Title: Contributions of M. D. A. Thomas to PCA Research

Author(s): Wilson

Publication: Web Session

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 10/17/2021

Abstract:
For over 25 years, Michael Thomas has been involved with PCA research and education involving concrete durability. Topics have included Use of SCMs, DEF, Sulfate Resistance, Marine Exposures, ASR, and Portland Limestone Cements. This session will highlight some of his more notable works that have greatly influenced the development of cement and concrete technology.