A New Mixture Proportioning Method for Performance- Based Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: A New Mixture Proportioning Method for Performance- Based Concrete

Author(s): K. Bharadwaj, O. B. Isgor, W. J. Weiss, K. S. T. Chopperla, A. Choudhary, G. D. Vasudevan, D. Glosser, J. H. Ideker, and D. Trejo

Publication: Materials Journal

Volume: 119

Issue: 2

Appears on pages(s): 207-220

Keywords: durability; mixture proportioning; supplementary cementitious materials (SCMs); thermodynamic modeling

DOI: 10.14359/51734301

Date: 3/1/2022

Abstract:
A new mixture proportioning method is developed for performance-based concrete with supplementary cementitious materials (SCMs). The method is based on the thermodynamic calculations of the properties for concrete and identifying the mixtures that satisfy a predefined set of performance criteria. This new approach considers the chemical composition and reactivity of SCMs while proportioning concrete mixtures. Performance criteria examples are shown for a bridge deck (corrosion and freezing-and-thawing damage), an unreinforced pavement (salt damage), and a foundation (moderate sulfate and alkali-aggregate reaction). The method is used to proportion concrete mixtures satisfying these three performance criteria using four ashes per mixture. Experiments show that these mixtures met the targets. The proposed approach can proportion mixtures that are optimized for predefined performance using a wide range of SCMs, which can be useful in reducing the cost and carbon footprint of concrete.

Related References:

1. ACI Committee 211, “Standard Practice for Selecting Proportions for Normal, Heavyweight, and Mass Concrete (ACI 211.1-91) (Reapproved 2009),” American Concrete Institute, Farmington Hills, MI, 1991, 38 pp.

2. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 520 pp.

3. INDOT, “Standard Specifications,” Indiana Department of Transportation, Indianapolis, IN, 2020, 1246 pp.

4. Papadakis, V. G., “Experimental Investigation and Theoretical Modeling of Silica Fume Activity in Concrete,” Cement and Concrete Research, V. 29, No. 1, 1999, pp. 79-86. doi: 10.1016/S0008-8846(98)00171-9

5. Papadakis, V. G., “Effect of Fly Ash on Portland Cement Systems: Part I. Low-Calcium Fly Ash,” Cement and Concrete Research, V. 29, No. 11, 1999, pp. 1727-1736. doi: 10.1016/S0008-8846(99)00153-2

6. Papadakis, V. G., “Effect of Fly Ash on Portland Cement Systems: Part II. High-Calcium Fly Ash,” Cement and Concrete Research, V. 30, No. 10, 2000, pp. 1647-1654. doi: 10.1016/S0008-8846(00)00388-4

7. Papadakis, V. G., and Tsimas, S., “Supplementary Cementing Materials in Concrete: Part I: Efficiency and Design,” Cement and Concrete Research, V. 32, No. 10, 2002, pp. 1525-1532. doi: 10.1016/S0008-8846(02)00827-X

8. BS EN 206-1:2000, “Concrete—Part 1: Specification, Performance, Production and Conformity,” British Standards Institution, London, UK, 2000, 74 pp.

9. ASTM C618-19, “Standard Specification for Coal Fly Ash and Raw or Calcined Natural Pozzolan for Use in Concrete,” ASTM International, West Conshohocken, PA, 2019, 5 pp.

10. Glosser, D.; Choudhary, A.; Isgor, O. B.; and Weiss, W. J., “Investigation of Reactivity of Fly Ash and Its Effect on Mixture Properties,” ACI Materials Journal, V. 116, No. 4, July 2019, pp. 193-200. doi: 10.14359/51716722

11. Glosser, D.; Suraneni, P.; Isgor, O. B.; and Weiss, W. J., “Estimating Reaction Kinetics of Cementitious Pastes Containing Fly Ash,” Cement and Concrete Composites, V. 112, Sept. 2020, p. 103655. doi: 10.1016/j.cemconcomp.2020.103655

12. Glosser, D. B., “Equilibrium and Non-Equilibrium Thermodynamic Modeling of Cement Pastes Containing Supplementary Cementitious Materials,” PhD thesis, Oregon State University, Corvallis, OR, 2020, 206 pp.

13. Suraneni, P.; Hajibabaee, A.; Ramanathan, S.; Wang, Y.; and Weiss, J., “New Insights from Reactivity Testing of Supplementary Cementitious Materials,” Cement and Concrete Composites, V. 103, Oct. 2019, pp. 331-338. doi: 10.1016/j.cemconcomp.2019.05.017

14. Bharadwaj, K.; Glosser, D.; Moradllo, M. K.; Isgor, O. B.; and Weiss, W. J., “Toward the Prediction of Pore Volumes and Freeze-Thaw Performance of Concrete Using Thermodynamic Modelling,” Cement and Concrete Research, V. 124, Oct. 2019, Article No. 105820. doi: 10.1016/j.cemconres.2019.105820

15. Snyder, K. A., “The Relationship Between the Formation Factor and the Diffusion Coefficient of Porous Materials Saturated With Concentrated Electrolytes: Theoretical and Experimental Considerations,” Concrete Science and Engineering, V. 3, No. 12, 2001, pp. 216-224.

16. Weiss, W. J.; Barrett, T. J.; Qiao, C.; and Todak, H., “Toward a Specification for Transport Properties of Concrete Based on the Formation Factor of a Sealed Specimen,” Advances in Civil Engineering Materials, V. 5, No. 1, 2016, pp. 179-194. doi: 10.1520/ACEM20160004

17. Weiss, W. J.; Spragg, R. P.; Isgor, O. B.; Ley, M. T.; and Van Dam, T., “Toward Performance Specifications for Concrete: Linking Resistivity, RCPT and Diffusion Predictions Using the Formation Factor for Use in Specifications,” High Tech Concrete: Where Technology and Engineering Meet—Proceedings of the 2017 fib Symposium, held in Maastricht, The Netherlands, June 12-14, 2017, D. A. Hordijk and M. Luković, eds., Springer, Cham, Switzerland, 2018, pp. 2057-2065.

18. Ghods, P.; Isgor, O. B.; McRae, G.; and Miller, T., “The Effect of Concrete Pore Solution Composition on the Quality of Passive Oxide Films on Black Steel Reinforcement,” Cement and Concrete Composites, V. 31, No. 1, 2009, pp. 2-11. doi: 10.1016/j.cemconcomp.2008.10.003

19. Thomas, M., Supplementary Cementing Materials in Concrete, CRC Press, Boca Raton, FL, 2013, 210 pp.

20. Lothenbach, B.; Scrivener, K.; and Hooton, R. D., “Supplementary Cementitious Materials,” Cement and Concrete Research, V. 41, No. 12, 2011, pp. 1244-1256. doi: 10.1016/j.cemconres.2010.12.001

21. Fagerlund, G., “The Critical Degree of Saturation Method of Assessing the Freeze/Thaw Resistance of Concrete,” Materials and Structures, V. 10, No. 4, 1977, pp. 217-229.

22. Li, W.; Pour-Ghaz, M.; Castro, J.; and Weiss, J., “Water Absorption and Critical Degree of Saturation Relating to Freeze-Thaw Damage in Concrete Pavement Joints,” Journal of Materials in Civil Engineering, ASCE, V. 24, No. 3, 2012, pp. 299-307. doi: 10.1061/(ASCE)MT.1943-5533.0000383

23. Todak, H. N., “Durability Assessments of Concrete Using Electrical Properties and Acoustic Emission Testing,” master’s thesis, Purdue University, West Lafayette, IN, 2015.

24. Todak, H.; Lucero, C.; and Weiss, W. J., “Why is the Air There? Thinking about Freeze-Thaw in Terms of Saturation,” Concrete InFocus, 2015, pp. 27-33.

25. Jones, W.; Farnam, Y.; Imbrock, P.; Spiro, J.; Villani, C.; Golias, M.; Olek, J.; and Weiss, W. J., “An Overview of Joint Deterioration in Concrete Pavement: Mechanisms, Solution Properties, and Sealers,” Purdue University, West Lafayette, IN, 2013, 69 pp.

26. Castro, J.; Li, W.; Pour-Ghaz, M.; Golias, M.; Tao, B.; Sun, H.; and Weiss, W. J., “Durability of Saw-Cut Joints in Plain Cement Concrete Pavements,” Joint Transportation Research Program, Purdue University, West Lafayette, IN, 2011, 42 pp.

27. Suraneni, P.; Azad, V. J.; Isgor, O. B.; and Weiss, W. J., “Calcium Oxychloride Formation in Pastes Containing Supplementary Cementitious Materials: Thoughts on the Role of Cement and Supplementary Cementitious Materials Reactivity,” RILEM Technical Letters, V. 1, May 2016, pp. 24-30. doi: 10.21809/rilemtechlett.2016.7

28. Suraneni, P.; Azad, V. J.; Isgor, O. B.; and Weiss, W. J., “Use of Fly Ash to Minimize Deicing Salt Damage in Concrete Pavements,” Transportation Research Record: Journal of the Transportation Research Board, V. 2629, No. 1, 2017, pp. 24-32. doi: 10.3141/2629-05

29. Monical, J.; Unal, E.; Barrett, T.; Farnam, Y.; and Weiss, W. J., “Reducing Joint Damage in Concrete Pavements: Quantifying Calcium Oxychloride Formation,” Transportation Research Record: Journal of the Transportation Research Board, V. 2577, No. 1, 2016, pp. 17-24. doi: 10.3141/2577-03

30. Suraneni, P.; Azad, V. J.; Isgor, O. B.; and Weiss, W. J., “Deicing Salts and Durability of Concrete Pavements and Joints,” Concrete International, V. 38, No. 4, Apr. 2016, pp. 48-54.

31. Suraneni, P.; Monical, J.; Unal, E.; Farnam, Y.; and Weiss, J., “Calcium Oxychloride Formation Potential in Cementitious Pastes Exposed to Blends of Deicing Salt,” ACI Materials Journal, V. 114, No. 4, July-Aug. 2017, pp. 631-641. doi: 10.14359/51689607

32. Suraneni, P.; Salgado, N.; Carolan, H.; Li, C.; Azad, V. J.; Isgor, O. B.; Ideker, J. H.; and Weiss, W. J., “Mitigation of Deicer Damage in Concrete Pavements Caused by Calcium Oxychloride Salt Formation—Use of Ground Lightweight Aggregates,” Proceedings, International RILEM Conference on Materials, Systems and Structures in Civil Engineering, Lyngby, Denmark, 2016.

33. Whatley, S. N.; Suraneni, P.; Azad, V. J.; Isgor, O. B.; and Weiss, J., “Mitigation of Calcium Oxychloride Formation in Cement Pastes Using Undensified Silica Fume,” Journal of Materials in Civil Engineering, ASCE, V. 29, No. 10, 2017, p. 04017198. doi: 10.1061/(ASCE)MT.1943-5533.0002052

34. Farnam, Y.; Wiese, A.; Bentz, D.; Davis, J.; and Weiss, J., “Damage Development in Cementitious Materials Exposed to Magnesium Chloride Deicing Salt,” Construction and Building Materials, V. 93, Sept. 2015, pp. 384-392. doi: 10.1016/j.conbuildmat.2015.06.004

35. ASTM C1778-06, “Standard Guide for Reducing the Risk of Deleterious Alkali-Aggregate Reaction in Concrete,” ASTM International, West Conshohocken, PA, 2006, 11 pp.

36. ASTM C1778-20, “Standard Guide for Reducing the Risk of Deleterious Alkali-Aggregate Reaction in Concrete,” ASTM International, West Conshohocken, PA, 2020, 11 pp.

37. Hooton, R. D.; Thomas, M. D. A.; and Ramlochan, T., “Use of Pore Solution Analysis in Design for Concrete Durability,” Advances in Cement Research, V. 22, No. 4, 2010, pp. 203-210. doi: 10.1680/adcr.2010.22.4.203

38. PCA, Design and Control of Concrete Mixtures, Portland Cement Association, Skokie, IL, 2003.

39. Hover, K., “Taking the Mystery Out of Mix Design, Part 2,” Concrete Construction, Jan. 2020, www.concreteconstruction.net/how-to/materials/taking-the-mystery-out-of-mix-design-part-2_o. (last accessed Feb. 17, 2022)

40. De la Varga, I.; Spragg, R. P.; Di Bella, C.; Castro, J.; Bentz, D. P.; and Weiss, J., “Fluid Transport in High Volume Fly Ash Mixtures with and without Internal Curing,” Cement and Concrete Composites, V. 45, Jan. 2014, pp. 102-110. doi: 10.1016/j.cemconcomp.2013.09.017

41. Mehta, P. K., and Gjørv, O. E., “Properties of Portland Cement Concrete Containing Fly Ash and Condensed Silica-Fume,” Cement and Concrete Research, V. 12, No. 5, 1982, pp. 587-595. doi: 10.1016/0008-8846(82)90019-9

42. Neithalath, N.; Persun, J.; and Manchiryal, R. K., “Electrical Conductivity Based Microstructure and Strength Prediction of Plain and Modified Concretes,” International Journal of Advances in Engineering Sciences and Applied Mathematics, V. 2, No. 3, 2010, pp. 83-94. doi: 10.1007/s12572-011-0023-1

43. Thomas, M., “Optimizing the Use of Fly Ash in Concrete,” Portland Cement Association, Skokie, IL, 2007, 24 pp.

44. ASTM C29/C29M-17, “Standard Test Method for Bulk Density (‘Unit Weight’) and Voids in Aggregate,” ASTM International, West Conshohocken, PA, 2017, 5 pp.

45. ASTM C127-15, “Standard Test Method for Relative Density (Specific Gravity) and Absorption of Coarse Aggregate,” ASTM International, West Conshohocken, PA, 2015, 5 pp.

46. ASTM C136/C136M-19, “Standard Test Method for Sieve Analysis of Fine and Coarse Aggregates,” ASTM International, West Conshohocken, PA, 2019, 5 pp.

47. ASTM C566-19, “Standard Test Method for Total Evaporable Moisture Content of Aggregate by Drying,” ASTM International, West Conshohocken, PA, 2019, 3 pp.

48. Mindess, S.; Young, J. F.; and Darwin, D., Concrete, second edition, Prentice Hall, New York, 2003, 644 pp.

49. Bentz, D. P., and Snyder, K. A., “Protected Paste Volume in Concrete Extension to Internal Curing Using Saturated Lightweight Fine Aggregate,” Cement and Concrete Research, V. 29, No. 11, 1999, pp. 1863-1867. doi: 10.1016/S0008-8846(99)00178-7

50. Barrett, T. J., “Improving Service Life of Concrete Structures through the Use of Internal Curing: Impact on Practice,” PhD thesis, Purdue University, West Lafayette, IN, 2015.

51. Shilstone, J. M., “Concrete Mixture Optimization,” Concrete International, V. 12, No. 6, June 1990, pp. 33-39.

52. Ley, T., and Cook, D., “Aggregate Gradations for Concrete Pavement Mixtures,” CP Road Map, Federal Highway Administration, Washington, DC, 2014, https://intrans.iastate.edu/app/uploads/2018/08/MAPbriefOctober2014.pdf. (last accessed Feb. 17, 2022)

53. Trejo, D., and Hendrix, G., “Influence of Aggregate and Proportions on Flowing Concrete Characteristics,” ACI Materials Journal, V. 115, No. 2, Mar. 2018, pp. 171-180. doi: 10.14359/51701930

54. Isgor, O. B.; Ideker, J. H.; Trejo, D.; Weiss, W. J.; Bhardwaj, K. R.; Choudhary, A.; Chopperla, K. S. T.; Glosser, D.; and Vasudevan, G., “Preliminary Experimental and Numerical Studies for a New Mixture Proportioning Approach for Concrete Incorporating Off-Spec Fly Ash (Technical Report),” Energy Power Research Institute, Palo Alto, CA, 2019, 134 pp.

55. Isgor, O. B.; Ideker, J.; Trejo, D.; Weiss, J.; Bharadwaj, K.; Choudhary, A.; Chopperla, K. S. T.; Glosser, D.; and Vasudevan, G., “Performance-

Based Mixture Proportioning Procedure for Concrete Incorporating Off-Spec Fly Ash (Technical Report),” Energy Power Research Institute, Palo Alto, CA, 2020, 78 pp.

56. Mehta, P. K., “Studies on Blended Portland Cements Containing Santorin Earth,” Cement and Concrete Research, V. 11, No. 4, 1981, pp. 507-518. doi: 10.1016/0008-8846(81)90080-6

57. Mehta, P. K., and Monteiro, P. J. M., Concrete: Microstructure, Properties, and Materials, fourth edition, McGraw-Hill Education, New York, 2006, 684 pp.

58. AASHTO TP 119-20, “Standard Method of Test for Electrical Resistivity of a Concrete Cylinder Tested in a Uniaxial Resistance Test,” American Association of State Highway and Transportation Officials, Washington, DC, 2020, 12 pp.

59. ASTM C39/C39M-20, “Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2020, 8 pp.

60. AASHTO TP 135-20, “Standard Method of Test for Determining the Total Pore Volume in Hardened Concrete Using Vacuum Saturation,” American Association of State Highway and Transportation Officials, Washington, DC, 2020, 7 pp.

61. Kim, T., and Olek, J., “Effects of Sample Preparation and Interpretation of Thermogravimetric Curves on Calcium Hydroxide in Hydrated Pastes and Mortars,” Transportation Research Record: Journal of the Transportation Research Board, V. 2290, No. 1, 2012, pp. 10-18. doi: 10.3141/2290-02

62. Tsui-Chang, M.; Suraneni, P.; Montanari, L.; Muñoz, J. F.; and Weiss, W. J., “Determination of Chemical Composition and Electrical Resistivity of Expressed Cementitious Pore Solutions Using X-Ray Fluorescence,” ACI Materials Journal, V. 116, No. 1, Jan. 2019, pp. 155-164. doi: 10.14359/51712242

63. Ding, Z., and Li, Z., “High-Early-Strength Magnesium Phosphate Cement with Fly Ash,” ACI Materials Journal, V. 102, No. 6, Nov.-Dec. 2005, pp. 375-381.

64. Li, Y., and Chen, B., “Factors That Affect the Properties of Magnesium Phosphate Cement,” Construction and Building Materials, V. 47, Oct. 2013, pp. 977-983. doi: 10.1016/j.conbuildmat.2013.05.103

65. Gardner, L. J.; Bernal, S. A.; Walling, S. A.; Corkhill, C. L.; Provis, J. L.; and Hyatt, N. C., “Characterisation of Magnesium Potassium Phosphate Cements Blended with Fly Ash and Ground Granulated Blast Furnace Slag,” Cement and Concrete Research, V. 74, Aug. 2015, pp. 78-87. doi: 10.1016/j.cemconres.2015.01.015

66. Ding, Z.; Dong, B.; Xing, F.; Han, N.; and Li, Z., “Cementing Mechanism of Potassium Phosphate Based Magnesium Phosphate Cement,” Ceramics International, V. 38, No. 8, 2012, pp. 6281-6288. doi: 10.1016/j.ceramint.2012.04.083


ALSO AVAILABLE IN:

Electronic Materials Journal