and Strauss, A., “Concrete Durability and the k-Value Concept,” Cement, Wapno, Beton, V. 2, 2014, pp. 81-92.

24. Shah, V., and Bishnoi, S., “Carbonation Resistance of Cements Containing Supplementary Cementitious Materials and Its Relation to Various Parameters of Concrete,” Construction and Building Materials, V. 178, July 2018, pp. 219-232. doi: 10.1016/j.conbuildmat.2018.05.162

25. Paul, S. C.; Panda, B.; ; Huang, Y.; Garg, A.; and Peng, X., “An Empirical Model Design for Evaluation and Estimation of Carbonation Depth in Concrete,” Measurement, V. 125, Aug. 2018, pp. 205-210.

26. Ribeiro, A. B.; Santos, T.; and Gonꞔalves, A., “Performance of Concrete Exposed to Natural Carbonation: Use of the k-Value Concept,” Construction and Building Materials, V. 175, June 2018, pp. 360-370. doi: 10.1016/j.conbuildmat.2018.04.206

27. STN EN 197-1:2012, “Cement – Part 1: Composition, Specifications and Conformity Criteria for Common Cements,” Office for Standardization, Metrology and Testing of the Slovak Republic, Bratislava, Slovakia, 2012.

28. STN EN 12620+A1:2008, “Aggregates for Concrete,” Office for Standardization, Metrology and Testing of the Slovak Republic, Bratislava, Slovakia, 2008, 56 pp.

29. Frías, M.; Sánchez de Rojas, M. I.; and Cabrera, J., “The Effect that the Pozzolanic Reaction of Metakaolin Has on the Heat Evolution in Metakaolin-Cement Mortars,” Cement and Concrete Research, V. 30, No. 2, Feb. 2000, pp. 209-216. doi: 10.1016/S0008-8846(99)00231-8

30. EN 196-5:2011, “Methods of Testing Cement – Part 5: Pozzolanicity Test for Pozzolanic Cement,” European Committee for Standardization, Brussels, Belgium, 2011, 12 pp.

31. EN 12350-2:2010, “Testing Fresh Concrete – Part 2: Slump-Test,” European Committee for Standardization, Brussels, Belgium, 2010, 9 pp.

32. EN 12350-6:2011, “Testing Fresh Concrete – Part 6: Density,” European Committee for Standardization, Brussels, Belgium, 2011, 13 pp.

33. EN 12350-7:2011, “Testing Fresh Concrete – Part 7: Air Content – Pressure Methods,” European Committee for Standardization, Brussels, Belgium, 2011, 24 pp.

34. EN 12390-3:2010/AC:2011, “Testing Hardened Concrete – Part 3: Compressive Strength of Test Specimens,” European Committee for Standardization, Brussels, Belgium, 2010, 20 pp.

35. STN 73 1316:1989, “Determination of Moisture Content, Absorptivity and Capillarity of Concrete,” Office for Standardization, Metrology and Testing of the Slovak Republic, Bratislava, Slovakia, 1989, 8 pp.

36. EN 12390-8:2009, “Testing Hardened Concrete – Part 8: Depth of Penetration of Water under Pressure,” European Committee for Standardization, Brussels, Belgium, 2009, 7 pp.

37. STN 73 1322:2016, “Determination of Frost Resistance of Concrete,” Office for Standardization, Metrology and Testing of the Slovak Republic, Bratislava, Slovakia, 2016, 12 pp.

38. EN 12390-5:2011, “Testing Hardened Concrete – Part 5: Flexural Strength of Test Specimens,” European Committee for Standardization, Brussels, Belgium, 2011, 11 pp.

39. EN 12390-2:2010, “Testing Hardened Concrete – Part 2: Making and Curing Specimens for Strength Tests,” European Committee for Standardization, Brussels, Belgium, 2010, 12 pp.

40. EN 196-1:2016, “Methods of Testing Cement – Part 1: Determination of Strength,” European Committee for Standardization, Brussels, Belgium, 2016, 38 pp.

41. EN 196-2:2013, “Methods of Testing Cement – Part 2: Chemical Analysis of Cement,” European Committee for Standardization, Brussels, Belgium, 2013, 78 pp.

42. Janotka, I.; Bačuvčík, M.; and Paulík, P., “Low Carbonation of Concrete Found on 100-Year-Old Bridges,” Case Studies in Construction Materials, V. 8, June 2018, pp. 97-115. doi: 10.1016/j.cscm.2017.12.006

43. EN 1992-1-1:2005, “Eurocode 2: Design of Concrete Structures – Part 1-1: General Rules and Rules for Buildings,” European Committee for Standardization, Brussels, Belgium, 2005, 227 pp.


ALSO AVAILABLE IN:

Electronic Materials Journal