Reliability Assessment and Strength Reduction Factor Calibration for Screw Anchors Concrete Breakout

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Reliability Assessment and Strength Reduction Factor Calibration for Screw Anchors Concrete Breakout

Author(s): Ahmad N. Tarawneh, Eman F. Saleh, and Sereen A. Majdalaweyh

Publication: Structural Journal

Volume: 119

Issue: 2

Appears on pages(s): 113-122

Keywords: first-order reliability method (FORM); Monte Carlo simulation (MCS); reliability analysis; screw anchors; strength reduction factors

DOI: 10.14359/51734190

Date: 3/1/2022

Abstract:
The screw anchor design model was recently adopted in ACI 318-19, and similar strength reduction factors for post-installed anchors were applied to screw anchors despite its reliable performance, which has been proven in experimental studies. Accordingly, this study presents a comprehensive reliability assessment of the safety level for the design of screw anchors governed by concrete breakout. A worldwide database that includes single anchors embedded in cracked and uncracked concrete, anchors with edge effects, and a group of anchors is used in the reliability analysis. Anchor design inherently has different uncertainties related to multiple variables like concrete strength and variability in load. These variables have been modeled using multiple distributions. Furthermore, in this paper, anchors are grouped into three classes based on the installation effort sensitivity classes 1 to 3, where this sensitivity is described in a beta distribution. Based on a 3.5 selected reliability index threshold, the ACI 318-19 strength reduction factors result in conservative reliability indexes that exceed the selected threshold. Thus, revised strength reduction factors (ϕ) are proposed. For anchors embedded in uncracked concrete, the proposed ϕ factors are 0.80 for anchor classes 1 and 2 and 0.75 for anchor class 3. For anchors embedded in cracked concrete, ϕ factors are 0.75, 0.7, and 0.65 for classes 1, 2, and 3, respectively. The study also presents a sensitivity analysis to quantify the effect of each model error parameter on the results.

Related References:

1. Cook, R. A.; Burtz, J. L.; and Ansley, M. H., “Design Guidelines and Specifications for Engineered Grouts Used in Anchorage and Pile Splice Applications (FDOT Research Report BC354 RPWO #48),” University of Florida, Gainesville, FL, Aug. 2003, 129 pp.

2. Tarawneh, A. N.; Ross, B. E.; and Cousins, T. E., “Tensile Behavior and Design of Screw Anchors in Thin Concrete Members,” ACI Structural Journal, V. 117, No. 1, Jan. 2020, pp. 91-102. doi: 10.14359/51718011

3. Olsen, J.; Pregartner, T.; and Lamanna, A. J., “Basis for Design of Screw Anchors in Concrete,” ACI Structural Journal, V. 109, No. 4, July-Aug. 2012, pp. 559-568.

4. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19),” American Concrete Institute, Farmington Hills, MI, 2019, 624 pp.

5. Farrow, C. B., and Klingner, R. E., “Tensile Capacity of Anchors with Partial or Overlapping Failure Surfaces: Evaluation of Existing Formulas on an LRFD Basis,” ACI Structural Journal, V. 92, No. 6, Nov.-Dec. 1995, pp. 698-708.

6. ASCE/SEI 7-16, “Minimum Design Loads and Associated Criteria for Buildings and Other Structures,” American Society of Civil Engineers, Reston, VA, 2017, 800 pp.

7. Fuchs, W.; Eligehausen, R.; and Breen, J. E., “Concrete Capacity Design (CCD) Approach for Fastening to Concrete,” ACI Structural Journal, V. 92, No. 1, Jan.-Feb. 1995, pp. 73-94.

8. Kuenzlen, J. H., “Load-Bearing Behavior of Screw Anchors under Axial Tension,” doctoral thesis, the University of Stuttgart, Stuttgart, Germany, 2004. (in German)

9. Owen, D. B., “Factors for One-Sided Tolerance Limits and for Variables Sampling Plans (SCR-607),” Sandia Corporation Monograph, Washington, DC, Mar. 1963, 414 pp.

10. Hokkanen, P. F., and Scheiwiller, A. P., “Probabilistic Models for the Resistance of Concrete Anchors,” V. 242, Institute of Structural Engineering, Swiss Federal Institute of Technology Zürich (ETH Zürich), Zürich, Switzerland, May 1999, 58 pp.

11. Melchers, R. E., and Beck, A. T., Structural Reliability Analysis and Prediction, John Wiley & Sons, Inc., Hoboken, NJ, 2018, 528 pp.

12. Nowak, A. S., and Collins, K. R., Reliability of Structures, CRC Press, London, UK, 2012, 407 pp.

13. Bergmeister, K., “Bemessung von Dübelverbindungen im Stahlbetonbau auf der Grundlage von Teilsicherheitsbeiwerten (Bericht Nr. 7/6-90/2),” Institute of Construction Materials, University of Stuttgart, Stuttgart, Germany, 1990.

14. Vrouwenvelder, T., “Special Issue Devoted to the Work of the Joint Committee on Structural Safety,” Structural Safety, V. 19, No. 3, 1997.

15. Wood, S. L., “Evaluation of the Long-Term Properties of Concrete,” ACI Materials Journal, V. 88, No. 6, Nov.-Dec. 1991, pp. 630-643.

16. Comité Euro-International du Béton, Design of Fastenings in Concrete: Design Guide, CEB Bulletin No. 233, Thomas Telford Ltd., London, UK, 1997, 83 pp.

17. Nowak, A. S., and Szerszen, M. M., “Calibration of Design Code for Buildings (ACI 318): Part 1—Statistical Models for Resistance,” ACI Structural Journal, V. 100, No. 3, May-June 2003, pp. 377-382.

18. Hasofer, A. M., and Lind, N. C., “Exact and Invariant Second-Moment Code Format,” Journal of the Engineering Mechanics Division, ASCE, V. 100, No. 1, Feb. 1974, pp. 111-121. doi: 10.1061/JMCEA3.0001848

19. MacGregor, J. G.; Mirza, S. A.; and Ellingwood, B., “Statistical Analysis of Resistance of Reinforced and Prestressed Concrete Members,” ACI Journal Proceedings, V. 80, No. 3, May-June, 1983, pp. 167-176.

20. Farrow, C. B., Frigui, I.; and Klingner, R. E., “Tensile Capacity of Single Anchors in Concrete: Evaluation of Existing Formulas on an LRFD Basis,” ACI Structural Journal, V. 93, No. 1, Jan.-Feb. 1996, pp. 128-137.

21. Szerszen, M. M., and Nowak, A. S., “Calibration of Design Code for Buildings (ACI 318): Part 2—Reliability Analysis and Resistance Factors,” ACI Structural Journal, V. 100, No. 3, May-June 2003, pp. 383-391.


ALSO AVAILABLE IN:

Electronic Structural Journal