Study on Reduction Effect of Vibration Propagation due to Internal Explosion Using Composite Materials

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Study on Reduction Effect of Vibration Propagation due to Internal Explosion Using Composite Materials

Author(s): Sangwoo Park, Jangwoon Beak, Kukjoo Kim and Young-Jun Park

Publication: IJCSM

Volume: 15

Issue:

Appears on pages(s):

Keywords: internal explosion, blast‑proof panel, explosion experiment, safety distance, numerical explosion model

DOI: 10.1186/s40069-021-00467-8

Date: 7/31/2021

Abstract:
With the increasing installation cases of underground explosive facilities (e.g., ammunition magazines, hydrogen tanks, etc.) in urban areas in recent years, the risk of internal explosions is also increasing. However, few studies on the measures for reducing damage by the ground vibration have been conducted except for maintaining safety distance. In this study, a method for attenuating the vibration propagated outward by installing a blast-proof panel was numerically and experimentally investigated. Two cubical reinforced concrete structures were manufactured according to the concrete strength and a blast-proof panel was installed on only one side of the structure. Then, acceleration sensors were installed on the external surface to evaluate the propagation of vibration outward depending on the installation of a blast-proof panel. Before a field experiment, a preliminary numerical simulation was performed. The results showed that the acceleration propagated outward could be effectively reduced by installing a blast-proof panel. Even though the performance of a blast-proof panel on vibration reduction was also investigated in the field experiment, significantly larger absolute accelerations were estimated due to the different experimental conditions. Finally, the vibration reduction effect of the blast-proof panel was numerically evaluated according to its thickness and the internal explosion load. A blast-proof panel more effectively reduced the acceleration propagated outward as its thickness increased and the explosion load decreased.




  