Title: Effects of Aggregate Content on Rheological Properties of Lubrication Layer and Pumping Concrete

Author(s): Yu Liu, Rui Jing, Fengze Cao, and Peiyu Yan

Publication: Materials Journal

Volume: 118

Issue: 6

Appears on pages(s): 7-18

Keywords: lubrication layer; paste-aggregate ratio; pumpability; rheological properties; sand-to-total aggregate ratio

DOI: 10.14359/51734147

Date: 11/1/2021

Abstract:
The lubrication layer plays a governing role in predicting the pumpability of fresh concrete. The effects of aggregate content on the rheological properties and formation of the lubrication layer were determined from the measurements of the sliding pipe rheometer, tribometer, and mortar rheology. The performance indexes of fresh concrete, including its rheological properties and workability, were investigated in parallel to fully characterize the impact of aggregate content on the pumpability of concrete. The results show that there is an optimal sand-to-total aggregate ratio (sand ratio) that yields the best rheological properties of the lubrication layer and pumpability of concrete. They also improve with the increase in paste-aggregate (PA) ratio. The shearing degree of bulk concrete is affected by the aggregate content, which leads to different formation processes of the lubrication layer. The rheological properties and workability of concrete are improved with a moderate sand ratio and an increased PA ratio due to the change in thickness of the paste layer on the surface of aggregate particles. The thixotropy of concrete is affected by the aggregate content. Moreover, the formation of the lubrication layer and its rheological property evolution depend on the measurement systems.

Related References:

1. Kwon, S. H.; Jang, K. P.; Kim, J. H.; and Shah, S. P., “State of the Art on Prediction of Concrete Pumping,” International Journal of Concrete Structures and Materials, V. 10, No. 3, 2016, pp. S75-S85. doi: 10.1007/s40069-016-0150-y

2. Secrieru, E.; Cotardo, D.; Mechtcherine, V.; Lohaus, L.; Schroefl, C.; and Begemann, C., “Changes in Concrete Properties during Pumping and Formation of Lubricating Material under Pressure,” Cement and Concrete Research, V. 108, 2018, pp. 129-139. doi: 10.1016/j.cemconres.2018.03.018

3. Feys, D.; Khayat, K. H.; and Khatib, R., “How do Concrete Rheology, Tribology, Flow Rate and Pipe Radius Influence Pumping Pressure?” Cement and Concrete Composites, V. 66, 2016, pp. 38-46. doi: 10.1016/j.cemconcomp.2015.11.002

4. Kaplan, D.; de Larrard, F.; and Sedran, T., “Avoidance of Blockages in Concrete Pumping Process,” ACI Materials Journal, V. 102, No. 3, May-June 2005, pp. 183-191.

5. Vosahlik, J.; Riding, K. A.; Feys, D.; Lindquist, W.; Keller, L.; Van Zetten, S.; and Schulz, B., “Concrete Pumping and Its Effect on the Air Void System,” Materials and Structures, V. 51, No. 4, 2018, p. 94. doi: 10.1617/s11527-018-1204-1

6. Kim, J. H.; Han, S. H.; and Choi, B. I., “Influence of Pumping Pressure on the Viscosity Curve and Rheological Stability of Mortar Incorporating Polycarboxylate,” Cement and Concrete Composites, V. 105, 2020, p. 7. doi: 10.1016/j.cemconcomp.2019.103419

7. Rio, O.; Rodriguez, A.; Nabulsi, S.; and Alvarez, M., “Pumping Quality Control Method Based on Online Concrete Pumpability Assessment,” ACI Materials Journal, V. 108, No. 4, July-Aug. 2011, pp. 423-431.

8. Feys, D.; De Schutter, G.; Khayat, K. H.; and Verhoeven, R., “Changes In Rheology Of Self-Consolidating Concrete Induced By Pumping,” Materials and Structures, V. 49, No. 11, 2016, pp. 4657-4677. doi: 10.1617/s11527-016-0815-7

9. Choi, M. S.; Kim, Y. S.; Kim, J. H.; Kim, J.-S.; and Kwon, S. H., “Effects of an Externally Imposed Electromagnetic Field on the Formation of a Lubrication Layer in Concrete Pumping,” Construction and Building Materials, V. 61, 2014, pp. 18-23. doi: 10.1016/j.conbuildmat.2014.02.071

10. Feys, D., “How Much is Bulk Concrete Sheared during Pumping?” Construction and Building Materials, V. 223, 2019, pp. 341-351. doi: 10.1016/j.conbuildmat.2019.06.224

11. Choi, M.; Roussel, N.; Kim, Y.; and Kim, J., “Lubrication Layer Properties during Concrete Pumping,” Cement and Concrete Research, V. 45, 2013, pp. 69-78. doi: 10.1016/j.cemconres.2012.11.001

12. Phillips, R. J.; Armstrong, R. C.; Brown, R. A.; Graham, A. L.; and Abbott, J. R., “A Constitutive Equation for Concentrated Suspensions that Accounts for Shear-Induced Particle Migration,” Physics of Fluids. A, Fluid Dynamics, V. 4, No. 1, 1992, pp. 30-40. doi: 10.1063/1.858498

13. Leighton, D., and Acrivos, A., “A Constitutive Equation for Concentrated Suspensions that Accounts for Shear-Induced Particle Migration,” Journal of Fluid Mechanics, V. 177, 1987, pp. 109-131. doi: 10.1017/S0022112087000880

14. Choi, M. S.; Kim, Y. J.; and Kwon, S. H., “Prediction on Pipe Flow of Pumped Concrete Based on Shear-Induced Particle Migration,” Cement and Concrete Research, V. 52, 2013, pp. 216-224. doi: 10.1016/j.cemconres.2013.07.004

15. Ngo, T. T.; Kadri, E. H.; Bennacer, R.; and Cussigh, F., “Use of Tribometer to Estimate Interface Friction and Concrete Boundary Layer Composition during the Fluid Concrete Pumping,” Construction and Building Materials, V. 24, No. 7, 2010, pp. 1253-1261. doi: 10.1016/j.conbuildmat.2009.12.010

16. Ngo, T. T.; Kadri, E. H.; Cussigh, F.; Bennacer, R.; and Duval, R., “Practical Tribometer to Estimate Pumpability of Fresh Concrete,” Journal of Asian Architecture and Building Engineering, V. 9, No. 1, 2010, pp. 229-236. doi: 10.3130/jaabe.9.229

17. Kwon, S. H.; Park, C. K.; Jeong, J. H.; Jo, S. D.; and Lee, S. H., “Prediction of Concrete Pumping: Part I—Development of New Tribometer for Analysis of Lubricating Layer,” ACI Materials Journal, V. 110, No. 6, Nov.-Dec. 2013, pp. 647-655.

18. Feys, D.; Khayat, K. H.; Perez-Schell, A.; and Khatib, R., “Development of a Tribometer to Characterize Lubrication Layer Properties of Self-Consolidating Concrete,” Cement and Concrete Composites, V. 54, 2014, pp. 40-52. doi: 10.1016/j.cemconcomp.2014.05.008

19. Feys, D.; Khayat, K. H.; Perez-Schell, A.; and Khatib, R., “Prediction of Pumping Pressure by Means of New Tribometer for Highly-Workable Concrete,” Cement and Concrete Composites, V. 57, 2015, pp. 102-115. doi: 10.1016/j.cemconcomp.2014.12.007

20. Nerella, V. N., and Mechtcherine, V., “Virtual Sliding Pipe Rheometer for Estimating Pumpability of Concrete,” Construction and Building Materials, V. 170, 2018, pp. 366-377. doi: 10.1016/j.conbuildmat.2018.03.003

21. Secrieru, E.; Butler, M.; and Mechtcherine, V., “Testing Pumpability of Concrete - From Laboratory Into Practice,” Bautechnik, V. 91, No. 11, 2014, pp. 797-811. doi: 10.1002/bate.201400072

22. Choi, M. S.; Park, S. B.; and Kang, S.-T., “Effect of the Mineral Admixtures on Pipe Flow of Pumped Concrete,” Journal of Advanced Concrete Technology, V. 13, No. 11, 2015, pp. 489-499. doi: 10.3151/jact.13.489

23. Morinaga, S., “Pumpability of Concrete and Pumping Pressure in Pipelines,” Proceedings of RILEM Seminar, Leeds, UK, 1973, pp 1-39.

24. Jacobsen, S.; Haugan, L.; Hammer, T. A.; and Kalogiannidis, E., “Flow Conditions of Fresh Mortar and Concrete in Different Pipes,” Cement and Concrete Research, V. 39, No. 11, 2009, pp. 997-1006. doi: 10.1016/j.cemconres.2009.07.005

25. De Schutter, G., and Feys, D., “Pumping of Fresh Concrete: Insights and Challenges,” RILEM Technical Letters, V. 1, 2016, pp. 76-80. doi: 10.21809/rilemtechlett.2016.15

26. Le, H. D.; Kadri, E. H.; Aggoun, S.; Vierendeels, J.; Troch, P.; and De Schutter, G., “Effect of Lubrication Layer on Velocity Profile of Concrete in a Pumping Pipe,” Materials and Structures, V. 48, No. 12, 2015, pp. 3991-4003. doi: 10.1617/s11527-014-0458-5

27. Secrieru, E.; Mohamed, W.; Fataei, S.; and Mechtcherine, V., “Assessment and Prediction of Concrete Flow and Pumping Pressure in Pipeline,” Cement and Concrete Composites, V. 107, 2020, p. 103495. doi: 10.1016/j.cemconcomp.2019.103495

28. Chen, J.; Xie, H.; Guo, J.; Chen, B.; and Liu, F., “Preliminarily Experimental Research on Local Pressure Loss of Fresh Concrete during Pumping,” Measurement, V. 147, 2019, p. 106897. doi: 10.1016/j.measurement.2019.106897

29. Kaplan, D.; de Larrard, F.; and Sedran, T., “Design of Concrete Pumping Circuit,” ACI Materials Journal, V. 102, No. 2, Mar.-Apr. 2005, pp. 110-117.

30. Kwon, S. H.; Park, C. K.; Jeong, J. H.; Jo, S. D.; and Lee, S. H., “Prediction of Concrete Pumping: Part II-Analytical Prediction and Experimental Verification,” ACI Materials Journal, V. 110, No. 6, Nov.-Dec. 2013, pp. 657-667.

31. Jeong, J. H.; Jang, K. P.; Park, C. K.; Lee, S. H.; and Kwon, S. H., “Effect of Admixtures on Pumpability for High-Strength Concrete,” ACI Materials Journal, V. 113, No. 3, May-June 2016, pp. 323-333. doi: 10.14359/51688644

32. Jang, K. P., and Choi, M. S., “How Affect the Pipe Length of Pumping Circuit on Concrete Pumping,” Construction and Building Materials, V. 208, 2019, pp. 758-766. doi: 10.1016/j.conbuildmat.2019.03.023

33. Spangenberg, J.; Roussel, N.; Hattel, J. H.; Stang, H.; Skocek, J.; and Geiker, M. R., “Flow Induced Particle Migration in Fresh Concrete: Theoretical Frame, Numerical Simulations and Experimental Results on Model Fluids,” Cement and Concrete Research, V. 42, No. 4, 2012, pp. 633-641. doi: 10.1016/j.cemconres.2012.01.007

34. Kim, J. S.; Kwon, S. H.; Jang, K. P.; and Choi, M. S., “Concrete Pumping Prediction Considering Different Measurement of the Rheological Properties,” Construction and Building Materials, V. 171, 2018, pp. 493-503. doi: 10.1016/j.conbuildmat.2018.03.194

35. Feys, D.; De Schutter, G.; and Verhoeven, R., “Parameters Influencing Pressure during Pumping of Self-Compacting Concrete,” Materials and Structures, V. 46, No. 4, 2013, pp. 533-555. doi: 10.1617/s11527-012-9912-4

36. Jiao, D.; Shi, C.; Yuan, Q.; An, X.; Liu, Y.; and Li, H., “Effect of Constituents on Rheological Properties of Fresh Concrete—A Review,” Cement and Concrete Composites, V. 83, 2017, pp. 146-159. doi: 10.1016/j.cemconcomp.2017.07.016

37. Aissoun, B. M.; Hwang, S.-D.; and Khayat, K. H., “Influence of Aggregate Characteristics on Workability of Superworkable Concrete,” Materials and Structures, V. 49, No. 1-2, 2016, pp. 597-609. doi: 10.1617/s11527-015-0522-9

38. Tattersall, G. H., Workability and Quality Control of Concrete, E&FN Spon, London, UK, 1990.

39. Hu, J., and Wang, K., “Effect of Coarse Aggregate Characteristics on Concrete Rheology,” Construction and Building Materials, V. 25, No. 3, 2011, pp. 1196-1204. doi: 10.1016/j.conbuildmat.2010.09.035

40. Hu, J., “A Study of Effects of Aggregate on Concrete Rheology,” PhD dissertation, Iowa State University, Ames, IA, 2005.

41. Choi, M. S.; Kim, Y. J.; Jang, K. P.; and Kwon, S. H., “Effect of the Coarse Aggregate Size on Pipe Flow of Pumped Concrete,” Construction and Building Materials, V. 66, 2014, pp. 723-730. doi: 10.1016/j.conbuildmat.2014.06.027

42. Reinhardt, H. W., and Wuestholz, T., “About the Influence of the Content and Composition of the Aggregates on the Rheological Behaviour of Self-Compacting Concrete,” Materials and Structures, V. 39, No. 7, 2006, pp. 683-693. doi: 10.1617/s11527-006-9102-3

43. Uysal, M., and Sumer, M., “Performance of Self-Compacting Concrete Containing Different Mineral Admixtures,” Construction and Building Materials, V. 25, No. 11, 2011, pp. 4112-4120. doi: 10.1016/j.conbuildmat.2011.04.032

44. Zhang, Z.; Zhang, B.; and Yan, P., “Comparative Study of Effect of Raw and Densified Silica Fume in the Paste, Mortar and Concrete,” Construction and Building Materials, V. 105, 2016, pp. 82-93. doi: 10.1016/j.conbuildmat.2015.12.045

45. Sun, K.; Zhou, X.; Gong, C.; Ding, Y.; and Lu, L., “Influence of Paste Thickness on Coated Aggregates on Properties of High-Density Sulphoaluminate Cement Concrete,” Construction and Building Materials, V. 115, 2016, pp. 125-131. doi: 10.1016/j.conbuildmat.2016.04.018

46. Quanji, Z.; Lomboy, G. R.; and Wang, K., “Influence of Nano-Sized Highly Purified Magnesium Alumino Silicate Clay on Thixotropic Behavior of Fresh Cement Pastes,” Construction and Building Materials, V. 69, 2014, pp. 295-300. doi: 10.1016/j.conbuildmat.2014.07.050

47. Mechtcherine, V.; Nerella, V. N.; and Kasten, K., “Testing Pumpability of Concrete Using Sliding Pipe Rheometer,” Construction and Building Materials, V. 53, 2014, pp. 312-323. doi: 10.1016/j.conbuildmat.2013.11.037

48. Wallevik, O. H.; Feys, D.; Wallevik, J. E.; and Khayat, K. H., “Avoiding Inaccurate Interpretations of Rheological Measurements for Cement-Based Materials,” Cement and Concrete Research, V. 78, 2015, pp. 100-109. doi: 10.1016/j.cemconres.2015.05.003

49. Koehler, E., and Fowler, D., “Development of a Portable Rheometer for Fresh Portland Cement Concrete,” ICAR Report:103-105, 2004.

50. Kovler, K., and Roussel, N., “Properties of Fresh and Hardened Concrete,” Cement and Concrete Research, V. 41, No. 7, 2011, pp. 775-792. doi: 10.1016/j.cemconres.2011.03.009

51. Xie, H. B.; Liu, F.; Fan, Y. R.; Yang, H. Y.; Chen, J.; Zhang, J.; and Zuo, C. G., “Workability and Proportion Design of Pumping Concrete Based on Rheological Parameters,” Construction and Building Materials, V. 44, 2013, pp. 267-275. doi: 10.1016/j.conbuildmat.2013.02.051

52. Acrivos, A., “Shear-Induced Particle Diffusion in Concentrated Suspensions of a Noncolloidal Particles,” Journal of Rheology (New York, N.Y.), V. 39, No. 5, 1995, pp. 813-826. doi: 10.1122/1.550619

53. Roussel, N., and Cussigh, F., “Distinct-Layer Casting of SCC: The Mechanical Consequences of Thixotropy,” Cement and Concrete Research, V. 38, No. 5, 2008, pp. 624-632. doi: 10.1016/j.cemconres.2007.09.023


ALSO AVAILABLE IN:

Electronic Materials Journal