Self Deicing and Strain Sensing Functionalities of Smart Concrete: Advanced Electrothermic Efficiency and Electromechanical Impedance Sensitivity

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Self Deicing and Strain Sensing Functionalities of Smart Concrete: Advanced Electrothermic Efficiency and Electromechanical Impedance Sensitivity

Author(s): Maria Konsta

Publication: Web Session

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 4/1/2021

Abstract:
New functionalities based on the advanced electrothermic and electromechanical properties of concrete with embedded nanoscale carbon fiber networks are presented. Nanofibers alter the nanocomposites’ heating characteristics leading to a rapidly accelerated deicing process under the application of a low electric current. A strong piezoelectric behavior is also reported by optimizing the fractional change of nanocomposites’ capacitance.