Simulation of Permeation of Saturated Cement Paste Based on a New Meso-scale Pore Network Model

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Simulation of Permeation of Saturated Cement Paste Based on a New Meso-scale Pore Network Model

Author(s): Yong Zhou, Yuxuan Yang, Bigya Gyawali and Weiping Zhang

Publication: IJCSM

Volume: 15

Issue:

Appears on pages(s):

Keywords: cementitious materials, hydration process, weighted Voronoi diagram, pore network model

DOI: 10.1186/s40069-021-00468-7

Date: 9/30/2021

Abstract:
This paper presents the simulation of the permeation of saturated cement paste based on a novel pore network model. First, a 2D hydration model of cement particles was developed by extending the work of Zheng et al. 2005 to provide the background for the network construction. Secondly, the establishment of the pore network model and simulation of permeation of saturated cement paste were carried out. The irregular pores between any two hydrated cement particles were linearized with clear distances as the diameters of pores. The straight tubular pores were interconnected with one another to form the network model. During this process, the weighted Voronoi diagram was employed to operate on the graphical expression of the hydrated cement particles. Water permeation in saturated cement paste was simulated to verify the pore network model. Finally, the factors including water–cement ratio, reaction temperature, reaction time and cement particle size that would influence water permeation were numerically investigated.