Mitigation of Alkali-Silica Reaction in Concrete Using Novel pH Reducing Admixtures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Mitigation of Alkali-Silica Reaction in Concrete Using Novel pH Reducing Admixtures

Author(s): Kaladharan

Publication: Web Session

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 10/17/2021

Abstract:
Presented By: Gopakumar Kaladharan, Pennsylvania State University