Development of Fault-Detection ANNs for Structural Damage Prediction

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Development of Fault-Detection ANNs for Structural Damage Prediction

Author(s): Mohammad H. AlHamaydeh, Ahmed F. Mohamed, and Mahmoud I. Awad

Publication: Symposium Paper

Volume: 350

Issue:

Appears on pages(s): 45-53

Keywords: structural damage, profile monitoring, fault detection, artificial neural network

DOI: 10.14359/51734311

Date: 11/1/2021

Abstract:
Structural systems are critical components of modern societies, and as such, need constant condition assessments. Incurred damage and its accumulation due to various loading conditions may lead to complete structural failures with safety consequences. Thus, damage assessment and early fault detection are essential to decision-makers for strategic planning, performing resource-allocation, and obtaining the logistics of these systems. In this article, a data-driven methodology using fault detection of structural systems is proposed. This method utilizes Artificial Neural Networks (ANNs) to model damage due to earthquake loading using sophisticated nonlinear analyses of structures. As a proof-of-concept, the ANN approach for damage-detection is applied to a typical four-story reinforced concrete (RC) structure having varied concrete strengths. The approach is found to have a high potential for successful anomaly identification in RC structural systems.

Related References:

1. N. M. Vichare and M. G. Pecht, “Prognostics and health management of electronics,” IEEE Trans. components Packag. Technol., vol. 29, no. 1, pp. 222–229, 2006.

2. A. Amiri, W. A. Jensen, and R. B. Kazemzadeh, “A case study on monitoring polynomial profiles in the automotive industry,” Qual. Reliab. Eng. Int., vol. 26, no. 5, pp. 509–520, 2010.

3. S. S. Fan, Y. Chang, and N. Aidara, “Nonlinear profile monitoring of reflow process data based on the sum of sine functions,” Qual. Reliab. Eng. Int., vol. 29, no. 5, pp. 743–758, 2013.

4. M. I. Awad, M. AlHamaydeh, and A. Faris, “Fault detection via nonlinear profile monitoring using artificial neural networks,” Qual. Reliab. Eng. Int., vol. 34, no. 6, pp. 1195–1210, 2018.

5. K. Yavuz and E. Şafak, “Real-Time Structural Health Monitoring and Damage Detection,” in Topics in Dynamics of Civil Structures, Volume 4, New York: Springer-Verlag, 2013, pp. 11–19.

6. Y. Liao, K. Balafas, A. Kiremidjian, R. Rajagopal, and C.-H. Loh, “Application of acceleration-based damage detection algorithms to experimental data from multi-story steel structures,” in 2015 International Workshop on Structural Health Monitoring, 2015.

7. Y. C. Huh, T. Y. Chung, S. J. Moon, H. G. Kil, and J. K. Kim, “Damage detection in beams using vibratory power estimated from the measured accelerations,” J. Sound Vib., vol. 330, no. 15, pp. 3645–3665, 2011.

8. N. T. Khiem and L. K. Toan, “A novel method for crack detection in beam-like structures by measurements of natural frequencies,” J. Sound Vib., vol. 333, no. 18, pp. 4084–4103, 2014.

9. K. H. Barad, D. S. Sharma, and V. Vyas, “Crack detection in cantilever beam by frequency based method,” procedia Eng., vol. 51, pp. 770–775, 2013.

10. K. S. C. Kuang, “Distributed damage detection of offshore steel structures using plastic optical fibre sensors,” Sensors Actuators A Phys., vol. 229, pp. 59–67, 2015.

11. J. Sładek, K. Ostrowska, P. Kohut, K. Holak, A. Gąska, and T. Uhl, “Development of a vision based deflection measurement system and its accuracy assessment,” Measurement, vol. 46, no. 3, pp. 1237–1249, 2013.

12. J. Guo and C. Zhu, “Dynamic displacement measurement of large-scale structures based on the Lucas–Kanade template tracking algorithm,” Mech. Syst. Signal Process., vol. 66, pp. 425–436, 2016.

13. J.-T. Kim, J.-H. Park, K.-Y. Koo, and J.-J. Lee, “Acceleration-based neural networks algorithm for damage detection in structures,” Smart Struct. Syst., vol. 4, no. 5, pp. 583–603, 2008.

14. P. Zhou, Y. Zhao, Z. Zhao, and T. Chai, “Source mapping and determining of soil contamination by heavy metals using statistical analysis, artificial neural network, and adaptive genetic algorithm,” J. Environ. Chem. Eng., vol. 3, no. 4, pp. 2569–2579, 2015.

15. J.-H. Park, J.-T. Kim, D.-S. Hong, D.-D. Ho, and J.-H. Yi, “Sequential damage detection approaches for beams using time-modal features and artificial neural networks,” J. Sound Vib., vol. 323, no. 1–2, pp. 451–474, 2009.

16. Liu, C., Wu, X., Wu, N., & Liu, C. (2014). Structural Damage Identification Based on Rough Sets and Artificial Neural Network. The Scientifi World Journal, doi: http://dx.doi.org/10.1155/2014/193284

17. Yang, J., Zhang, L., Chen, C., Li, Y., Li, R., Wang, G., . . . Zeng, Z. (2020). A hierarchical deep convolutional neural network and gatedrecurrent unit framework for structural damage detection Infrmation Sciences, 540: 117-130.

18. A. M. Reinhorn et al., “IDARC2D Version 7.0: A Program for the Inelastic Damage Analysis of Structures (MCEER-09-0006),” Multidisciplinary center for earthquake engineering research (MCEER …, 2009.

19. M. AlHamaydeh, M. Najib, and L. Elayyan, “INSPECT-Lite: A GUI Pre-Processor Package for IDARC-2D Ver 7.0,” in The 2015 World Congress on Advances in Structural Engineering and Mechanics (ASEM15), August 25, 2015, vol. 29.

20. M. AlHamaydeh, M. Najib, and S. Alawnah, “INSPECT: a graphical user interface software package for IDARC-2D,” SoftwareX, vol. 5, pp. 243–251, 2016.

21. M. H. Al Satari, “Estimation of seismic response demands for RC framed structures,” University of Southern California, 2005.

22. M. Al Satari, Estimation of seismic response demands for R/C framed structures: an insight into the nonlinear seismic behavior. VDM Verlag, Saarbrücken, Germany, 2008.

23. M. Al Satari and J. Anderson, “Nonlinearity effects on the seismic behavior of RC framed structures,” in The 76th SEAOC Annual Convention, September 26-29, 2007.

24. M. AlHamaydeh and G. Al-Shamsi, “Development of analytical fragility curves for representative buildings in Dubai, United Arab Emirates,” in The International Conference on Earthquake Engineering; Skopje Earthquake - 50 Years of European Earthquake Engineering (SE-50EEE), May 29-31, 2013.

25. M. Al Satari and J. Anderson, “Estimating inelastic seismic demands by elastic analysis for reinforced concrete (RC) framed structures,” in The 75th SEAOC Annual Convention, September 13-16, 2006, pp. 153–167.

26. M. AlHamaydeh, N. Aly, and K. Galal, “Impact of seismicity on performance and cost of RC shear wall buildings in Dubai, United Arab Emirates,” ASCE, J. Perform. Constr. Facil., no., 2017 doi: 10.1061/(ASCE)CF.1943-5509.0001079

27. M. AlHamaydeh, N. Aly, and K. Galal, “Seismic response and life-cycle cost of reinforced concrete special structural wall buildings in Dubai, UAE,” Struct. Concr., pp. 1–12, 2017, doi: 10.1002/suco.201600177

28. N. Aly, M. AlHamaydeh, and K. Galal, “Quantification of the impact of detailing on the performance and cost of RC shear wall buildings in regions with high uncertainty in seismicity hazards,” J. Earthq. Eng., pp. 1-26., 2018. doi: 10.1080/13632469.2018.1453406

29. M. AlHamaydeh, S. Abdullah, A. Hamid, and A. Mustapha, “Seismic design factors for RC special moment resisting frames in Dubai, UAE,” Earthq. Eng. Eng. Vib., vol. 10, no. 4, pp. 495–506, 2011.

30. M. AlHamaydeh, J. Abdalla, S. Abdalla, A. Al-Rahmani, and A. Mostafa, “Inelastic seismic demands for reinforced concrete frames in Dubai,” in The 14th European Earthquake Engineering Conference (14EEEC), Aug. 30-Sept. 3, 2010.

31. M. AlHamaydeh, N. Aly, and K. Galal, “Effect of diverse seismic hazard estimates on design and performance of RC shear wall buildings in Dubai, UAE,” in The 2015 World Congress on Advances in Structural Engineering and Mechanics (ASEM15), August 25-29, 2015.

32. W. H. Woodall, D. J. Spitzner, D. C. Montgomery, and S. Gupta, “Using control charts to monitor process and product quality profiles,” J. Qual. Technol., vol. 36, no. 3, pp. 309–320, 2004.

33. M. AlHamaydeh, S. Yehia, N. Aly, A. Douba, and L. Hamzeh, “Design alternatives for lateral forceresisting systems of tall buildings in Dubai, UAE,” Int. J. Civ. Environ. Eng., vol. 6, pp. 185–188, 2012.

34. M. Awad, M. AlHamaydeh, and A. F. Mohamed, “Structural damage fault detection using Artificial Neural network profile monitoring,” in 2017 7th International Conference on Modeling, Simulation, and Applied Optimization (ICMSAO), 2017, pp. 1–6.

35. M. AlHamaydeh, K. Wong, R. Fernandes, J. Seok, E. Abdel-Rahman, and S. El-Borgi, “Structural health monitoring using time-delay embedding and phase-space warping,” in The 5th International Conference on Computational Methods in Structural Dynamics and Earthquake Engineering (COMPDYN2015), 2015, pp. 2568–2575.

36. A. F. Mohamed, “Non-linear profile monitoring using artificial neural network fault detection,” M.Sc. thesis, Engineering Systems Management, College of Engineering, American Univeristy of Sharjah, 2018.