Optimization of Ultra-High-Performance Concrete Using Soft and Hard Inert Fillers (Limestone and Quartz)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Optimization of Ultra-High-Performance Concrete Using Soft and Hard Inert Fillers (Limestone and Quartz)

Author(s): Guillermo Hernández-Carrillo, Alejandro Durán-Herrera, and Arezki Tagnit-Hamou

Publication: Materials Journal

Volume: 119

Issue: 1

Appears on pages(s): 275-288

Keywords: durability; filler effect; microstructure; sustainability; ultra-highperformance concrete

DOI: 10.14359/51734222

Date: 1/1/2022

Abstract:
Ultra-high-performance concrete is a milestone of both durability and mechanical performance; nevertheless, its high consumption of clinker generates a large carbon footprint, and a large quantity of this clinker remains anhydrous due to the very low water availability in the compound. Studies of back-scattered electrons, X-ray diffraction, and quantitative energy-dispersive spectroscopy were done to propose that the cement replacement by inert fillers having a hardness between the limestone and quartz powder is possible due to a higher dissolution of both cement and silica fume that allows the formation of lower Ca/Si ratio C-S-H if enough silica fume is present to keep porosity next to the aggregate constant. Finally, the replaced mixtures had a 37% lower carbon footprint than the reference. The results showed no difference between quartz and limestone systems—both with an adequate silica fume dosage, where able—to keep both compressive strength and bulk resistivity performance at a 37.5% cement replacement.

Related References:

1. Richard, P., and Cheyrezy, M., “Composition of Reactive Powder Concretes,” Cement and Concrete Research, V. 25, No. 7, 1995, pp. 1501-1511. doi: 10.1016/0008-8846(95)00144-2

2. Jensen, O. M., and Hansen, P. F., “Water-Entrained Cement-Based Materials: I. Principles and Theoretical Background,” Cement and Concrete Research, V. 31, No. 4, 2000, pp. 647-654. doi: 10.1016/S0008-8846(01)00463-X

3. Yunsheng, Z.; Wei, S.; Sifeng, L.; Chujie, J.; and Jianzhong, L., “Preparation of C200 Green Reactive Powder Concrete and Its Static-Dynamic Behaviors,” Cement and Concrete Composites, V. 30, No. 9, 2008, pp. 831-838. doi: 10.1016/j.cemconcomp.2008.06.008

4. Yang, S. L.; Millard, S. G.; Soutsos, M. N.; Barnett, S. J.; and Le, T. T., “Influence of Aggregate and Curing Regime on the Mechanical Properties of Ultra-High Performance Fibre Reinforced Concrete (UHPFRC),” Construction and Building Materials, V. 23, No. 6, 2009, pp. 2291-2298. doi: 10.1016/j.conbuildmat.2008.11.012

5. Yazıcı, H.; Yardımcı, M. Y.; Aydın, S.; and Karabulut, A. Ş., “Mechanical Properties of Reactive Powder Concrete Containing Mineral Admixtures under Different Curing Regimes,” Construction and Building Materials, V. 23, No. 3, 2009, pp. 1223-1231. doi: 10.1016/j.conbuildmat.2008.08.003

6. Soliman, N. A., and Tagnit-Hamou, A., “Development of Ultra-High-Performance Concrete Using Glass Powder—Towards Ecofriendly Concrete,” Construction and Building Materials, V. 125, Oct. 2016, pp. 600-612. doi: 10.1016/j.conbuildmat.2016.08.073

7. Hernández Carrillo, G.; Durán Herrera, A.; and Valdez Tamez, P. L., “Ultra High Performance Concrete (UHPC) with Low Silica Fume Contents and Limestone Aggregates,” Proceedings, RILEM International Conference on Materials, Systems and Structures in Civil Engineering Conference Segment on Concrete with Supplementary Cementitious Materials, Lyngby, Denmark, 2016, pp. 349-358.

8. Rossen, J. E.; Lothenbach, B.; and Scrivener, K. L., “Composition of C–S–H in Pastes with Increasing Levels of Silica Fume Addition,” Cement and Concrete Research, V. 75, Sept. 2015, pp. 14-22. doi: 10.1016/j.cemconres.2015.04.016

9. Sarkar, S. L., and Aïtcin, P.-C., “Dissolution Rate of Silica Fume in Very High Strength Concrete,” Cement and Concrete Research, V. 17, No. 4, 1987, pp. 591-601. doi: 10.1016/0008-8846(87)90132-3

10. Scrivener, K. L.; John, V. M.; and Gartner, E. M., “Eco-Efficient Cements: Potential Economically Viable Solutions for a Low-CO2 Cement-Based Materials Industry,” Cement and Concrete Research, V. 114, Dec. 2018, pp. 2-26. doi: 10.1016/j.cemconres.2018.03.015

11. Zajac, M.; Rossberg, A.; Le Saout, G.; and Lothenbach, B., “Influence of Limestone and Anhydrite on the Hydration of Portland Cements,” Cement and Concrete Composites, V. 46, Feb. 2014, pp. 99-108. doi: 10.1016/j.cemconcomp.2013.11.007

12. Menéndez, G.; Bonavetti, V.; and Irassar, E. F., “Strength Development of Ternary Blended Cement with Limestone Filler and Blast-Furnace Slag,” Cement and Concrete Composites, V. 25, No. 1, 2003, pp. 61-67. doi: 10.1016/S0958-9465(01)00056-7

13. Skaropoulou, A.; Kakali, G.; and Tsivilis, S., “Thaumasite Form of Sulfate Attack in Limestone Cement Concrete: The Effect of Cement Composition, Sand Type and Exposure Temperature,” Construction and Building Materials, V. 36, Nov. 2012, pp. 527-533. doi: 10.1016/j.conbuildmat.2012.06.048

14. Tsivilis, S.; Sotiriadis, K.; and Skaropoulou, A., “Thaumasite Form of Sulfate Attack (TSA) in Limestone Cement Pastes,” Journal of the European Ceramic Society, V. 27, No. 2-3, 2007, pp. 1711-1714. doi: 10.1016/j.jeurceramsoc.2006.05.048

15. Skaropoulou, A.; Sotiriadis, K.; Kakali, G.; and Tsivilis, S., “Use of Mineral Admixtures to Improve the Resistance of Limestone Cement Concrete against Thaumasite Form of Sulfate Attack,” Cement and Concrete Composites, V. 37, No. 1, 2013, pp. 267-275. doi: 10.1016/j.cemconcomp.2013.01.007

16. Wang, Y.; He, X.; Su, Y.; Huang, J.; and Ma, B., “Effect of Silica Fume on the Thaumasite Form of Sulfate Attack on Cement-Based Materials,” Journal of Wuhan University of Technology, Materials Science Edition, V. 32, No. 5, 2017, pp. 1108-1114. doi: 10.1007/s11595-017-1718-3

17. Broz, M. E.; Cook, R. F.; and Whitney, D. L., “Microhardness, Toughness, and Modulus of Mohs Scale Minerals,” The American Mineralogist, V. 91, No. 1, 2006, pp. 135-142. doi: 10.2138/am.2006.1844

18. Sorelli, L.; Constantinides, G.; Ulm, F. J.; and Toutlemonde, F., “The Nano-Mechanical Signature of Ultra High Performance Concrete by Statistical Nanoindentation Techniques,” Cement and Concrete Research, V. 38, No. 12, 2008, pp. 1447-1456. doi: 10.1016/j.cemconres.2008.09.002

19. Wilson, W.; Sorelli, L.; and Tagnit-Hamou, A., “Unveiling Micro-Chemo-Mechanical Properties of C–(A)–S–H and Other Phases in Blended-Cement Pastes,” Cement and Concrete Research, V. 107, May 2018, pp. 317-336. doi: 10.1016/j.cemconres.2018.02.010

20. Oliver, W. C., and Pharr, G. M., “An Improved Technique for Determining Hardness and Elastic Modulus Using Load and Displacement Sensing Indentation Experiments,” Journal of Materials Research, V. 7, No. 6, 1992, pp. 1564-1583. doi: 10.1557/JMR.1992.1564

21. Bentz, D. P., and Aitcin, P. C., “The Hidden Meaning of Water-Cement Ratio,” Concrete International, V. 30, No. 5, May 2008, pp. 51-54.

22. Feldman, R. F., and Beaudoin, J. J., “Microstructure and Strength of Hydrated Cement,” Cement and Concrete Research, V. 6, No. 3, 1976, pp. 389-400. doi: 10.1016/0008-8846(76)90102-2

23. Kunther, W.; Ferreiro, S.; and Skibsted, J., “Influence of the Ca/Si Ratio on the Compressive Strength of Cementitious Calcium-Silicate-Hydrate Binders,” Journal of Materials Chemistry. A, Materials for Energy and Sustainability, V. 5, No. 33, 2017, pp. 17401-17412. doi: 10.1039/C7TA06104H

24. Jensen, O. M., and Hansen, P. F., “Water-Entrained Cement-Based Materials: I. Principles and Theoretical Background,” Cement and Concrete Research, V. 31, No. 4, 2000, pp. 1-13.

25. Wille, K.; Naman, A. E.; and Parra-Montesinos, G. J., “Ultra-High Performance Concrete with Compressive Strength Exceeding 150 MPa (22 ksi): A Simpler Way,” ACI Materials Journal, V. 108, No. 1, Jan.-Feb. 2011, pp. 46-53. doi: 10.14359/51664215

26. Tue, N. V.; Ma, J.; Orgass, M.; and Fehling, E., “Influence of Addition Method of Superplasticizer on the Properties of Fresh UHPC,” Ultra High Performance Concrete (UHPC), E. Fehling, M. Schmidt, and S. Stuwald, eds., Kassel University Press, Germany, 2008, pp. 93-103.

27. Snellings, R.; Bazzoni, A.; and Scrivener, K., “The Existence of Amorphous Phase in Portland Cements: Physical Factors Affecting Rietveld Quantitative Phase Analysis,” Cement and Concrete Research, V. 59, May 2014, pp. 139-146. doi: 10.1016/j.cemconres.2014.03.002

28. Scrivener, K.; Snellings, R.; and Lothenbach, B., A Practical Guide to Microstructural Analysis of Cementitious Materials, CRC Press, London, UK, 2016.

29. Scrivener, K. L.; Bentur, A.; and Pratt, P. L., “Quantitative Characterization of the Transition Zone in High Strength Concretes,” Advances in Cement Research, V. 1, No. 4, 1988, pp. 230-237. doi: 10.1680/adcr.1988.1.4.230

30. Deschner, F.; Münch, B.; Winnefeld, F.; and Lothenbach, B., “Quantification of Fly Ash in Hydrated, Blended Portland Cement Pastes by Backscattered Electron Imaging,” Journal of Microscopy, V. 251, No. 2, 2013, pp. 188-204. doi: 10.1111/jmi.12061

31. Alexander, M. G., “Engineering and Transport Properties of the Interfacial Transition Zone in Cementitious Composites,” RILEM Publications, Paris, France 1999.

32. Scrivener, K. L., “Backscattered Electron Imaging of Cementitious Microstructures: Understanding and Quantification,” Cement and Concrete Composites, V. 26, No. 8, 2004, pp. 935-945. doi: 10.1016/j.cemconcomp.2004.02.029

33. Wilson, W.; Sorelli, L.; and Tagnit-Hamou, A., “Automated Coupling of NanoIndentation and Quantitative Energy-Dispersive Spectroscopy (NI-QEDS): A Comprehensive Method to Disclose the Micro-Chemo-Mechanical Properties of Cement Pastes,” Cement and Concrete Research, V. 103, Jan. 2018, pp. 49-65. doi: 10.1016/j.cemconres.2017.08.016

34. Wilson, W.; Sorelli, L.; and Tagnit-Hamou, A., “Chemo-Mechanical Properties of Cement Matrices with Fly Ash and Slag,” 10th ACI/RILEM International Conference on Cementitious Materials and Alternative Binders for Sustainable Concrete, SP-320, American Concrete Institute, Farmington Hills, MI, Aug. 2017, pp. 29.1-29.14.

35. Ritchie, N. W. M., “Standards-Based Quantification in DTSA-II—Part II,” Microscopy Today, V. 20, No. 1, 2012, pp. 24-28. doi: 10.1017/S1551929511001398

36. Breton, D., “Low-Heat High-Performance,” United States Patent 5531823, 1995.

37. Vogt, C., “Ultrafine Particles in Concrete—Influence of Ultrafine Particles on Concrete Properties and Application to Concrete Mix Design,” doctoral thesis, School of Architecture and the Built Environment Division of Concrete Structures, Stockholm, Sweden, 2010, 177 pp.

38. Huang, W.; Kazemi-Kamyab, H.; Sun, W.; and Scrivener, K., “Effect of Cement Substitution by Limestone on the Hydration and Microstructural Development of Ultra-High Performance Concrete (UHPC),” Cement and Concrete Composites, V. 77, Mar. 2017, pp. 86-101. doi: 10.1016/j.cemconcomp.2016.12.009

39. Morris, W.; Moreno, E. I.; and Sagüés, A. A., “Practical Evaluation of Resistivity of Concrete in Test Cylinders Using a Wenner Array Probe,” Cement and Concrete Research, V. 26, No. 12, 1996, pp. 1779-1787. doi: 10.1016/S0008-8846(96)00175-5

40. Moosberg-Bustnes, H.; Lagerblad, B.; and Forssberg, E., “The Function of Fillers in Concrete,” Materials and Structures, V. 37, Mar. 2004, pp. 74-81. doi: 10.1007/BF02486602

41. Aitcin, P.-C., Binders for Durable and Sustainable Concrete, CRC Press, London, UK, 2018.

42. Taylor, H. F. W., Cement Chemistry, Thomas Telford, London, UK, 1990.

43. Müller, H. S.; Haist, M.; and Vogel, M., “Assessment of the Sustainability Potential of Concrete and Concrete Structures Considering Their Environmental Impact, Performance and Lifetime,” Construction and Building Materials, V. 67, Part C, 2014, pp. 321-337. doi: 10.1016/j.conbuildmat.2014.01.039

44. Khatib, J. M., Sustainability of Construction Materials, second edition, Elsevier, Amsterdam, the Netherlands, 2016.


ALSO AVAILABLE IN:

Electronic Materials Journal