ACI 350.3-20: Code Requirements for Seismic Analysis and Design of Liquid-Containing Concrete Structures (ACI 350.3-20) and Commentary

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: ACI 350.3-20: Code Requirements for Seismic Analysis and Design of Liquid-Containing Concrete Structures (ACI 350.3-20) and Commentary

Author(s):

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 52

Keywords:

DOI:

Date: 10/1/2021

Abstract:
This Code prescribes procedures for the seismic analysis and design of liquid-containing concrete structures. These procedures address the loading side of seismic design and are intended to complement Section 1.1.9 and Chapter 13 of ACI 350-20. Keywords: circular tanks; concrete tanks; convective component; earthquake resistance; environmental concrete structures; impulsive component; liquid-containing structures; rectangular tanks; seismic resistance; sloshing; storage tanks.