Rheological Response of Magnetorheological Cementitious Inks Tuned for Active Control in Digital Construction

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Rheological Response of Magnetorheological Cementitious Inks Tuned for Active Control in Digital Construction

Author(s): Aparna S. Deshmukh, Reed T. Heintzkill, Rosalba A. Huerta, and Konstantin Sobolev

Publication: Materials Journal

Volume: 118

Issue: 6

Appears on pages(s): 263-274

Keywords: additive manufacturing; Bingham-Papanastasiou model; Class F fly ash; four-dimensional (4D) printing; magnetorheology; nanomaterials; rheology; smart materials; three-dimensional (3D) printing of concrete

DOI: 10.14359/51733128

Date: 11/1/2021

Abstract:
Systematically designed cement mixtures incorporating various proportions of portland cement (PC), high-ferrous Class F fly ash (FA), nanosilica (NS), and nanoalumina (NA) were blended and characterized for rheological response with and without the application of a magnetic field to better understand the effects of doping cement with magnetic material for application in four-dimensional (4D) printing of cementitious smart materials (SM). Control groups doped with industrial-grade magnetite powder (primarily used as pigment) were likewise mixed and characterized to provide contrast to coal-combustion byproduct FA. Mixtures supplemented with ferromagnetic particles showed increased yield stress when exposed to applied magnetic field, leading to non-Newtonian rheological models exhibiting ‘sticky particles’ paradigms as discussed herein. These results suggest that the principle of using an applied magnetic field to modify the flow and slump of cementitious materials extruded through a three-dimensional (3D) printing apparatus is worthy of further pursuit and development.

Related References:

1. Bos, F.; Wolfs, R.; Ahmed, Z.; and Salet, T., “Additive Manufacturing of Concrete in Construction: Potentials and Challenges of 3D Concrete Printing,” Virtual and Physical Prototyping, V. 11, No. 3, 2016, pp. 209-225. doi: 10.1080/17452759.2016.1209867

2. Bogue, R., “Smart Materials: A Review of Capabilities and Applications,” Assembly Automation, V. 34, No. 1, 2014, pp. 16-22. doi: 10.1108/AA-10-2013-094

3. Tibbits, S., “The Emergence of ‘4D Printing,’” filmed in Long Beach, CA, TED video, 8:10, https://www.ted.com/talks/skylar_tibbits_the_emergence_of_4d_printing.

4. Tibbits, S., “4D Printing: Multi-Material Shape Change,” Architectural Design, V. 84, No. 1, 2014, pp. 116-121. doi: 10.1002/ad.1710

5. Momeni, F., and Mehdi Hassani, “A Review of 4D Printing,” Materials & Design, V. 122, 2017, pp. 42-79. doi: 10.1016/j.matdes.2017.02.068

6. Kuang, X.; Roach, D. J.; Wu, J.; Hamel, C. M.; Ding, Z.; Wang, T.; Dunn, M. L.; and Qi, H. J., “Advances in 4D Printing: Materials and Applications,” Advanced Functional Materials, V. 29, No. 2, 2019, p. 1805290. doi: 10.1002/adfm.201805290

7. Sossou, C., “A Holistic Approach to Design for 4D Printing,” doctoral thesis, Universite Bourgogne Franche-Comté, Besançon, France, 2019, 202 pp.

8. Wallevik, O. H., and Wallevik, J. E., “Rheology as a Tool in Concrete Science: The Use of Rheographs and Workability Boxes,” Cement and Concrete Research, V. 41, No. 12, 2011, pp. 1279-1288. doi: 10.1016/j.cemconres.2011.01.009

9. Nair, S. D., and Ferron, R. D., “Set-on-Demand Concrete,” Cement and Concrete Research, V. 57, 2014, pp. 13-27. doi: 10.1016/j.cemconres.2013.12.001

10. Jiao, D.; Lesage, K.; Yardimci, M. Y.; El Cheikh, K.; Shi, C.; and De Schutter, G., “Quantitative Assessment of the Influence of External Magnetic Field on Clustering of Nano-Fe3O4 Particles in Cementitious Paste,” Cement and Concrete Research, V. 142, 2021, p. 106345. doi: 10.1016/j.cemconres.2020.106345

11. Ashtiani, M.; Hashemabadi, S. H.; and Ghaffari, A., “A Review on the Magnetorheological Fluid Preparation and Stabilization,” Journal of Magnetism and Magnetic Materials, V. 374, 2015, pp. 716-730. doi: 10.1016/j.jmmm.2014.09.020

12. Carlson, J. D., and Jolly, M. R., “MR Fluid, Foam and Elastomer Devices,” Mechatronics, V. 10, Issues 4-5, June 2000, pp. 555-569.

13. Liu, Y. D.; Hong, C. H.; and Choi, H. J., “Polymeric Colloidal Magnetic Composite Microspheres and Their Magneto-Responsive Characteristics,” Macromolecular Research, V. 20, No. 12, 2012, pp. 1211-1218. doi: 10.1007/s13233-012-0198-8

14. Li, W. H.; Chen, G.; and Yeo, S. H., “Viscoelastic Properties of MR Fluids,” Smart Materials and Structures, V. 8, No. 4, 1999, pp. 460-468. doi: 10.1088/0964-1726/8/4/303

15. Bingham, E. C., “An Investigation of the Laws of Plastic Flow,” Bulletin of the Bureau of Standards, V. 13, No. 2, 1916, p. 309. doi: 10.6028/bulletin.304

16. Olabi, A. G., and Grunwald, A., “Design and Application of Magneto-Rheological Fluid ‘MRF,’” Materials & Design, V. 28, No. 10, 2007, pp. 2658-2664.

17. Acary-Robert, C.; Fernández-Nieto, E. D.; Narbona-Reina, G.; and Vigneaux, P., “Viscoplastic Free-Surface Flows: The Herschel-Bulkley Case,” Seventh International Conference on Computational Fluid Dynamics (ICCFD7), Kamuela, HI, July 9-13, 2012, 15 pp.

18. Chooi, W. W., and Oyadiji, S. O., “Design, Modelling and Testing of Magnetorheological (MR) Dampers Using Analytical Flow Solutions,” Computers & Structures, V. 86, No. 3-5, 2008, pp. 473-482. doi: 10.1016/j.compstruc.2007.02.002

19. de Vicente, J.; Klingenberg, D. J.; and Hidalgo-Alvarez, R., “Magnetorheological Fluids: A Review,” Soft Matter, V. 7, No. 8, 2011, p. 3701. doi: 10.1039/c0sm01221a

20. Park, J. H.; Kwon, M. H.; and Park, O. O., “Rheological Properties and Stability of Magnetorheological Fluids Using Viscoelastic Medium and Nanoadditives,” Korean Journal of Chemical Engineering, V. 18, No. 5, 2001, pp. 580-585. doi: 10.1007/BF02706371

21. Guerrero-Sanchez, C.; Lara-Ceniceros, T.; Jimenez-Regalado, E.; Raşa, M.; and Schubert, U. S., “Magnetorheological Fluids Based on Ionic Liquids,” Advanced Materials, V. 19, No. 13, 2007, pp. 1740-1747. doi: 10.1002/adma.200700302

22. Bica, I.; Liu, Y. D.; and Choi, H. J., “Physical Characteristics of Magnetorheological Suspensions and Their Applications,” Journal of Industrial and Engineering Chemistry, V. 19, No. 2, 2013, pp. 394-406. doi: 10.1016/j.jiec.2012.10.008

23. Nair, S. D., and Ferron, R. D., “Real Time Control of Fresh Cement Paste Stiffening: Smart Cement-Based Materials Via a Magnetorheological Approach,” Rheologica Acta, V. 55, No. 7, 2016, pp. 571-579. doi: 10.1007/s00397-016-0923-x

24. De Schutter, G., and Lesage, K., “Active Control of Properties of Concrete: A (P)review,” Materials and Structures, V. 51, No. 5, 2018, p. 123. doi: 10.1617/s11527-018-1256-2

25. Kosson, M.; Brown, L.; and Sanchez, F., “Early-Age Performance of 3D Printed Carbon Nanofiber and Carbon Microfiber Cement Composites,” Transportation Research Record: Journal of the Transportation Research Board, V. 2674, No. 2, 2020, pp. 10-20. doi: 10.1177/0361198120902704

26. Sobolev, K., and Ferrada Gutiérrez, M., “How Nanotechnology Can Change the Concrete World,” Progress in Nanotechnology, John Wiley & Sons, Inc., Hoboken, NJ, 2014. pp. 113-116.

27. Li, Q.; Gao, X.; and Xu, S., “Multiple Effects of Nano-SiO2 and Hybrid Fibers on Properties of High Toughness Fiber Reinforced Cementitious Composites with High-Volume Fly Ash,” Cement and Concrete Composites, V. 72, 2016, pp. 201-212. doi: 10.1016/j.cemconcomp.2016.05.011

28. Muzenski, S.; Flores-Vivian, I.; and Sobolev, K., “Ultra-High Strength Cement-Based Composites Designed With Aluminum Oxide Nano-Fibers,” Construction and Building Materials, V. 220, 2019, pp. 177-186. doi: 10.1016/j.conbuildmat.2019.05.175

29. Flores-Vivian, I.; Hejazi, V.; Kozhukhova, M. I.; Nosonovsky, M.; and Sobolev, K., “Self-Assembling Particle-Siloxane Coatings for Superhydrophobic Concrete,” ACS Applied Materials & Interfaces, V. 5, No. 24, 2013, pp. 13284-13294. doi: 10.1021/am404272v

30. Collepardi, M.; Collepardi, S.; Skarp, U.; and Troli, R., “Optimization of Silica Fume, Fly Ash, and Amorphous Nano-Silica in Superplasticized High-Performance Concretes,” Eighth CANMET/ACI International Conference on Fly Ash, Silica Fume, Slag, and Natural Pozzolans in Concrete, SP-221, V. M. Malhotra, ed., American Concrete Institute, Farmington Hills, MI, 2004, 963 pp.

31. Serna, P.; Monte, F. L.; Mezquida-Alcaraz, E. J.; and Cuenca, E., “Upgrading the Concept of UHPFRC For High Durability in the Cracked State: The Concept of Ultra High Durability Concrete (UHDC) in the Approach of the H2020 Project Reshealience,” RILEM Publications SARL V. 128: Sustainable Materials Systems and Structures, SMMS 2019, Croatia, 8 pp.

32. Jiao, D.; El Cheikh, K.; Shi, C.; Lesage, K.; and De Schutter, G., “Structural Build-Up of Cementitious Paste with Nano-Fe3O4 under Time-Varying Magnetic Fields,” Cement and Concrete Research, V. 124, 2019, p. 105857. doi: 10.1016/j.cemconres.2019.105857

33. Martys, N. S.; Peltz, M. A.; George, W. L.; Toman, B.; and Garboczi, E. J., “Certification of SRM 2497: Standard Reference Concrete for Rheological Measurements,” NIST SP 260-194, National Institute of Standards and Technology, Gaithersburg, MD, 2019.

34. ASTM C305-99, “Standard Practice for Mechanical Mixing of Hydraulic Cement Pastes and Mortars of Plastic Consistency,” ASTM International, West Conshohocken, PA, 1999, 3 pp.

35. Banfill, P. F. G., ed., Rheology of Fresh Cement and Concrete, Taylor & Francis, Abingdon, UK, 1991.

36. Banfill, P. F. G., “The Rheology of Fresh Cement and Concrete – A Review,” th International Cement Chemistry Congress, Durban, South Africa, May 2003, 14 pp.

37. Zhu, H.; Martys, N. S.; Ferraris, C.; and Kee, D. D., “A Numerical Study of the Flow of Bingham-Like Fluids in Two-Dimensional Vane and Cylinder Rheometers Using a Smoothed Particle Hydrodynamics (SPH) Based Method,” Journal of Non-Newtonian Fluid Mechanics, V. 165, No. 7-8, 2010, pp. 362-375. doi: 10.1016/j.jnnfm.2010.01.012

38. Roussel, N.; Stefani, C.; and Leroy, R., “From Mini-Cone Test to Abrams Cone Test: Measurement of Cement-Based Materials Yield Stress Using Slump Tests,” Cement and Concrete Research, V. 35, No. 5, 2005, pp. 817-822. doi: 10.1016/j.cemconres.2004.07.032

39. Assaad, J., and Khayat, K. H., “Assessment of Thixotropy of Self-Consolidating Concrete and Concrete-Equivalent-Mortar—Effect of Binder Composition and Content,” ACI Materials Journal, V. 101, No. 5, Sept.-Oct. 2004, pp. 400-408.

40. Ferron, R. P.; Gregori, A.; Sun, Z.; and Shah, S. P., “Rheological Method to Evaluate Structural Buildup in Self-Consolidating Concrete Cement Pastes,” ACI Materials Journal, V. 104, No. 3, May-June 2007, pp. 242-250.


ALSO AVAILABLE IN:

Electronic Materials Journal