Title: PRC-364.2-21: Increasing Shear Capacity within Existing Reinforced Concrete Structures—TechNote
Author(s): ACI Committee 364
Publication: Technical Documents
Volume:
Issue:
Appears on pages(s): 9
Keywords:
DOI:
Date: 8/1/2021
Abstract: Rehabilitation projects often involve the need to increase the load-carrying capacity of members within existing concrete structures that are deficient due to increased load demand associated with change of use, deficiencies in the original design or construction, or deterioration. Such strengthening often includes increasing shear capacity. Keywords: external reinforcement; fabric-reinforced cementitious matrix (FRCM); fiber-reinforced polymer (FRP); internal reinforcement; post-tensioning; section enlargement; shear strengthening.
ACI Collection of Concrete Codes, Specifications, and Practices - Digital Subscription
ACI 562 PLUS Concrete Repair Subscription
The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.
Edit Module Settings to define Page Content Reviewer