Title: Effect of Waste Tire Rubber Particles on Concrete Abrasion Resistance Under High-Speed Water Flow

Author(s): Ling-Yun Feng, Ai-Jiu Chen and Han-Dong Liu

Publication: IJCSM

Volume: 15

Issue:

Appears on pages(s):

Keywords: Rubberized concrete, Rubber particles, Abrasion resistance, High-velocity flow, Compressive strength

DOI: 10.1186/s40069-021-00475-8

Date: 9/30/2021

Abstract:
Rubberized concrete is an environmentally friendly building material that mixes rubber particles from old automobile tires into normal concrete in place of fine aggregate. The addition of rubber particles can improve the abrasion resistance of normal concrete observably. It has a good application prospect in hydraulic engineering, especially in the concrete building parts with high abrasion resistance. However, there are few experimental studies on the abrasion resistance of rubberized concrete, and the influence law and mechanism of rubber particles on the abrasion resistance of concrete are not understood. In this paper, the abrasion resistance of rubberized concrete is studied using the underwater-steel-ball method. The results show that rubber particles increase the slump of concrete mixtures. The abrasion resistance of rubberized concrete increases significantly with increasing rubber particle content, whereas the compressive strength decreases linearly. For the same rubber particle size and content, the abrasion resistance of rubberized concrete positively correlates with compressive strength and larger rubber particles significantly improve the abrasion resistance. Rubber particle content is the factor that most strongly affects abrasion resistance of rubberized concrete, followed by the compressive strength. Rubber particle pretreatment methods of NaOH + KH570 can significantly improve the abrasion resistance of rubberized concrete.