Shear Strength Evaluation of Diagonally Reinforced Concrete Coupling Beams with Steel Fibers

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Shear Strength Evaluation of Diagonally Reinforced Concrete Coupling Beams with Steel Fibers

Author(s): Dong-Hee Son, Baek-Il Bae, and Chang-Sik Choi

Publication: Structural Journal

Volume: 119

Issue: 4

Appears on pages(s): 291-302

Keywords: reinforced concrete coupling beam; shear strength; steel fiber; transverse reinforcement

DOI: 10.14359/51734525

Date: 7/1/2022

Abstract:
This study evaluated the shear strength of a diagonally reinforced coupling beam with steel fibers subjected to cyclic loading through experiments. A total of seven specimens were examined using the amount of transverse reinforcement, concrete strength, and volume fraction of steel fiber as variables. The experiments showed that sufficient ductility and strength were ensured even when steel fibers were incorporated and transverse reinforcement was simplified. In particular, with a 2% volume fraction of steel fibers, the strength and ductility satisfied ACI 318-19 because steel fiber-reinforced concrete sufficiently replaced the transverse reinforcement to prevent buckling of the diagonal reinforcing bars. When evaluating the shear strength of steel fiber-reinforced coupling beams with regard to the ACI provision, the shear strength was predicted more accurately when the shear contribution of the concrete was considered and the diagonal reinforcement was properly confined.

Related References:

1. Park, R., and Paulay, T., Reinforced Concrete Structures, John Wiley & Sons, Inc., New York, 1975.

2. Paulay, T., and Priestley, M. J. N., Seismic Design of Reinforced Concrete and Masonry Buildings, John Wiley & Sons, Inc., New York, 1992.

3. Paulay, T., and Binney, J. R., “Diagonally Reinforced Coupling Beams of Shear Walls,” Shear in Reinforced Concrete, SP-42, American Concrete Institute, Farmington Hills, MI, Jan. 1974, pp. 579-598.

4. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19),” American Concrete Institute, Farmington Hills, MI, 2019, 624 pp.

5. Barney, G. B.; Shiu, K. N.; Rabbat, B. G.; Fiorato, A. E.; Russell, H. G.; and Corley, W. G., “Behavior of Coupling Beams Under Load Reversals,” Research and Development Bulletin RD 068, Portland Cement Association, Skokie, IL, 1980, 22 pp.

6. Tassios, T. P.; Moretti, M.; and Bezas, A., “On the Behavior and Ductility of Reinforced Concrete Coupling Beams of Shear Walls,” ACI Structural Journal, V. 93, No. 6, Nov.-Dec. 1996, pp. 711-720.

7. Jang, S.-J.; Jeong, G.-Y.; and Yun, H.-D., “Use of Steel Fibers as Transverse Reinforcement in Diagonally Reinforced Coupling Beams with Normal- and High-Strength Concrete,” Construction and Building Materials, V. 187, Oct. 2018, pp. 1020-1030. doi: 10.1016/j.conbuildmat.2018.08.063

8. Parra-Montesinos, G. J., “Shear Strength of Beams with Deformed Steel Fibers,” Concrete International, V. 28, No. 11, Nov. 2006, pp. 57-66.

9. ACI Committee 544, “Design Considerations for Steel Fiber Reinforced Concrete (ACI 544.4R-88) (Reapproved 2009),” American Concrete Institute, Farmington Hills, MI, 2009, 18 pp.

10. Choi, C.-S., and Bae, B.-I., “Effectiveness of Steel Fibers as Hoops in Exterior Beam-to-Column Joints under Cyclic Loading,” ACI Structural Journal, V. 116, No. 2, Mar. 2019, pp. 205-219. doi: 10.14359/51712278

11. Bae, B.-I.; Chung, J.-H.; Choi, H.-K.; Jung, H.-S.; and Choi, C.-S., “Experimental Study on the Cyclic Behavior of Steel Fiber Reinforced High Strength Concrete Columns and Evaluation of Shear Strength,” Engineering Structures, V. 157, Feb. 2018, pp. 250-267. doi: 10.1016/j.engstruct.2017.11.072

12. Zhong, A.; Sofi, M.; Lumantarna, E.; Zhou, Z.; and Mendis, P., “Flexural Capacity Prediction Model for Steel Fibre-Reinforced Concrete Beams,” International Journal of Concrete Structures and Materials, V. 15, No. 1, 2021, Article No. 28. doi: 10.1186/s40069-021-00461-0

13. Caballero-Morrison, K. E.; Bonet, J. L.; Navarro-Gregori, J.; and Serna-Ros, P., “An Experimental Study of Steel Fiber-Reinforced High-Strength Concrete Slender Columns under Cyclic Loading,” Engineering Structures, V. 57, Dec. 2013, pp. 565-577. doi: 10.1016/j.engstruct.2012.06.052

14. Kawashima, K.; Zafra, R.; Sasaki, T.; Kajiwara, K.; and Nakayama, M., “Effect of Polypropylene Fiber Reinforced Cement Composite and Steel Fiber Reinforced Concrete for Enhancing the Seismic Performance of Bridge Columns,” Journal of Earthquake Engineering, V. 15, No. 8, 2011, pp. 1194-1211. doi: 10.1080/13632469.2011.569051

15. Yun, H.-D.; Kim, S.-W.; Jeon, E.; Park, W.-S.; and Lee, Y.-T., “Effects of Fibre-Reinforced Cement Composites’ Ductility on the Seismic Performance of Short Coupling Beams,” Magazine of Concrete Research, V. 60, No. 3, 2008, pp. 223-233. doi: 10.1680/macr.2007.00081

16. Canbolat, B. A.; Parra-Montesinos, G. J.; and Wight, J. K., “Experimental Study on Seismic Behavior of High-Performance Fiber-Reinforced Cement Composite Coupling Beams,” ACI Structural Journal, V. 102, No. 1, Jan.-Feb. 2005, pp. 159-166.

17. Lequesne, R. D.; Parra-Montesinos, G. J.; and Wight, J. K., “Seismic Behavior and Detailing of High-Performance Fiber-Reinforced Concrete Coupling Beams and Coupled Wall Systems,” Journal of Structural Engineering, ASCE, V. 139, No. 8, 2013, pp. 1362-1370. doi: 10.1061/(ASCE)ST.1943-541X.0000687

18. Hung, C.-C., and El-Tawil, S., “Seismic Behavior of a Coupled-Wall System with HPFRCC Coupling Beams,” Proceedings, Structures Congress 2010, S. Senapathi, K. Casey, and M. Hoit, eds., Orlando, FL, 2010, pp. 1864-1873.

19. Kim, J.-S.; Bae, B.-I.; and Choi, C.-S., “A Study on the Effect of Steel Fiber in Reinforced Concrete Coupling Beam Subjected to Cyclic Loading,” Journal of the Architectural Institute of Korea Structure & Construction, V. 35, No. 10, 2019, pp. 181-190.

20. ACI Committee 374, “Guide for Testing Reinforced Concrete Structural Elements under Slowly Applied Simulated Seismic Loads (ACI 374.2R-13),” American Concrete Institute, Farmington Hills, MI, 2013, 18 pp.

21. ACI Committee 544, “Guide for Specifying, Proportioning, and Production of Fiber-Reinforced Concrete (ACI 544.3R-08),” American Concrete Institute, Farmington Hills, MI, 2008, 14 pp.

22. Wight, J. K., and MacGregor, J. G., Reinforced Concrete: Mechanics and Design, fifth edition, Prentice Hall, Upper Saddle River, NJ, 2008.

23. Harries, K. A.; Fortney, P. J.; Shahrooz, B. M.; and Brienen, P. J., “Practical Design of Diagonally Reinforced Concrete Coupling Beams—Critical Review of ACI 318 Requirements,” ACI Structural Journal, V. 102, No. 6, Nov.-Dec. 2005, pp. 876-882.

24. Thomas, J., and Ramaswamy, A., “Mechanical Properties of Steel Fiber-Reinforced Concrete,” Journal of Materials in Civil Engineering, ASCE, V. 19, No. 5, 2007, pp. 385-392. doi: 10.1061/(ASCE)0899-1561(2007)19:5(385)

25. Gao, J.; Sun, W.; and Morino, K., “Mechanical Properties of Steel Fiber-Reinforced, High-Strength, Lightweight Concrete,” Cement and Concrete Composites, V. 19, No. 4, 1997, pp. 307-313. doi: 10.1016/S0958-9465(97)00023-1

26. Sharma, A. K., “Shear Strength of Steel Fiber Reinforced Concrete Beams,” ACI Journal Proceedings, V. 83, No. 4, July-Aug. 1986, pp. 624-628.

27. Chung, J.-H.; Son, D.-H.; Kim, S.-Y.; Bae, B.-I.; and Choi, C.-S., “Hysteretic Behavior of Reinforced Concrete Coupling Beams According to Volume Fraction of Steel Fiber,” Sustainability, V. 13, No. 1, 2021, p. 182. doi: 10.3390/su13010182

28. Park, R., “Evaluation of Ductility of Structures and Structural Assemblages from Laboratory Testing,” Bulletin of the New Zealand Society for Earthquake Engineering, V. 22, No. 3, 1989, pp. 155-166. doi: 10.5459/bnzsee.22.3.155-166

29. ASCE/SEI 41-17, “Seismic Evaluation and Retrofit of Existing Buildings,” American Society of Civil Engineers, Reston, VA, 2017.

30. Lim, E.; Hwang, S.-J.; Wang, T.-W.; and Chang, Y.-H., “An Investigation on the Seismic Behavior of Deep Reinforced Concrete Coupling Beams,” ACI Structural Journal, V. 113, No. 2, Mar.-Apr. 2016, pp. 217-226. doi: 10.14359/51687939

31. Kim, W.; Kim, J.; and Kwak, Y.-K., “Evaluation of Flexural Strength Prediction of Reinforced Concrete Beams with Steel Fibres,” Journal of Structural Integrity and Maintenance, V. 1, No. 4, 2016, pp. 156-166. doi: 10.1080/24705314.2016.1240522

32. ACI Committee 544, “Guide to Design with Fiber-Reinforced Concrete (ACI 544.4R-18),” American Concrete Institute, Farmington Hills, MI, 2018, 44 pp.

33. Fédération internationale du béton, “fib Model Code for Concrete Structures 2010,” fib, Lausanne, Switzerland, 2013, 434 pp.

34. Park, W.-S.; Kang, T. H.-K.; Kim, S.; and Yun, H.-D., “Seismic Performance of Moderately Short Concrete Coupling Beams with Various Reinforcements,” ACI Structural Journal, V. 117, No. 3, May 2020, pp. 141-154.


ALSO AVAILABLE IN:

Electronic Structural Journal