Title: Tales From the Road

Author(s): Folliard

Publication: Web Session

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 10/17/2021

Abstract:
This presentation recounts various lessons learned, both personally and professionally, over 20+ years of friendship and collaboration with Michael Thomas. This presentation will primarily focus on field trials focusing on the prevention or mitigation of ASR in field structures throughout the United States, but other selected aspects of our long journey will be highlighted. What a long, strange trip it’s been!