Title: Reducing Drying Shrinkage and Micro-Cracking in Concrete using Superabsorbent Cellulose Fibers

Author(s): Afraa Hassan

Publication: Web Session

Volume: ws_S21_Hassan.pdf

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 4/1/2021

Abstract: