Compression Tests of Very Large Reinforced Concrete Pile Caps and Comparison with Predicted Strength

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Compression Tests of Very Large Reinforced Concrete Pile Caps and Comparison with Predicted Strength

Author(s): Yasmeen Al-Sakin, Anthony Sorentino, Christopher Higgins, James Newell, and Kent Yu

Publication: Structural Journal

Volume: 119

Issue: 5

Appears on pages(s): 141-152

Keywords:

DOI: 10.14359/51734663

Date: 9/1/2022

Abstract:
An experimental program consisting of four full-scale specimens was conducted to assess the structural behavior of very large reinforced concrete (RC) pile caps supported on steel pipe piles. The tested specimens replicated the geometry, reinforcement details and placement, material properties, as well as support and loading conditions typical of in-service 1980s vintage pile caps. Prior to testing, three-dimensional (3-D) strut-and-tie models were developed to predict the strength of the specimens and expected failure modes. During tests, widespread reinforcement yielding was observed in all specimens. One specimen failed in one-way shear, two specimens failed in two-way shear, and one specimen did not reach failure before reaching the load capacity of the test setup. Based on the experimental results, the strut-and-tie capacity predictions were highly conservative for all specimens and would have required retrofit of the pile caps to carry the expected column axial loads associated with a potential vertical expansion of the building. The high degree of conservatism is attributed to neglecting the beneficial effects of active confinement in the 3-D structure, especially at the pile locations, that underestimates the available bond strength, thereby minimizing the available tension ties.

Related References:

1. Clarke, J. L., “Behaviour and Design of Pile Caps with Four Piles,” Cement and Concrete Association, London, UK, 1973.

2. Sabnis, G. M., and Gogate, A. B., “Investigation of Thick Slab (Pile Cap) Behavior,” ACI Journal Proceedings, V. 81, No. 1, Jan.-Feb. 1984, pp. 35-39.

3. Schlaich, J.; Schafer, K.; and Jennewein, M., “Toward a Consistent Design of Structural Concrete,” PCI Journal, V. 32, No. 3, 1987, pp. 74-150. doi: 10.15554/pcij.05011987.74.150

4. Adebar, P.; Kuchma, D.; and Collins, M. P., “Strut-and-Tie Models for The Design of Pile Caps: An Experimental Study,” ACI Structural Journal, V. 87, No. 1, Jan.-Feb. 1990, pp. 81-92.

5. Suzuki, K.; Otsuki, K.; and Tsubata, T., “Influence of Bar Arrangement on Ultimate Strength of Four-Pile Caps,” Transactions of the Japan Concrete Institute, V. 20, 1998, pp. 195-202.

6. Suzuki, K., and Otsuki, K., “Experimental Study on Corner Shear Failure of Pile Caps,” Transactions of the Japan Concrete Institute, V. 23, 2002, pp. 303-310.

7. Miguel, M. G.; Takeya, T.; and Giongo, J. S., “Structural Behaviour of Three-Pile Caps Subjected to Axial Compressive Loading,” Materials and Structures, V. 41, No. 1, 2007, pp. 85-98. doi: 10.1617/s11527-007-9221-5

8. Gu, Q.; Sun, C.; and Peng, S., “Experimental Study on Deep Four-Pile Caps with Different Reinforcement Layouts Based on 3D Strut-and-Tie Analogy,” Key Engineering Materials, V. 400, 2009, pp. 917-922.

9. Miguel-Tortola, L.; Pallarés, L.; and Miguel, P. F., “Punching Shear Failure in Three-Pile Caps: Influence of The Shear Span-Depth Ratio and Secondary Reinforcement,” Engineering Structures, V. 155, 2018, pp. 127-143. doi: 10.1016/j.engstruct.2017.10.077

10. Guo, H., “Investigation on Punching Behavior of Pile Cap under Column Reinforced by Section Steel Truss,” ACI Structural Journal, V. 115, No. 2, 2018, pp. 379-390. doi: 10.14359/51700948

11. Reineck, K.-H., and Novak, L. C., eds., Further Examples for The Design of Structural Concrete with Strut-and-Tie Models, SP-273, American Concrete Institute, Farmington Hills, MI, 2010, 288 pp.

12. Darwin, D.; Dolan, C. W.; and Nilson, A. H., Design of Concrete Structures, 15th edition, McGraw-Hill Education, New York, 2016, 786 pp.

13. ASTM C42/C42M-04, “Test Method for Obtaining and Testing Drilled Cores and Sawed Beams of Concrete,” ASTM International, West Conshohocken, PA, 2004, 6 pp.

14. ASTM C39/C39M-05, “Test Method for Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2005, 7 pp.

15. ASTM C496/C496M-04e1, “Test Method for Splitting Tensile Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2004, 5 pp.

16. ASTM A615/A615M-05a, “Specification for Deformed and Plain Carbon-Steel Bars for Concrete Reinforcement,” ASTM International, West Conshohocken, PA, 2005, 6 pp.

17. ASTM E8/E8-04, “Test Methods for Tension Testing of Metallic Materials,” ASTM International, West Conshohocken, PA, 2004, 24 pp.

18. Higgins, C., and Sorentino, A., “Report: VA Hospital Pile Cap Tests,” Oregon State University, Corvallis, OR, 2011, 98 pp. (available on request)

19. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-02) and Commentary (ACI 318R-02),” American Concrete Institute, Farmington Hills, MI, 2002, 443 pp.

20. Reineck, K.-H., ed., Examples for the Design of Structural Concrete with Strut-and-Tie Models, SP-208, American Concrete Institute, Farmington Hills, MI, 2002, 242 pp.

21. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19),” American Concrete Institute, Farmington Hills, MI, 2019, 623 pp.

22. Mitchell, D.; Collins, M. P.; Bhide, S. B.; and Rabbat, B., AASHTO LRFD Strut-and-Tie Model Design Examples, Portland Cement Association, Skokie, IL, 2004.

23. Boulifa, R.; Samai, M. L.; Benhassine, M. T.; and Tekkouk, A., “Predicting Strength Capacity of Three-Dimensional Concrete Struts in Pile Caps,” ACI Structural Journal, V. 118, No. 2, Mar. 2021, pp. 111-126.