Three-Dimensional (3D)-Printed Wood-Starch Composite as Support Material for 3D Concrete Printing (Open Source)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Three-Dimensional (3D)-Printed Wood-Starch Composite as Support Material for 3D Concrete Printing (Open Source)

Author(s): Viacheslav Markin, Christof Schröfl, Paul Blankenstein, and Viktor Mechtcherine

Publication: Materials Journal

Volume: 118

Issue: 6

Appears on pages(s): 301-310

Keywords: material development; support material; sustainability; three-dimensional (3D) concrete printing

DOI: 10.14359/51733131

Date: 11/1/2021

Abstract:
The applicability of wood-based, starch-bonded composite materials for three-dimensional (3D)-printed temporal, fully recyclable support structures was studied experimentally with respect to delivering the specific geometric and load-bearing features of the product of a continuous 3D concrete printing process. Extrudability of the support material developed was verified by direct test using a conventional screw extruder. The observations and quantitative results were compared with those gained with a ram extruder. The development of the compressive strength of the support materials was analyzed experimentally from an early age, beginning a few minutes after extrusion. The results obtained confirmed the sufficiency of the product’s strength in withstanding prospective weight loads of concrete layers printed on top of the support. Furthermore, methods of enhancing early-age compressive strength were analyzed, and a most promising approach was experimentally implemented—namely, the deposition of the material under a constant defined airflow. In contrast to its promising mechanical material characteristics, massive fungi formation was observed as early as 1 day, amounting to a severe drawback. Consequently, improvements to the material’s composition are suggested that will not impair the environmental sustainability of the support material.

Related References:

1. Buswell, R. A.; Leal de Silva, W. R.; Jones, S. Z.; and Dirrenberger, J., “3D Printing Using Concrete Extrusion: A Roadmap for Research,” Cement and Concrete Research, V. 112, Oct. 2018, pp. 37-49. doi: 10.1016/j.cemconres.2018.05.006

2. Buswell, R. A.; da Silva, W. L.; Bos, F. P.; Schipper, H. R.; Lowke, D.; Hack, N.; Kloft, H.; Mechtcherine, V.; Wangler, T.; and Roussel, N., “A Process Classification Framework for Defining and Describing Digital Fabrication with Concrete,” Cement and Concrete Research, V. 134, Aug. 2020, pp. 1-12.

3. Mechtcherine, V.; Bos, F. P.; Perrot, A.; da Silva, W. L.; Nerella, V. N.; Fataei, S.; Wolfs, R. J. M.; Sonebi, M.; and Roussel, N., “Extrusion-Based Additive Manufacturing with Cement-Based Materials—Production Steps, Processes, and Their Underlying Physics: A Review,” Cement and Concrete Research, V. 132, June 2020, pp. 1-14. doi: 10.1016/j.cemconres.2020.106037

4. Menna, C.; Mata-Falcón, J.; Bos, F. P.; Vantyghem, G.; Ferrara, L.; Asprone, D.; Salet, T.; and Kaufmann, W., “Opportunities and Challenges for Structural Engineering of Digitally Fabricated Concrete,” Cement and Concrete Research, V. 133, July 2020, pp. 1-19.

5. De Schutter, G.; Lesage, K.; Mechtcherine, V.; Nerella, V. N.; Habert, G.; and Agusti-Juan, I., “Vision of 3D Printing with Concrete—Technical, Economic and Environmental Potentials,” Cement and Concrete Research, V. 112, Oct. 2018, pp. 25-36. doi: 10.1016/j.cemconres.2018.06.001

6. Xtree, “XtreeE—3D Printed Wall with Integrated Window Frame,” 2019, https://www.youtube.com/watch?v=0byQtXW5Gm8. (last accessed Nov. 5, 2021)

7. ICON—3D Tech, “ICON 3D-Printing for the Homeless in Austin,” 2019, https://www.youtube.com/watch?v=is2UVodNphY. (last accessed Nov. 5, 2021)

8. Rudenko, A., “3D-Printed Castle—Photo Gallery,” Total Kustom, 2015, http://www.totalkustom.com/photo.html. (last accessed Nov. 5, 2021)

9. Hoffmann, M.; Skibicki, S.; Pankratow, P.; Zieliński, A.; Pajor, M.; and Techman, M., “Automation in the Construction of a 3D-Printed Concrete Wall with the Use of a Lintel Gripper,” Materials (Basel), V. 13, No. 8, 2020, pp. 1-15. doi: 10.3390/ma13081800

10. Tay, Y. W. D.; Li, M. Y.; and Tan, M. J., “Effect of Printing Parameters in 3D Concrete Printing: Printing Region and Support Structures,” Journal of Materials Processing Technology, V. 271, Sept. 2019, pp. 261-270. doi: 10.1016/j.jmatprotec.2019.04.007

11. Molitch-Hou, M., “‘Finally, It Stands!’ Andrey Rudenko’s 3D-Printed Concrete Castle,” 2014, https://3dprintingindustry.com/news/finally-stands-andrey-rudenkos-3d-printed-concrete-castle-32097/. (last accessed Nov. 5, 2021)

12. Khoshnevis, B., “Automated Construction by Contour Crafting—Related Robotics and Information Technologies,” Automation in Construction, V. 13, No. 1, 2004, pp. 5-19. doi: 10.1016/j.autcon.2003.08.012

13. Kondo, H., “3D Printer Support Material: Which One to Use for My Project?” All3DP, 2019, https://all3dp.com/2/3d-printer-support-material-which-one-to-use-for-my-project/. (last accessed Nov. 5, 2021)

14. Ngo, T. D.; Kashani, A.; Imbalzano, G.; Nguyen, K. T. Q.; and Hui, D., “Additive Manufacturing (3D Printing): A Review of Materials, Methods, Applications and Challenges,” Composites Part B: Engineering, V. 143, June 2018, pp. 172-196. doi: 10.1016/j.compositesb.2018.02.012

15. Duballet, R.; Baverel, O.; and Dirrenberger, J., “Classification of Building Systems for Concrete 3D Printing,” Automation in Construction, V. 83, Nov. 2017, pp. 247-258. doi: 10.1016/j.autcon.2017.08.018

16. Kaufhold, J.; Kohl, J.; Nerella, V. N.; Schroefl, C.; Wenderdel, C.; Blankenstein, P.; and Mechtcherine, V., “Wood-Based Support Material for Extrusion-Based Digital Construction,” Rapid Prototyping Journal, V. 4, No. 12, 2019, pp. 690-698. doi: 10.1108/RPJ-04-2018-0109

17. Belitz, H.-D.; Grosch, W.; and Schieberle, P., “Lehrbuch der Lebensmittelchemie: Mit 634 Tabellen,” Sechste, Vollständig Überarbeitete Auflage, Springer, Berlin, 2008, 1118 pp.

18. Nerella, V. N.; Näther, M.; Iqbal, A.; Butler, M.; and Mechtcherine, V., “Inline Quantification of Extrudability of Cementitious Materials for Digital Construction,” Cement and Concrete Composites, V. 95, Jan. 2019, pp. 260-270. doi: 10.1016/j.cemconcomp.2018.09.015

19. Nerella, V. N.; Hempel, S.; and Mechtcherine, V., “Effects of Layer-Interface Properties on Mechanical Performance of Concrete Elements Produced by Extrusion-Based 3D-Printing,” Construction and Building Materials, V. 205, Apr. 2019, pp. 586-601. doi: 10.1016/j.conbuildmat.2019.01.235

20. Ivaniuk, E., “Investigations on Very Early Strength of 3D-Printable Cementitious Materials,” Project Report Submitted in Partial Fulfilment of the Requirement for the Award of the MSc Degree, Technische Universität Dresden, Dresden, Germany, 2019.

21. Ghourchian, S.; Butler, M.; Krüger, M.; and Mechtcherine, V., “Modelling the Development of Capillary Pressure in Freshly 3D-Printed Concrete Elements,” Cement and Concrete Research, V. 145, July 2021, p. 106457. doi: 10.1016/j.cemconres.2021.106457

22. Perrot, A.; Mélinge, Y.; Rangeard, D.; Micaelli, F.; Estellé, P.; and Lanos, C., “Use of Ram Extruder as a Combined Rheo-Tribometer to Study the Behaviour of High Yield Stress Fluids at Low Strain Rate,” Rheologica Acta, V. 51, No. 8, 2012, pp. 743-754. doi: 10.1007/s00397-012-0638-6

23. Perrot, A.; Rangeard, D.; Mélinge, Y.; Estellé, P.; and Lanos, C., “Extrusion Criterion for Firm Cement-Based Materials,” Applied Rheology (Lappersdorf, Germany), V. 19, No. 5, 2009, p. 53042

24. Khelifi, H.; Perrot, A.; Lecompte, T.; Rangeard, D.; and Ausias, G., “Prediction of Extrusion Load and Liquid Phase Filtration during Ram Extrusion of High Solid Volume Fraction Pastes,” Powder Technology, V. 249, No. 6, 2013, pp. 258-268. doi: 10.1016/j.powtec.2013.08.023

25. Gordon, S. M., and Avery, R. K., “Aspergillosis in Lung Transplantation: Incidence, Risk Factors, and Prophylactic Strategies,” Transplant Infectious Disease, V. 3, No. 3, 2001, pp. 161-167. doi: 10.1034/j.1399-3062.2001.003003161.x