Title: ACI PRC-207.1-21: Mass Concrete—Guide

Author(s): ACI Committee 207

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 34

Keywords:

DOI:

Date: 2/1/2022

Abstract:
This guide contains a history of the development of mass concrete practice and discussion of materials and concrete mixture proportioning, properties, construction methods, and equipment. It covers traditionally placed and consolidated mass concrete for massive structures such as dams and provides information applicable to mass structural heavily reinforced concrete and for thermally controlled concrete such as bridge elements and building foundations. This guide does not cover roller-compacted concrete. Keywords: cement; cracking; fly ash; heat of hydration; mass concrete; mixture proportioning; supplementary cementitious materials; temperature rise; thermal control plan; thermal expansion; volume change.