Pseudo-Ductile Cementitious Composites by Hierarchical Crack Bridging

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Pseudo-Ductile Cementitious Composites by Hierarchical Crack Bridging

Author(s): B. S. Sindu and Saptarshi Sasmal

Publication: Materials Journal

Volume: 119

Issue: 1

Appears on pages(s): 145-158

Keywords: continuous fibers; high strength; hybrid fibers; inverse analysis; length scales; numerical modeling; strain-hardened

DOI: 10.14359/51734193

Date: 1/1/2022

Abstract:
An attempt has been made to develop hierarchically crack-abridged, strain-hardened cementitious composite by judiciously incorporating hybrid fibers of three distinctly different length scales (nano-, micro-, and continuous fibers). Unlike textile-reinforced cement composites, here, the nano- to macrofibers are used to improve the cementitious matrix properties through appropriate crack bridging, and at the macroscale, only onedimensional (1-D) long fibers/yarns are used. A distinct and categorical improvement in the property(ies) is found to take place at each scale of bridging. The structural composite systems made using the developed composite exhibited very promising properties, such as high strength (flexural) of approximately 20 MPa (2.90 ksi), an ultimate strain of 8000 με, and rotational capacity of approximately 10 degrees. A detailed numerical model is developed to carry out nonlinear finite element analysis where the interface properties, strain state, and so on are the parameters. Finally, a constitutive model is proposed for the developed composite through inverse analysis. The proposed constitutive model will help engineers design structural components/retrofit schemes by employing the developed composite without complex analysis (using smeared properties).

Related References:

1. Lawler, J. S.; Zampini, D.; and Shah, S. P., “Microfiber and Macrofiber Hybrid Fiber-Reinforced Concrete,” Journal of Materials in Civil Engineering, ASCE, V. 17, No. 5, Oct. 2005, pp. 595-604. doi: 10.1061/(ASCE)0899-1561(2005)17:5(595)

2. Bandelt, M. J., and Billington, S. L., “Bond Behavior of Steel Reinforcement in High-Performance Fiber-Reinforced Cementitious Composite Flexural Members,” Materials and Structures, V. 49, No. 1-2, Jan. 2016, pp. 71-86. doi: 10.1617/s11527-014-0475-4

3. Fantilli, A. P.; Mihashi, H.; and Vallini, P., “Multiple Cracking and Strain Hardening in Fiber-Reinforced Concrete under Uniaxial Tension,” Cement and Concrete Research, V. 39, No. 12, Dec. 2009, pp. 1217-1229. doi: 10.1016/j.cemconres.2009.08.020

4. Trottier, J.-F., and Banthia, N., “Toughness Characterization of Steel-Fiber Reinforced Concrete,” Journal of Materials in Civil Engineering, ASCE, V. 6, No. 2, May 1994, pp. 264-289. doi: 10.1061/(ASCE)0899-1561(1994)6:2(264)

5. Yoo, D.-Y.; Shin, H.-O.; Yang, J.-M.; and Yoon, Y.-S., “Material and Bond Properties of Ultra High Performance Fiber Reinforced Concrete with Micro Steel Fibers,” Composites Part B: Engineering, V. 58, Mar. 2014, pp. 122-133. doi: 10.1016/j.compositesb.2013.10.081

6. Park, S.-J.; Seo, M.-K.; Shim, H.-B.; and Rhee, K.-Y., “Effect of Different Cross-Section Types on Mechanical Properties of Carbon Fibers-Reinforced Cement Composites,” Materials Science and Engineering: A, V. 366, No. 2, Feb. 2004, pp. 348-355. doi: 10.1016/j.msea.2003.08.123

7. Shu, X.; Graham, R. K.; Huang, B.; and Burdette, E. G., “Hybrid Effects of Carbon Fibers on Mechanical Properties of Portland Cement Mortar,” Materials & Design, V. 65, Jan. 2015, pp. 1222-1228. doi: 10.1016/j.matdes.2014.10.015

8. Stynoski, P.; Mondal, P.; and Marsh, C., “Effects of Silica Additives on Fracture Properties of Carbon Nanotube and Carbon Fiber Reinforced Portland Cement Mortar,” Cement and Concrete Composites, V. 55, Jan. 2015, pp. 232-240. doi: 10.1016/j.cemconcomp.2014.08.005

9. Hossain, M. Z., and Abdul Awal, A. S. M., “Flexural Response of Hybrid Carbon Fiber Thin Cement Composites,” Construction and Building Materials, V. 25, No. 2, Feb. 2011, pp. 670-677. doi: 10.1016/j.conbuildmat.2010.07.022

10. Atahan, H. N.; Pekmezci, B. Y.; and Tuncel, E. Y., “Behavior of PVA Fiber-Reinforced Cementitious Composites under Static and Impact Flexural Effects,” Journal of Materials in Civil Engineering, ASCE, V. 25, No. 10, Oct. 2013, pp. 1438-1445. doi: 10.1061/(ASCE)MT.1943-5533.0000691

11. Fischer, G., and Li, V. C., “Deformation Behavior of Fiber-Reinforced Polymer Reinforced Engineered Cementitious Composite (ECC) Flexural Members under Reversed Cyclic Loading Conditions,” ACI Structural Journal, V. 100, No. 1, Jan.-Feb. 2003, pp. 25-35. doi: 10.14359/12436

12. Said, S. H., and Razak, H. A., “The Effect of Synthetic Polyethylene Fiber on the Strain Hardening Behavior of Engineered Cementitious Composite (ECC),” Materials & Design, V. 86, Dec. 2015, pp. 447-457. doi: 10.1016/j.matdes.2015.07.125

13. Sasmal, S., and Avinash, G., “Investigations on Mechanical Performance of Cementitious Composites Micro-Engineered with Poly Vinyl Alcohol Fibers,” Construction and Building Materials, V. 128, Dec. 2016, pp. 136-147. doi: 10.1016/j.conbuildmat.2016.10.025

14. Naaman, A. E., and Reinhardt, H. W., “Proposed Classification of HPFRC Composites Based on Their Tensile Response,” Materials and Structures, V. 39, No. 5, June 2006, pp. 547-555. doi: 10.1617/s11527-006-9103-2

15. Zhang, C., and Cao, M., “Fiber Synergy in Multi-Scale Fiber-Reinforced Cementitious Composites,” Journal of Reinforced Plastics and Composites, V. 33, No. 9, May 2014, pp. 862-874. doi: 10.1177/0731684413514785

16. Sindu, B. S., and Sasmal, S., “Multi-Scale Abridged Cement Composite with Enhanced Mechanical Properties,” ACI Materials Journal, V. 117, No. 4, July 2020, pp. 105-117. doi: 10.14359/51724625

17. Alrekabi, S.; Cundy, A. B.; Lampropoulos, A.; Whitby, R. L. D.; and Savina, I., “Mechanical Performance of Novel Cement-Based Composites Prepared with Nano-Fibres, and Hybrid Nano- and Micro-Fibres,” Composite Structures, V. 178, Oct. 2017, pp. 145-156. doi: 10.1016/j.compstruct.2017.06.045

18. Alshaghel, A.; Parveen, S.; Rana, S.; and Fangueiro, R., “Effect of Multiscale Reinforcement on the Mechanical Properties and Microstructure of Microcrystalline Cellulose-Carbon Nanotube Reinforced Cementitious Composites,” Composites Part B: Engineering, V. 149, Sept. 2018, pp. 122-134. doi: 10.1016/j.compositesb.2018.05.024

19. Barhum, R., and Mechtcherine, V., “Effect of Short, Dispersed Glass and Carbon Fibres on the Behaviour of Textile-Reinforced Concrete under Tensile Loading,” Engineering Fracture Mechanics, V. 92, Sept. 2012, pp. 56-71. doi: 10.1016/j.engfracmech.2012.06.001

20. Haim, E., and Peled, A., “Impact Behavior of Textile and Hybrid Cement-Based Composites,” ACI Materials Journal, V. 108, No. 3, May-June 2011, pp. 235-243. doi: 10.14359/51682485

21. Li, B.; Xiong, H.; Jiang, J.; and Dou, X., “Tensile Behavior of Basalt Textile Grid Reinforced Engineering Cementitious Composite,” Composites Part B: Engineering, V. 156, Jan. 2019, pp. 185-200. doi: 10.1016/j.compositesb.2018.08.059

22. Bournas, D. A.; Lontou, P. V.; Papanicolaou, C. G.; and Triantafillou, T. C., “Textile-Reinforced Mortar versus Fiber-Reinforced Polymer Confinement in Reinforced Concrete Columns,” ACI Structural Journal, V. 104, No. 6, Nov. 2007, pp. 740-748. doi: 10.14359/18956

23. Brückner, A.; Ortlepp, R.; and Curbach, M., “Textile Reinforced Concrete for Strengthening in Bending and Shear,” Materials and Structures, V. 39, No. 8, Oct. 2006, pp. 741-748. doi: 10.1617/s11527-005-9027-2

24. Si Larbi, A.; Contamine, R.; and Hamelin, P., “TRC and Hybrid Solutions for Repairing and/or Strengthening Reinforced Concrete Beams,” Engineering Structures, V. 45, Dec. 2012, pp. 12-20. doi: 10.1016/j.engstruct.2012.06.002

25. Triantafillou, T. C., and Papanicolaou, C. G., “Shear Strengthening of Reinforced Concrete Members with Textile Reinforced Mortar (TRM) Jackets,” Materials and Structures, V. 39, No. 1, Jan. 2006, pp. 93-103. doi: 10.1007/s11527-005-9034-3

26. Kang, S.-T.; Choi, J.-I.; Koh, K.-T.; Lee, K. S.; and Lee, B. Y., “Hybrid Effects of Steel Fiber and Microfiber on the Tensile Behavior of Ultra-High Performance Concrete,” Composite Structures, V. 145, June 2016, pp. 37-42. doi: 10.1016/j.compstruct.2016.02.075

27. Ganesan, N.; Indira, P. V.; and Sabeena, M. V., “Tension Stiffening and Cracking of Hybrid Fiber-Reinforced Concrete,” ACI Materials Journal, V. 110, No. 6, Nov.-Dec. 2013, pp. 715-722. doi: 10.14359/51686341

28. Li, Q.; Zhao, X.; Xu, S.; and Gao, X., “Influence of Steel Fiber on Dynamic Compressive Behavior of Hybrid Fiber Ultra High Toughness Cementitious Composites at Different Strain Rates,” Construction and Building Materials, V. 125, Oct. 2016, pp. 490-500. doi: 10.1016/j.conbuildmat.2016.08.066

29. Zhang, J.; Wang, Q.; and Wang, Z., “Properties of Polyvinyl Alcohol-Steel Hybrid Fiber-Reinforced Composite with High-Strength Cement Matrix,” Journal of Materials in Civil Engineering, ASCE, V. 29, No. 7, July 2017, p. 04017026. doi: 10.1061/(ASCE)MT.1943-5533.0001868

30. Ngo, T. T., and Kim, D. J., “Synergy in Shear Response of Ultra-High-Performance Hybrid-Fiber-Reinforced Concrete at High Strain Rates,” Composite Structures, V. 195, July 2018, pp. 276-287. doi: 10.1016/j.compstruct.2018.04.075

31. Kwon, S.; Nishiwaki, T.; Kikuta, T.; and Mihashi, H., “Development of Ultra-High-Performance Hybrid Fiber-Reinforced Cement-Based Composites,” ACI Materials Journal, V. 111, No. 3, May-June 2014, pp. 309-318. doi: 10.14359/51686890

32. Meng, W., and Khayat, K. H., “Effect of Hybrid Fibers on Fresh Properties, Mechanical Properties, and Autogenous Shrinkage of Cost-Effective UHPC,” Journal of Materials in Civil Engineering, ASCE, V. 30, No. 4, Apr. 2018, p. 04018030. doi: 10.1061/(ASCE)MT.1943-5533.0002212

33. Tóth, M.; Juhász, K. P.; and Pluzsik, A., “Effect of Mixed Fibers on the Ductility of Concrete,” Journal of Materials in Civil Engineering, ASCE, V. 29, No. 9, Sept. 2017, p. 04017082. doi: 10.1061/(ASCE)MT.1943-5533.0001927

34. Rossi, P., and Parant, E., “Damage Mechanisms Analysis of a Multi-Scale Fibre Reinforced Cement-Based Composite Subjected to Impact and Fatigue Loading Conditions,” Cement and Concrete Research, V. 38, No. 3, Mar. 2008, pp. 413-421. doi: 10.1016/j.cemconres.2007.09.002

35. Chorzepa, M. G.; Masud, M.; Yaghoobi, A.; and Jiang, H., “Impact Test: Multiscale Fiber-Reinforced Concrete Including Polypropylene and Steel Fibers,” ACI Structural Journal, V. 114, No. 6, Nov.-Dec. 2017, pp. 1429-1444. doi: 10.14359/51700832

36. Sindu, B. S., and Sasmal, S., “On the Development and Studies of Nano-And Micro-Fiber Hybridized Strain Hardened Cementitious Composite,” Archives of Civil and Mechanical Engineering, V. 19, No. 2, 2019, pp. 348-359. doi: 10.1016/j.acme.2018.11.008

37. Červenka, V.; Jendele, L.; and Červenka, J., “ATENA Program Documentation—Part 1: Theory,” Červenka Consulting, Prague, Czech Republic, 2006, 330 pp.

38. Menétrey, P., and Willam, K. J., “Triaxial Failure Criterion for Concrete and Its Generalization,” ACI Structural Journal, V. 92, No. 3, May-June 1995, pp. 311-318. doi: 10.14359/1132

39. Bažant, Z. P., and Oh, B. H., “Crack Band Theory for Fracture of Concrete,” Materials and Structures, V. 16, No. 3, May 1983, pp. 155-177. doi: 10.1007/BF02486267

40. van Mier, J. G. M., “Multiaxial Strain-Softening of Concrete—Part II: Load-Histories,” Materials and Structures, V. 19, No. 3, May 1986, pp. 179-190. doi: 10.1007/BF02472034

41. Sasmal, S.; Novák, B.; Rmanjaneyulu, K.; Roehm, C.; Srinivas, V.; Lakshmanan, N.; and Iyer, N. R., “Upgradation of Gravity Load Designed Sub-Assemblages Subjected to Seismic Type Loading,” Composite Structures, V. 93, No. 6, May 2011, pp. 1561-1573. doi: 10.1016/j.compstruct.2011.01.001

42. Sasmal, S., and Nath, D., “Evaluation of Performance of Non-Invasive Upgrade Strategy for Beam–Column Sub-Assemblages of Poorly Designed Structures under Seismic Type Loading,” Earthquake Engineering & Structural Dynamics, V. 45, No. 11, 2016, pp. 1817-1835. doi: 10.1002/eqe.2730

43. Rigaud, S.; Chanvillard, G.; and Chen, J., “Characterization of Bending and Tensile Behavior of Ultra-High Performance Concrete Containing Glass Fibers,” High Performance Fiber Reinforced Cement Composites 6 – HPFRCC 6, G. J. Parra-Montesinos, H. W. Reinhardt, and A. E. Naaman, eds., Springer, Dordrecht, the Netherlands, 2012, pp. 373-380. doi: 10.1007/978-94-007-2436-5_45


ALSO AVAILABLE IN:

Electronic Materials Journal