Seismic Behavior of Frames with Special-Shaped Concrete-Filled Steel Tubular Columns and H-Shaped Steel Beams

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Seismic Behavior of Frames with Special-Shaped Concrete-Filled Steel Tubular Columns and H-Shaped Steel Beams

Author(s): Yuanlong Yang, Weiqi Yang, Xin Tang, and Guozhong Cheng

Publication: Structural Journal

Volume: 119

Issue: 3

Appears on pages(s): 29-42

Keywords: finite element analysis; frame; nonlinear static analysis; pseudo static test; seismic behavior; special-shaped concrete-filled steel tubular column

DOI: 10.14359/51734489

Date: 5/1/2022

Abstract:
A pseudo static test of four special-shaped concrete-filled steel tubular column to H-shaped steel beam plane frames (SCFSTF) was previously conducted by the authors and a typical strongcolumn/ weak-beam failure mode was determined. The degradation in strength and rigidity were minimal and the energy dissipation capacity and ductility of frames were adequate, demonstrating excellent seismic performance. Besides, energy dissipation capacity and horizontal resistance were improved with axial load ratio increasing within the parametric range of this test. Based on the test results, an investigation on seismic performance of SCFSTF with fiber model and nonlinear static analysis method was developed. The fiber model of SCFSTF specimens was established with OpenSEES software and the simulation results agreed well with the test results. The load-displacement hysteretic curve, skeleton curve, and plastic hinge formation of SCFSTF were accurately predicted. Based on a parametric analysis, the effects of compression ratio, beam-to-column stiffness ratio, and beam-to-column resistance ratio on the seismic behavior of SCFSTF were analyzed and moreover corresponding design suggestions were proposed. Besides, two design models (a nine-story residence and a 14-story dormitory) of SCFSTF were designed with structural analysis software ETABS. The two design models of SCFSTF meet the seismic fortification target according to the Chinese standard “Code for seismic design of buildings,” which proved that the SCFSTF structure has good seismic performance and can be used in engineering practices.

Related References:

ATC-40, 1996, “Seismic Evaluation and Retrofit of Concrete Buildings,” Applied Technology Council, Redwood City, CA.

Du, G. F.; Ma, C.; and Xu, C. X., 2012, “Experimental Research on Seismic Behavior of Exterior Frame Joints with T-Shaped CFST Column and Steel Beam,” Advanced Materials Research, V. 368-373, pp. 183-188. doi: 10.4028/www.scientific.net/AMR.368-373.183

FEMA 440, 2005, “Improvement of Static Nonlinear Analysis Procedures,” Federal Emergency Management Agency, Washington, DC.

GB 50009-2012, 2014, “Load Code for the Design of Building Structures,” Ministry of Housing and Urban-Rural Development of the People’s Republic of China, Beijing, China.

GB 50010-2010, 2010, “Code for Design of Concrete Structures,” Ministry of Housing and Urban-Rural Development of the People’s Republic of China, Beijing, China.

GB 50011-2010, 2010, “Code for Seismic Design of Buildings,” Ministry of Housing and Urban-Rural Development of the People’s Republic of China, Beijing, China.

GB 50936-2014, 2014, “Technical Code for Concrete Filled Steel Tubular Structures,” Ministry of Housing and Urban-Rural Development of the People’s Republic of China, Beijing, China.

Han, L.-H.; Wang, W.-D.; and Tao, Z., 2011, “Performance of Circular CFST Column to Steel Beam Frames under Lateral Cyclic Loading,” Journal of Constructional Steel Research, V. 67, No. 5, pp. 876-890. doi: 10.1016/j.jcsr.2010.11.020

JGJ 3-2010, 2010, “Technical Specification for Concrete Structures of Tall Building,” Ministry of Housing and Urban-Rural Development of the People’s Republic of China, Beijing, China.

JGJ 149-2017, 2017, “Technical Specification for Concrete Structures with Specially Shaped Columns,” Ministry of Housing and Urban-Rural Development of the People’s Republic of China, Beijing, China.

Li, B.; Yang, X. Y.; and Gao, C. Y., 2015, “Pseudo-Static Experimental Research of the Concrete-Filled Rectangular Steel Tubular Frame,” Journal of Xi’an University of Architecture and Technology, V. 47, No. 3, pp. 321-326.

Li, Y. T.; Xu, C. X.; and Du, G. F., 2014, “Seismic Performance of T-Shaped CFT Column to Steel Frame Beam Connection—Experimental Study,” Advanced Materials Research, V. 919-921, pp. 951-959. doi: 10.4028/www.scientific.net/AMR.919-921.951

Lin, Z. Y.; Shen, Z. Y.; and Luo, J. H., 2009, “Hysteretic Behavior of Concrete-Filled L-Section Steel Tubular Columns under Cyclic Loading,” Progress in Steel Building Structures, V. 11, No. 2, pp. 12-17. (in Chinese)

Liu, J. C.; Yang, Y. L.; Liu, J. P.; and Zhou, X. H., 2017, “Experimental Investigation of Special-Shaped Concrete-Filled Steel Tubular Column to Steel Beam Connections under Cyclic Loading,” Engineering Structures, V. 151, pp. 68-84. doi: 10.1016/j.engstruct.2017.07.021

Liu, J. X.; Dai, S. B.; Huo, K. C.; Huang, J.; and Lin, M. S., 2015, “Study on Earthquake Resistance Behavior of Top and Seat Angle Joint of Special-Shaped Concrete-Filled Rectangular Composite Tubular Column with Steel Beam,” Journal of Sichuan University, V. 47, No. 1, pp. 128-137. (in Chinese)

Liu, X. G.; Xu, C. Z.; Liu, J. P.; and Yang, Y. L., 2018, “Research on Special-Shaped Concrete-Filled Steel Tubular Columns under Axial Compression,” Journal of Constructional Steel Research, V. 147, pp. 203-223. doi: 10.1016/j.jcsr.2018.04.014

Mander, J. B.; Priestley, M. J. N.; and Park, R., 1988, “Theoretical Stress-Strain Model for Confined Concrete,” Journal of Structural Engineering, ASCE, V. 114, No. 8, pp. 1804-1826. doi: 10.1061/(ASCE)0733-9445(1988)114:8(1804)

Mazzoni, S.; Mckenna, F.; Scott, M. H; and Fenves, G. L., 2006, “OpenSEES Command Language Manual,” https://opensees.berkeley.edu/OpenSees/manuals/usermanual/OpenSeesCommandLanguageManualJune2006.pdf. (last accessed Mar. 14, 2022)

Ren, F. M.; Zhou, Y.; Zhang, J. B.; and Lin, S. M., 2013, “Experimental Study on Seismic Performance of CFST Frame Structures with Energy Dissipation Devices,” Journal of Constructional Steel Research, V. 90, pp. 120-132. doi: 10.1016/j.jcsr.2013.07.032

Tang, X.; Yang, Y. L.; Yang, W. Q.; Lanning, J.; and Chen, Y. F., 2021, “Experimental and Numerical Investigation on the Seismic Behavior of Plane Frames with Special-Shaped Concrete-Filled Steel Tubular Columns,” Journal of Building Engineering, V. 35, p. 102070. doi: 10.1016/j.jobe.2020.102070

Wang, D., and Lv, X. L., 2005, “Experimental Study on Seismic Behavior of Concrete-Filled Steel T-Section and L-Section Columns,” Journal of Building Structures, V. 26, No. 4, pp. 39-44. (in Chinese)

Xu, C. X.; Wu, Z. J.; and Zeng, L., 2011, “Experimental Research on Seismic Behaviors of T-Shaped Concrete-Filled Steel Tubular Frame Joints,” Advanced Materials Research, V. 368-373, pp. 38-41.

Yang, Y.; Yang, W.; Tang, X.; and Cheng, Y., 2021, “Seismic Behavior of Plane Frame with Special-Shaped CFST Columns, H-Shaped Steel Beams and Vertical Rib Connections,” Structures, V. 31, pp. 721-739. doi: 10.1016/j.istruc.2021.02.017

Yang, Y. L., 2011, “Study on Mechanical Properties of T-Shaped Composite Columns,” Harbin Institute of Technology, Harbin, China.

Yang, Y. L.; Wang, Y. Y.; Fu, F.; and Liu, J. C., 2015, “Static Behavior of T-Shaped Concrete-Filled Steel Tubular Columns Subjected to Concentric and Eccentric Compressive Loads,” Thin-Walled Structures, V. 95, pp. 374-388. doi: 10.1016/j.tws.2015.07.009

Zhang, J. C.; Shen, Z. Y.; Lin, Z. Y.; and Luo, J. H., 2010, “Experimental Research on Seismic Behavior of Concrete-Filled L-Shaped Steel Tubular Frames,” Journal of Building Structures, V. 31, No. 8, pp. 1-7. (in Chinese)

Zhou, T.; Chen, Z. H.; and Liu, H. B., 2012, “Seismic behavior of special shaped column composed of concrete filled steel tubes,” Journal of Constructional Steel Research, V. 75, No. 75, pp. 131-141. doi: 10.1016/j.jcsr.2012.03.015

Zhou, T.; Jia, Y. M.; Xu, M. X.; Wang, X. D.; and Chen, Z. H., 2015, “Experimental Study on the Seismic Performance of L-Shaped Column Composed of Concrete-Filled Steel Tubes Frame Structures,” Journal of Constructional Steel Research, V. 114, pp. 77-88. doi: 10.1016/j.jcsr.2015.07.009

Zuo, Z. L.; Cai, J.; Yang, C.; and Chen, Q. J., 2012b, “Eccentric Load Behavior of L-Shaped CFT Stub Columns with Binding Bars,” Journal of Constructional Steel Research, V. 72, pp. 105-118. doi: 10.1016/j.jcsr.2011.11.003

Zuo, Z. L.; Cai, J.; Yang, C.; Chen, Q. J.; and Sun, G., 2012a, “Axial Load Behavior of L-Shaped CFT Stub Columns with Binding Bars,” Engineering Structures, V. 37, No. 5, pp. 88-98. doi: 10.1016/j.engstruct.2011.12.042


ALSO AVAILABLE IN:

Electronic Structural Journal