Analytical and Parametric Studies on Flexural Performance of Reinforced Concrete Beams Strengthened by Fiber- Reinforced Geopolymer Composites

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Analytical and Parametric Studies on Flexural Performance of Reinforced Concrete Beams Strengthened by Fiber- Reinforced Geopolymer Composites

Author(s): Ernesto J. Guades and Henrik Stang

Publication: Structural Journal

Volume: 119

Issue: 3

Appears on pages(s): 99-116

Keywords: analytical study; geopolymer composites; jacketed reinforced concrete (RC) beams; parametric study; repair and strengthening

DOI: 10.14359/51734487

Date: 5/1/2022

Abstract:
This paper presents an analytical method to predict the flexural performance of reinforced concrete (RC) beams strengthened by fiber-reinforced geopolymer composites (FRGC). In addition, a parametric study was performed to determine the effect of the thickness and tensile strength of the strengthening material on the moment, ductility, and energy absorption capacity of the composite beam. The proposed model adopts sectional strip discretization and incorporates the constitutive relationship of each component material. The strengthening configurations considered in the analysis include bottom, two-sided, and three-sided jackets. Four failure conditions were simulated to account for the original failure of the RC beam and are described in terms of the steel reinforcement ratio in the range of 0.87 to 2.29%. The result showed a good agreement between the predicted and experimental values and that the proposed analytical method can be used to predict the momentcurvature response. The parametric study revealed that the change in the moment and ductility value is more sensitive in the variation of FRGC thickness than the tensile strength regardless of the jacketing configurations and failure type of the unstrengthened beam.

Related References:

1. Sakr, M.; El Naggar, M. H.; and Nehdi, M., “Interface Characteristics and Laboratory Constructability Tests of Novel Fiber-Reinforced Polymer/Concrete Piles,” Journal of Composites for Construction, ASCE, V. 9, No. 3, June 2005, pp. 274-283. doi: 10.1061/(ASCE)1090-0268(2005)9:3(274)

2. Bencardino, F., and Condello, A., “Innovative Solution to Retrofit RC Members: Inhibiting-Repairing-Strengthening (IRS),” Construction and Building Materials, V. 117, Aug. 2016, pp. 171-181. doi: 10.1016/j.conbuildmat.2016.05.053

3. Donnini, J., and Corinaldesi, V., “Concrete Columns Confined with Different Composite Materials,” MATEC Web of Conferences, V. 199, International Conference on Concrete Repair, Rehabilitation and Retrofitting (ICCRRR 2018), 2018, Article No. 09012, 5 pp.

4. Jawdhari, A.; Fam, A.; and Harik, I., “Bond between CFRP Rod Panels and Concrete Using Cementitious Mortar,” Construction and Building Materials, V. 235, Feb. 2020, Article No. 117503, 12 pp. doi: 10.1016/j.conbuildmat.2019.117503

5. Jawdhari, A.; Semendary, A.; Fam, A.; Khoury, I.; and Steinberg, E., “Bond Characteristics of CFRP Rod Panels Adhered to Concrete under Bending Effects,” Journal of Composites for Construction, ASCE, V. 23, No. 1, Feb. 2019, p. 0401807712. doi: 10.1061/(ASCE)CC.1943-5614.0000909

6. Jawdhari, A.; Harik, I.; and Fam, A., “Behavior of Reinforced Concrete Beams Strengthened with CFRP Rod Panels CRP 195,” Structures, V. 16, Nov. 2018, pp. 239-253. doi: 10.1016/j.istruc.2018.09.014

7. Ding, Y., and Bai, Y.-L., “Fracture Properties and Softening Curves of Steel Fiber-Reinforced Slag-Based Geopolymer Mortar and Concrete,” Materials (Basel), V. 11, No. 8, 2018, p. 1445. doi: 10.3390/ma11081445

8. Alanazi, H.; Yang, M.; Zhang, D.; and Gao, Z. J., “Bond Strength of PCC Pavement Repairs Using Metakaolin-Based Geopolymer Mortar,” Cement and Concrete Composites, V. 65, Jan. 2016, pp. 75-82. doi: 10.1016/j.cemconcomp.2015.10.009

9. Hu, S.; Wang, H.; Zhang, G.; and Ding, Q., “Bonding and Abrasion Resistance of Geopolymeric Repair Material Made with Steel Slag,” Cement and Concrete Composites, V. 30, No. 3, Mar. 2008, pp. 239-244. doi: 10.1016/j.cemconcomp.2007.04.004

10. Yudhbir, and Honjo, Y., “Applications of Geotechnical Engineering to Environmental Control,” Proceedings of the Ninth Asian Regional Conference in Soil Mechanics and Foundation Engineering, V. 2, Dec. 1991, Bangkok, Thailand, pp. 431-466.

11. Ishak, N. I.; Johari, M. A. M.; and Hashim, S. F. S., “Effects of Using Blended Binder of RHA and GGBS on the Properties of Concrete: A Review,” AIP Conference Proceedings, V. 1892, No. 1, 2017, p. 020027. doi: 10.1063/1.5005658

12. Kuenzel, C.; Neville, T. P.; Donatello, S.; Vandeperre, L.; Boccaccini, A. R.; and Cheeseman, C. R., “Influence of Metakaolin Characteristics on the Mechanical Properties of Geopolymers,” Applied Clay Science, V. 83-84, Oct. 2013, pp. 308-314. doi: 10.1016/j.clay.2013.08.023

13. Zheng, Z., and Feldman, D., “Synthetic Fibre-Reinforced Concrete,” Progress in Polymer Science, V. 20, No. 2, 1995, pp. 185-210. doi: 10.1016/0079-6700(94)00030-6

14. Bhutta, A.; Farooq, M.; and Banthia, N., “Matrix Hybridization Using Waste Fuel Ash and Slag in Alkali-Activated Composites and Its Influence on Maturity of Fiber-Matrix Bond,” Journal of Cleaner Production, V. 177, Mar. 2018, pp. 857-867. doi: 10.1016/j.jclepro.2018.01.001

15. Sukontasukkul, P.; Pongsopha, P.; Chindaprasirt, P.; and Songpiriyakij, S., “Flexural Performance and Toughness of Hybrid Steel and Polypropylene Fibre Reinforced Geopolymer,” Construction and Building Materials, V. 161, Feb. 2018, pp. 37-44. doi: 10.1016/j.conbuildmat.2017.11.122

16. Adam, A. A., and Horianto, X. X. X., “The Effect of Temperature and Duration of Curing on the Strength of Fly Ash Based Geopolymer Mortar,” Procedia Engineering, V. 95, 2014, pp. 410-414.

17. Olivia, M., and Nikraz, H., “Properties of Fly Ash Geopolymer Concrete Designed by Taguchi Method,” Materials & Design, V. 36, Apr. 2012, pp. 191-198. doi: 10.1016/j.matdes.2011.10.036

18. Kong, D. L. Y., and Sanjayan, J. G., “Damage Behavior of Geopolymer Composites Exposed to Elevated Temperatures,” Cement and Concrete Composites, V. 30, No. 10, Nov. 2008, pp. 986-991. doi: 10.1016/j.cemconcomp.2008.08.001

19. Cui, Y.; Kayali, O.; Zhao, T.; and Zhang, C., “Bond Strength of Steel Bar and Plain or Fiber-Reinforced Geopolymer Concrete,” Proceedings of the 2017 World Congress on Advances in Structural Engineering and Mechanics, 2017, Seoul, South Korea, pp. 1-14.

20. Matthews, J.; Selvakumar, A.; Vaidya, S.; and Condit, W., “Large-Diameter Sewer Rehabilitation Using a Spray-Applied Fiber-Reinforced Geopolymer Mortar,” Practice Periodical on Structural Design and Construction, ASCE, V. 20, No. 4, Nov. 2015, p. 04014050. doi: 10.1061/(ASCE)SC.1943-5576.0000246

21. Müller, S., and Mechtcherine, V., “Use of Strain-Hardening Cement-Based Composites (SHCC) for Retrofitting,” MATEC Web of Conferences, V. 199, International Conference on Concrete Repair, Rehabilitation and Retrofitting (ICCRRR 2018), 2018, Article No. 09006, 6 pp.

22. Al-Majidi, M. H.; Lampropoulos, A. P.; Cundy, A. B.; Tsioulou, O. T.; and Al-Rekabi, S., “A Novel Corrosion Resistant Repair Technique for Existing Reinforced Concrete (RC) Elements Using Polyvinyl Alcohol Fibre Reinforced Geopolymer Concrete (PVAFRGC),” Construction and Building Materials, V. 164, Mar. 2018, pp. 603-619. doi: 10.1016/j.conbuildmat.2017.12.213

23. Zaher, Y. A., and Abdel Aziz, Y. H., “Effect of Elevated Temperature on RC Pre-Cracked Beams Repaired and Strengthened Using Jackets of Cementitious Materials,” International Journal of Civil Engineering and Technology, V. 8, No. 5, 2017, pp. 819-831.

24. Guades, E. J.; Stang, H.; Schmidt, J. W.; and Fischer, G., “Flexural Behavior of Hybrid Fibre-Reinforced Geopolymer Composites (FRGC)-Jacketed RC Beams,” Engineering Structures, V. 235, May 2021, Article No. 112053, 16 pp. doi: 10.1016/j.engstruct.2021.112053

25. Mohammad, M., and Zahari, R. A., “Structural Repair to Conserve Langkawi’s Main Tourist Attraction: Practical Approach,” MATEC Web of Conferences, V. 199, International Conference on Concrete Repair, Rehabilitation and Retrofitting (ICCRRR 2018), 2018, Article No. 10009, 6 pp.

26. Hognestad, E.; Hanson, N. W.; and McHenry, D., “Concrete Stress Distribution in Ultimate Strength Design,” ACI Journal Proceedings, V. 52, No. 12, Dec. 1955, pp. 455-480.

27. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19),” American Concrete Institute, Farmington Hills, MI, 2019, 624 pp.

28. Yuan, F.; Pan, J.; and Leung, C. K. Y., “Flexural Behaviors of ECC and Concrete/ECC Composite Beams Reinforced with Basalt Fiber-Reinforced Polymer,” Journal of Composites for Construction, ASCE, V. 17, No. 5, Oct. 2013, pp. 591-602. doi: 10.1061/(ASCE)CC.1943-5614.0000381

29. Naaman, A. E. and Reinhardt, H. W., High Performance Fiber Reinforced Cement Composites 2 (HPFRCC 2): Proceedings of the Second International RILEM Workshop, CRC Press, Boca Raton, FL, 1996, 528 pp.


ALSO AVAILABLE IN:

Electronic Structural Journal