Axial Compression Capacity of Concrete Columns Reinforced with GFRP and Stainless Reinforcement

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Axial Compression Capacity of Concrete Columns Reinforced with GFRP and Stainless Reinforcement

Author(s): J.W. Wright and C.P. Pantelides

Publication: Symposium Paper

Volume: 351

Issue:

Appears on pages(s): 1-18

Keywords: carbon steel, columns, concrete, corrosion, glass fiber reinforced polymer, stainless clad, stainless steel.

DOI: 10.14359/51734671

Date: 4/1/2022

Abstract:
Axial compression performance of concrete columns reinforced with GFRP bars and spiral, 2304 duplex stainless bars and spiral, and 316L stainless clad bars, in varying combinations is examined after exposure to accelerated corrosion. The hybrid columns were reinforced with a combination of metallic and GFRP reinforcement. After corrosion exposure the columns were tested under axial compression to failure. Columns with GFRP vertical bars and stainless steel spiral were less corrosion resistant and had smaller axial load capacity than hybrid columns with stainless clad or stainless steel vertical bars and GFRP spiral. Columns reinforced with stainless steel spiral achieving two to three times the maximum axial displacement of columns with GFRP spiral. Axial compression capacity of hybrid columns in both corroded and uncorroded conditions was modeled using concrete confinement models for metallic and GFRP reinforcement with good agreement.