Experimental Study on Spall Resistance of Steel-Fiber Reinforced Concrete Slab Subjected to Explosion

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Experimental Study on Spall Resistance of Steel-Fiber Reinforced Concrete Slab Subjected to Explosion

Author(s): Dapeng Yang, Bei Zhang and Guojun Liu

Publication: IJCSM

Volume: 15

Issue:

Appears on pages(s):

Keywords: steel-fiber reinforced concrete slab, explosion test, steel-fiber parameters, spall damage

DOI: 10.1186/s40069-021-00459-8

Date: 7/31/2021

Abstract:
Steel-fiber reinforced concrete slabs have good blast and spall resistance. In this study, compression and splitting tensile experiments were carried out to obtain the basic quasi-static mechanical properties of the steel-fiber concrete specimens and the influence of steel-fiber parameters was revealed. In-field explosion experiments were performed to study the dynamic responses and damage modes of the steel-fiber reinforced concrete slabs. Five typical spall damage modes were observed, the distribution law of the spalling fragments was obtained, and the influence of steel-fiber shape, length, length–diameter ratio and volume percentage on the spall performance were revealed. These results will provide a basis for the application of steel-fiber reinforced concrete slabs in protective structures.