On Punching Shear Strength of Steel Fiber-Reinforced Concrete Slabs-on-Ground

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: On Punching Shear Strength of Steel Fiber-Reinforced Concrete Slabs-on-Ground

Author(s): Raphael Palmier Manfredi, Flávio de Andrade Silva, and Daniel Carlos Taissum Cardoso

Publication: Structural Journal

Volume: 119

Issue: 4

Appears on pages(s): 185-196

Keywords: crack kinematics; punching shear; slabs-on-ground; steel fiber-reinforced concrete (SFRC)

DOI: 10.14359/51734520

Date: 7/1/2022

Abstract:
The work in hand presents the results of an experimental investigation on the punching shear performance of steel fiber-reinforced concrete (SFRC) slabs-on-ground, a problem that has received little attention worldwide. In the first part of the experimental program, residual strengths are obtained according to different methodologies, namely EN 14651 and ASTM C1609, considering normal concrete matrixes reinforced with hooked-end steel fibers in contents of 20, 30, and 40 kg/m3 (33.71, 50.56, and 67.42 lb/yd3). Then, three slabs-on-ground were fabricated (one for each content) and tested for a central single-point load and it was confirmed that the use of fibers increased ultimate load and ductility. The results are compared with those obtained using the predictions of the fourth edition of Technical Report 34 (TR 34) issued by The Concrete Society, and differences of less than 10% are observed. The influence of rotation and relative displacement between the central shear cone and surrounding slab are studied, confirming the relevance of the latter to the crack kinematics. A simple mechanical model is proposed, revealing that the contributions of each load-transfer mechanism according to TR 34 are unrealistic and that the fiber action responds roughly for 40% of the capacity. Finally, design recommendations are proposed to account in a meaningful way for the actual contributions of concrete, fibers, and subgrade to the punching shear strength.

Related References:

1. Beckett, D., “Comparative Tests on Plain, Fabric Reinforced and Steel Fibre Reinforced Concrete Ground Slabs,” Concrete (London), V. 24, No. 3, 1990, pp. 43-45.

2. Falkner, H.; Huang, Z.; and Teutsch, M., “Comparative Study of Plain and Steel Fiber Reinforced Concrete Ground Slabs,” Concrete International, V. 17, No. 1, Jan. 1995, pp. 45-51.

3. Beckett, D.; Van De Woestyne, T.; and Callens, S. J. P., “Corner and Edge Loading on Concrete Industrial Ground Floors Reinforced with Steel Fibres,” Concrete (London), V. 33, No. 3, 1999, pp. 22-24.

4. Elsaigh, W. A., “Steel Fiber Reinforced Concrete Ground Slabs: A Comparative Evaluation of Plain and Steel Fiber Reinforced Concrete Ground Slabs,” Master’s dissertation, University of Pretoria, Pretoria, Gauteng, South Africa, 2001, 154 pp.

5. Roesler, J. R.; Lange, D. A.; Altoubat, S. A.; Rieder, K.-A.; and Ulreich, G. R., “Fracture of Plain and Fiber-Reinforced Concrete Slabs under Monotonic Loading,” Journal of Materials in Civil Engineering, ASCE, V. 16, No. 5, Oct. 2004, pp. 452-460. doi: 10.1061/(ASCE)0899-1561(2004)16:5(452)

6. Sorelli, L.; Meda, A.; Plizzari, G. A.; and Rossi, B., “Experimental Investigation on Slabs on Grade: Steel Fibers vs. Conventional Reinforcement,” Fibre-Reinforced Concretes: Proceedings of the Sixth International RILEM Symposium (BEFIB 2004), M. di Prisco, R. Felicetti, and G. A. Plizzari, eds., RILEM Publications SARL, Varenna, Italy, 2004, pp. 1083-1092.

7. Roesler, J. R.; Altoubat, S. A.; Lange, D. A.; Rieder, K.-A.; and Ulreich, G. R., “Effect of Synthetic Fibers on Structural Behavior of Concrete Slabs-on-Ground,” ACI Materials Journal, V. 103, No. 1, Jan.-Feb. 2006, pp. 3-10. doi: 10.14359/15121

8. Chen, S., “Strength of Steel Fibre Reinforced Concrete Ground Slabs,” Proceedings of the Institution of Civil Engineers – Structures and Buildings, V. 157, No. 2, Apr. 2004, pp. 157-163. doi: 10.1680/stbu.2004.157.2.157

9. Meda, A., and Plizzari, G. A., “New Design Approach for Steel Fiber-Reinforced Concrete Slabs-on-Ground Based on Fracture Mechanics,” ACI Structural Journal, V. 101, No. 3, May-June 2004, pp. 298-303. doi: 10.14359/13089

10. Beckett, D., “Comparative Tests on Plain, Fabric Reinforced and Steel Reinforced Concrete Ground Slabs: Beckett, D. Concrete Vol 24 No 3 (1990) pp 43–45,” Composites, V. 21, No. 4, July 1990, p. 355. doi: 10.1016/0010-4361(90)90353-X

11. Westergaard, H. M., “On the Design of Slabs on Elastic Foundation with Special Reference to Stresses in Concrete Pavements,” Ingeniøren, V. 12, 1923. (in German)

12. Meyerhof, G. G., “Load-Carrying Capacity of Concrete Pavements,” Journal of the Soil Mechanics and Foundations Division, ASCE, V. 88, No. 3, June 1962, pp. 89-116. doi: 10.1061/JSFEAQ.0000432

13. Aldossari, K. M.; Elsaigh, W. A.; and Alshannag, M. J., “High-Strength Steel-Fibre-Reinforced Concrete: Potential Use for Ground Slabs Applications,” Proceedings of the Institution of Civil Engineers – Transport, V. 171, No. 3, June 2018, pp. 156-165. doi: 10.1680/jtran.15.0011810.1680/jtran.15.00118

14. The Concrete Society, “Concrete Industrial Ground Floors: A Guide to Design and Construction (Technical Report 34),” fourth edition, The Concrete Society, Surrey, UK, 2013, 104 pp.

15. ACI Committee 360, “Guide to Design of Slabs-on-Ground (ACI 360R-10),” American Concrete Institute, Farmington Hills, MI, 2010, 72 pp.

16. ACI Committee 544, “Guide to Design with Fiber-Reinforced Concrete (ACI 544.4R-18),” American Concrete Institute, Farmington Hills, MI, 2018, 44 pp.

17. Alani, A.; Beckett, D.; and Khosrowshahi, F., “Mechanical Behaviour of a Steel Fibre Reinforced Concrete Ground Slab,” Magazine of Concrete Research, V. 64, No. 7, July 2012, pp. 593-604. doi: 10.1680/macr.11.00077

18. The Concrete Society, “Concrete Industrial Ground Floors: A Guide to Design and Construction (Technical Report No. 34),” third edition, The Concrete Society, Berkshire, UK, 2003, 148 pp.

19. Altoubat, S. A.; Roesler, J. R.; Lange, D. A.; and Rieder, K.-A., “Simplified Method for Concrete Pavement Design with Discrete Structural Fibers,” Construction and Building Materials, V. 22, No. 3, Mar. 2008, pp. 384-393. doi: 10.1016/j.conbuildmat.2006.08.008

20. Shentu, L.; Jiang, D.; and Hsu, C.-T. T., “Load-Carrying Capacity for Concrete Slabs on Grade,” Journal of Structural Engineering, ASCE, V. 123, No. 1, Jan. 1997, pp. 95-103. doi: 10.1061/(ASCE)0733-9445(1997)123:1(95)

21. Fédération internationale du béton, “fib Model Code for Concrete Structures 2010,” fib, Lausanne, Switzerland, 2013, 434 pp.

22. Vandewalle, L.; Nemegeer, D.; Balázs, G. L.; Barr, B.; Barros, J.; Bartos, P.; Banthia, N.; Criswell, M.; Denarié, E.; Di Prisco, M.; Falkner, H.; Gettu, R.; Gopalaratnam, V.; Groth, P.; Häusler, V.; Kooiman, A.; Kovler, K.; Massicotte, B.; Mindess, S.; Reinhardt, H.-W.; Rossi, P.; Schaerlaekens, S.; Schumacher, P.; Schnütgen, B.; Shah, S.; Skarendahl, Å.; Stang, H.; Stroeven, P.; Swamy, R.; Tatnall, P.; Teutsch, M.; and Walraven, J., “Final Recommendation of RILEM TC 162-TDF: Test and Design Methods for Steel Fibre Reinforced Concrete Sigma-Epsilon-Design Method,” Materials and Structures, V. 36, No. 8, Oct. 2003, pp. 560-567. doi: 10.1617/14007

23. Barros, J. A. O., and Figueiras, J. A., “Model for the Analysis of Steel Fibre Reinforced Concrete Slabs on Grade,” Computers & Structures, V. 79, No. 1, Jan. 2001, pp. 97-106. doi: 10.1016/S0045-7949(00)00061-4

24. Belletti, B.; Cerioni, R.; Meda, A.; and Plizzari, G., “Design Aspects on Steel Fiber-Reinforced Concrete Pavements,” Journal of Materials in Civil Engineering, ASCE, V. 20, No. 9, Sept. 2008, pp. 599-607. doi: 10.1061/(ASCE)0899-1561(2008)20:9(599)

25. Gouveia, N. D.; Fernandes, N. A. G.; Faria, D. M. V.; Ramos, A. M. P.; and Lúcio, V. J. G., “SFRC Flat Slabs Punching Behaviour – Experimental Research,” Composites Part B: Engineering, V. 63, July 2014, pp. 161-171. doi: 10.1016/j.compositesb.2014.04.005

26. Nguyen-Minh, L.; Rovňák, M.; and Tran-Quoc, T., “Punching Shear Capacity of Interior SFRC Slab-Column Connections,” Journal of Structural Engineering, ASCE, V. 138, No. 5, May 2012, pp. 613-624. doi: 10.1061/(ASCE)ST.1943-541X.0000497

27. Maya, L. F.; Fernández Ruiz, M.; Muttoni, A.; and Foster, S. J., “Punching Shear Strength of Steel Fibre Reinforced Concrete Slabs,” Engineering Structures, V. 40, July 2012, pp. 83-94. doi: 10.1016/j.engstruct.2012.02.009

28. Kueres, D.; Polak, M. A.; and Hegger, J., “Two-Parameter Kinematic Theory for Punching Shear in Steel Fiber Reinforced Concrete Slabs,” Engineering Structures, V. 205, Feb. 2020, Article No. 110086. doi: 10.1016/j.engstruct.2019.110086

29. Alani, A. M., and Beckett, D., “Mechanical Properties of a Large Scale Synthetic Fibre Reinforced Concrete Ground Slab,” Construction and Building Materials, V. 41, Apr. 2013, pp. 335-344. doi: 10.1016/j.conbuildmat.2012.11.043

30. EN 14651:2005, “Test Method for Metallic Fibre Concrete – Measuring the Flexural Tensile Strength (Limit of Proportionality (LOP), Residual),” European Committee for Standardization, Brussels, Belgium, 2005, 20 pp.

31. ASTM C1609/C1609M-19a, “Standard Test Method for Flexural Performance of Fiber-Reinforced Concrete (Using Beam with Third-Point Loading),” ASTM International, West Conshohocken, PA, 2019, 9 pp.

32. de Oliveira e Sousa, J. L. A., and Gettu, R., “Determining the Tensile Stress-Crack Opening Curve of Concrete by Inverse Analysis,” Journal of Engineering Mechanics, ASCE, V. 132, No. 2, Feb. 2006, pp. 141-148. doi: 10.1061/(ASCE)0733-9399(2006)132:2(141)

33. Meskenas, A.; Kaklauskas, G.; Daniunas, A.; Bacinskas, D.; Jakubovskis, R.; Gribniak, S.; and Gelazius, V., “Determination of the Stress–Crack Opening Relationship of SFRC by an Inverse Analysis,” Mechanics of Composite Materials, V. 49, No. 6, Jan. 2014, pp. 685-690. doi: 10.1007/s11029-013-9385-8

34. Amin, A.; Foster, S. J.; and Muttoni, A., “Derivation of the σ-w Relationship for SFRC from Prism Bending Tests,” Structural Concrete, V. 16, No. 1, Mar. 2015, pp. 93-105. doi: 10.1002/suco.201400018

35. Manfredi, R. P., “Mechanical Properties and Design of Steel Fiber Reinforced Concrete Structures,” Master’s thesis, Pontifical Catholic University of Rio de Janeiro (PUC-Rio), Rio de Janeiro, RJ, Brazil, 2020.

36. Armelin, H. S., “Rebound and Toughening Mechanisms in Steel Fiber Reinforced Dry-Mix Shotcrete,” PhD thesis, The University of British Columbia, Vancouver, BC, Canada, 1997, 285 pp. doi: 10.14288/1.005031910.14288/1.0050319

37. EN 1992-1-1:2004, “Eurocode 2: Design of Concrete Structures – Part 1-1: General Rules and Rules for Buildings,” European Committee for Standardization, Brussels, Belgium, 2004, 227 pp.

38. Huber, P.; Huber, T.; and Kollegger, J., “Investigation of the Shear Behavior of RC Beams on the Basis of Measured Crack Kinematics,” Engineering Structures, V. 113, Apr. 2016, pp. 41-58. doi: 10.1016/j.engstruct.2016.01.025

39. Cavagnis, F.; Fernández Ruiz, M.; and Muttoni, A., “An Analysis of the Shear-Transfer Actions in Reinforced Concrete Members without Transverse Reinforcement Based on Refined Experimental Measurements,” Structural Concrete, V. 19, No. 1, Feb. 2018, pp. 49-64. doi: 10.1002/suco.201700145

40. Simões, J. T.; Faria, D. M. V.; Fernández Ruiz, M.; and Muttoni, A., “Strength of Reinforced Concrete Footings without Transverse Reinforcement According to Limit Analysis,” Engineering Structures, V. 112, Apr. 2016, pp. 146-161. doi: 10.1016/j.engstruct.2016.01.010

41. Muttoni, A.; Fernández Ruiz, M.; and Simões, J. T., “The Theoretical Principles of the Critical Shear Crack Theory for Punching Shear Failures and Derivation of Consistent Closed-Form Design Expressions,” Structural Concrete, V. 19, No. 1, Feb. 2018, pp. 174-190. doi: 10.1002/suco.201700088


ALSO AVAILABLE IN:

Electronic Structural Journal