Tensile Behavior of Fiber-Reinforced Polymer Sheets Under Elevated Temperatures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Tensile Behavior of Fiber-Reinforced Polymer Sheets Under Elevated Temperatures

Author(s): Muhammad Faizan Qureshi and Shamim A. Sheikh

Publication: Structural Journal

Volume: 119

Issue: 5

Appears on pages(s): 179-192

Keywords:

DOI: 10.14359/51734664

Date: 9/1/2022

Abstract:

As part of a comprehensive study on the effects of climate change, tensile tests were performed on glass fiber-reinforced polymer (GFRP) and carbon FRP (CFRP) sheets under different temperature loadings to simulate field conditions. Specimens were loaded under two scenarios—that is, sustained temperature (ST) for 15 minutes followed by monotonic load until failure, and sustained deformation or sustained load (SD/SL) while the temperature was increased until the specimen failed. The elevated temperature caused a sharp decrease in the mechanical properties of the FRP as the temperature approached the glass-transition temperature (Tg) of epoxy. Beyond Tg, almost 40% and 50% residual tensile strength were retained by the GFRP and CFRP sheets, respectively. Elevated temperatures also shifted the failure pattern from brittle to softer failure due to epoxy softening. An equation is proposed for FRP properties subjected to elevated temperatures.

Related References:

Aktaş, M., and Karakuzu, R., 2009, “Determination of Mechanical Properties of Glass-Epoxy Composites in High Temperatures,” Polymer Composites, V. 30, No. 10, Oct., pp. 1437-1441.

ASTM D3039/D3039M-17, 2017, “Standard Test Method for Tensile Properties of Polymer Matrix Composite Materials,” ASTM International, West Conshohocken, PA, 13 pp.

Bisby, L. A.; Green, M. F.; and Kodur, V. K. R., 2005, “Response to Fire of Concrete Structures that Incorporate FRP,” Progress in Structural Engineering and Materials, V. 7, No. 3, July/Sept., pp. 136-149.

Cao, S., and Wu, Z., 2008, “Tensile Properties of FRP Composites at Elevated and High Temperatures,” Journal of Applied Mechanics, V. 11, Aug., pp. 963-970.

Cao, S.; Wu, Z.; and Wang, X., 2009, “Tensile Properties of CFRP and Hybrid FRP Composites at Elevated Temperatures,” Journal of Composite Materials, V. 43, No. 4, Feb., pp. 315-330.

Chowdhury, E. U.; Eedson, R.; Bisby, L. A.; Green, M. F.; and Benichou, N., 2011, “Mechanical Characterization of Fibre Reinforced Polymers Materials at High Temperature,” Fire Technology, V. 47, No. 4, Oct., pp. 1063-1080.

Di Ludovico, M.; Piscitelli, F.; Prota, A.; Lavorgna, M.; Mensitieri, G.; and Manfredi, G., 2012, “Improved Mechanical Properties of CFRP Laminates at Elevated Temperatures and Freeze–Thaw Cycling,” Construction and Building Materials, V. 31, June, pp. 273-283.

Environment and Climate Change Canada, 2021, “Record Heat Under the Dome,” Environment and Climate Change Canada, Canada, https://www.canada.ca/en/environment-climate-change/news/2021/12/the-impacts-of-a-changing-climate-canadas-top-ten-weather-stories-of-2021.html. (last accessed June 21, 2022)

Feih, S., and Mouritz, A. P., 2012, “Tensile Properties of Carbon Fibres and Carbon Fibre–Polymer Composites in Fire,” Composites Part A: Applied Science and Manufacturing, V. 43, No. 5, May, pp. 765-772. doi: 10.1016/j.compositesa.2011.06.016

Feih, S.; Boiocchi, E.; Kandare, E.; Mathys, Z.; Gibson, A. G.; and Mouritz, A. P., 2009, “Strength Degradation of Glass and Carbon Fibres at High Temperature,” School of Aerospace, Mechanical and Manufacturing Engineering, RMIT University, Melbourne, VIC, Australia, 10 pp.

Foster, S. K., and Bisby, L. A., 2005, “High Temperature Residual Properties of Externally-Bonded FRP Systems,” 7th International Symposium on Fiber-Reinforced Polymer (FRP) Reinforcement for Concrete Structures, SP-230, C. K. Shield, J. P. Busel, S. L. Walkup, and D. D. Gremel, eds., American Concrete Institute, Farmington Hills, MI, pp. 1235-1252.

Hawileh, R. A.; Abu-Obeidah, A.; Abdalla, J. A.; and Al-Tamimi, A., 2015, “Temperature Effect on the Mechanical Properties of Carbon, Glass and Carbon–Glass FRP Laminates,” Construction and Building Materials, V. 75, Jan., pp. 342-348.

Intergovernmental Panel on Climate Change, 2021, “Climate Change 2021: The Physical Science Basis,” IPCC, Geneva, Switzerland, 3949 pp., https://www.ipcc.ch/report/ar6/wg1/downloads/report/IPCC_AR6_WGI_Full_Report.pdf. (last accessed June 21, 2022)

Jarrah, M.; Najafabadi, E. P.; Khaneghahi, M. H.; and Oskouei, A. V., 2018, “The Effect of Elevated Temperatures on the Tensile Performance of GFRP and CFRP Sheets,” Construction and Building Materials, V. 190, Nov., pp. 38-52.

Lu, Z.; Xian, G.; and Li, H., 2016, “Effects of Elevated Temperatures on the Mechanical Properties of Basalt Fibers and BFRP Plates,” Construction and Building Materials, V. 127, Nov., pp. 1029-1036.

Nardone, F.; Di Ludovico, M.; De Caso y Basalo, F. J.; Prota, A.; and Nanni, A, 2012, “Tensile Behavior of Epoxy Based FRP Composites under Extreme Service Conditions,” Composites Part B: Engineering, V. 43, No. 3, Apr., pp. 1468-1474.

Ou, Y.; Zhu, D.; Zhang, H.; Huang, L.; Yao, Y.; Li, G.; and Mobasher, B., 2016, “Mechanical Characterization of the Tensile Properties of Glass Fiber and Its Reinforced Polymer (GFRP) Composite under Varying Strain Rates and Temperatures,” Polymers (Basel), V. 8, No. 5, May, Article No. 196. doi: 10.3390/polym805019610.3390/polym8050196

Qureshi, M. F.; Sheikh, S. A.; and Almansour, H., 2021, “Temperature Effects on the Mechanical Properties of the GFRP Sheets,” 10th International Conference on FRP Composites in Civil Engineering: Proceedings of CICE2020/2021, A. Ilki, M. Ispir, and P. Inci, eds., Istanbul, Turkey, pp. 809-822.

Rezaei, M.; Karatzas, V.; Berggreen, C.; and Carlsson, L. A., 2020, “The Effect of Elevated Temperature on the Mechanical Properties and Failure Modes of GFRP Face Sheets and PET Foam Cored Sandwich Beams,” Journal of Sandwich Structures and Materials, V. 22, No. 4, May, pp. 1235-1255.

Yang, Y.; Jiang, Y.; Liang, H.; Yin, X.; and Huang, Y., 2019, “Study on Tensile Properties of CFRP Plates under Elevated Temperature Exposure,” Materials (Basel), V. 12, No. 12, June, Article No. 1995. doi: 10.3390/ma12121995


ALSO AVAILABLE IN:

Electronic Structural Journal