Simple Test Method for Determining Shear Strength of Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Simple Test Method for Determining Shear Strength of Concrete

Author(s): Muhammad N. S. Hadi, Umer Sajjad, and M. Neaz Sheikh

Publication: Materials Journal

Volume: 119

Issue: 1

Appears on pages(s): 173-180

Keywords: double shear; high-strength concrete; normal-strength concrete; shear fracture; shear strength of concrete; test method

DOI: 10.14359/51732986

Date: 1/1/2022

Abstract:
Various test methods and techniques are used to determine the shear strength of concrete. However, the available test methods and techniques used for determining the shear strength of concrete are prone to several inconsistencies and limitations, which cause inaccuracies in measuring the shear strength of concrete. A simple test method is proposed in this paper to achieve an accurate measurement of the shear strength of concrete. The proposed method was applied to two groups of concrete representing normal-strength concrete and high-strength concrete. The specimens failed at locations where the area was reduced, providing an accurate estimate of the shear strength of concrete.

Related References:

1. Bažant, Z., and Pfeiffer, P., “Shear Fracture Tests of Concrete,” Materials and Structures, V. 19, No. 2, 1986, pp. 111-121. doi: 10.1007/BF02481755

2. Xu, B.; Bompa, D.; Elghazouli, A.; Ruiz-Teran, A.; and Stafford, P., “Behaviour of Rubberised Concrete Members in Asymmetric Shear Tests,” Construction and Building Materials, V. 159, 2018, pp. 361-375. doi: 10.1016/j.conbuildmat.2017.10.091

3. Khanlou, A.; MacRae, G.; Scott, A.; Hicks, S.; and Clifton, G., “Shear Performance of Steel Fiber-Reinforced Concrete,” Engineering: Conference Contributions, Australasian Structural Engineering Conference, Perth Australia, July 11-13, 2012.

4. Tuan, H. N.; Otsuka, H.; Ishikawa, Y.; and Takeshita, E., “A Study on Shear Strength of Concrete under Direct Shear Test,” JCI Proceedings, V. 28, No. 1. 2006, pp. 1529-1534.

5. Sharma, A., “Shear Strength of Steel Fiber Reinforced Concrete Beams,” ACI Journal Proceedings, V. 83, No. 4, July-Aug. 1986, pp. 624-628.

6. Kani, G., “The Riddle of Shear Failure and Its Solution,” ACI Journal Proceedings, V. 61, No. 4, Apr. 1964, pp. 441-468.

7. Arezoumandi, M.; Smith, A.; Volz, J. S.; and Khayat, K. H., “An Experimental Study on Shear Strength of Reinforced Concrete Beams with 100% Recycled Concrete Aggregate,” Construction and Building Materials, V. 53, 2014, pp. 612-620. doi: 10.1016/j.conbuildmat.2013.12.019

8. Kwak, Y. K.; Eberhard, M. O.; Kim, W. S.; and Kim, J., “Shear Strength of Steel Fiber-Reinforced Concrete Beams without Stirrups,” ACI Structural Journal, V. 99, No. 4, July-Aug. 2002, pp. 530-538.

9. Mansur, M.; Ong, K.; and Paramasivam, P., “Shear Strength of Fibrous Concrete Beams without Stirrups,” Journal of Structural Engineering, ASCE, V. 112, No. 9, 1986, pp. 2066-2079. doi: 10.1061/(ASCE)0733-9445(1986)112:9(2066)

10. Bentz, E. C.; Vecchio, F. J.; and Collins, M. P., “Simplified Modified Compression Field Theory for Calculating Shear Strength of Reinforced Concrete Elements,” ACI Structural Journal, V. 103, No. 4, July-Aug. 2006, pp. 614-624.

11. Fédération Internationale de la Précontrainte, “Shear at the Interface of Precast and In-Situ Concrete,” Lausanne, Switzerland, 1978.

12. JSCE-SF6, “Method of Test for Shear Strength of Steel Fiber Reinforced Concrete (SFRC),” Japanese Society of Civil Engineering, Tokyo, Japan, 1990, pp. 67-69.

13. Wang, W.; Kou, S.; and Xing, F., “Deformation Properties and Direct Shear of Medium Strength Concrete Prepared with 100% Recycled Coarse Aggregates,” Construction and Building Materials, V. 48, 2013, pp. 187-193. doi: 10.1016/j.conbuildmat.2013.06.065

14. Mirsayah, A. A., and Banthia, N., “Shear Strength of Steel Fiber-Reinforced Concrete,” ACI Materials Journal, V. 99, No. 5, Sept.-Oct. 2002, pp. 473-479.

15. Davies, J., “Fracture Behaviour of Mortar in Shear-Compression Field,” Journal of Materials Science Letters, V. 6, No. 8, 1987, pp. 879-881. doi: 10.1007/BF01729856

16. Boulifa, R.; Samai, M. L.; and Benhassine, M. T., “A New Technique for Studying the Behaviour of Concrete in Shear,” Journal of King Saud University-Engineering Sciences, V. 25, No. 2, 2013, pp. 149-159. doi: 10.1016/j.jksues.2012.07.001

17. Uomoto, K., and Minematsu, T., “Fundamental Study on Testing Method for Shear Strength of Concrete,” Concrete Engineering, V. 23, No. 3, Mar. 1985, pp. 17-18.

18. Hofbeck, J. A.; Ibrahim, I. O.; and Mattock, A. H., “Shear Transfer in Reinforced Concrete,” ACI Journal Proceedings, V. 66, No. 2, Feb. 1969, pp. 119-128.

19. Jang, H. O.; Lee, H. S.; Cho, K.; and Kim, J., “Numerical and Experimental Analysis of the Shear Behavior of Ultrahigh-Performance Concrete Construction Joints,” Advances in Materials Science and Engineering, 2018, pp. 1-17. doi: 10.1155/2018/6429767

20. Wong, R.; Ma, S.; Wong, R.; and Chau, K., “Shear Strength Components of Concrete under Direct Shearing,” Cement and Concrete Research, V. 37, No. 8, 2007, pp. 1248-1256. doi: 10.1016/j.cemconres.2007.02.021

21. Bairagi, N., and Modhera, C., “An Experimental Study of Shear Strength Test Method for SFRC,” Proceedings of International Conference on Advances in Concrete and Construction, V. 1, No. 1, 2004.

22. Rahal, K., “Mechanical Properties of Concrete with Recycled Coarse Aggregate,” Building and Environment, V. 42, No. 1, 2007, pp. 407-415. doi: 10.1016/j.buildenv.2005.07.033

23. Alhussainy, F.; Hasan, H. A.; Sheikh, M. N.; and Hadi, M. N. S., “A New Method for Direct Tensile Testing of Concrete,” Journal of Testing and Evaluation, V. 47, No. 2, 2019, pp. 704-718. doi: 10.1520/JTE20170067

24. AS 1012.3.1-2014, “Methods of Testing Concrete-Method 3.1: Determination of Properties Related to the Consistency of Concrete-Slump Test,” 2014, 6 pp.

25. AS 1012.9-14, “Methods of Testing Concrete—Method 9: Determination of the Compressive Strength of Concrete Specimens,” Standards Australia, Sydney, NSW, Australia, 2014, 12 pp.

26. AS 1012.10-2000, “Methods of Testing Concrete—Method 10: Determination of Indirect Tensile Strength of Concrete Cylinders (Brazil or Splitting Test) (R2014),” Standards Australia, Sydney, NSW, Australia, 2000, 5 pp.

27. AS 1012.11-2000, “Methods of Testing Concrete—Method 11: Determination of Modulus of Rupture (R2014),” Standards Australia, Sydney, NSW, Australia, 2000, 5 pp.

28. AS 1012.17-1997-R2014, “Method of Testing Concrete—Method 17: Determination of the Static Chord Modulus of Elasticity and Poisson’s Ratio of Concrete Specimens,” Standards Australia, Sydney, NSW, Australia, 2014, 11 pp.

29. Sadowski, Ł., and Mathia, T. G., “Multi-Scale Metrology of Concrete Surface Morphology: Fundamentals and Specificity,” Construction and Building Materials, V. 113, 2016, pp. 613-621. doi: 10.1016/j.conbuildmat.2016.03.099

30. Feng, H.; Chen, G.; Hadi, M. N. S.; Sheikh, M. N.; and Zhou, B., “Mechanical Behaviour of Micro-Fine Steel Fiber Reinforced Sulphoaluminate Cement Composite,” Construction and Building Materials, V. 170, 2018, pp. 91-100. doi: 10.1016/j.conbuildmat.2018.03.065

31. Tran, T. M., and Hadi, M. N. S., “Shear Strength Model of Reinforced-Concrete Exterior Joint under Cyclic Loading,” Proceedings of the Institution of Civil Engineers. Structures and Buildings, V. 170, No. 8, 2017, pp. 603-617. doi: 10.1680/jstbu.15.00022

32. Algburi, A. H.; Sheikh, M. N.; and Hadi, M. N., “Mechanical Properties of Steel, Glass, and Hybrid Fiber Reinforced Reactive Powder Concrete,” Frontiers of Structural and Civil Engineering, V. 13, No. 4, 2019, pp. 998-1006. doi: 10.1007/s11709-019-0533-7

33. Boulekbache, B.; Hamrat, M.; Chemrouk, M.; and Amziane, S., “Influence of Yield Stress and Compressive Strength on Direct Shear Behaviour of Steel Fiber-Reinforced Concrete,” Construction and Building Materials, V. 27, No. 1, 2012, pp. 6-14. doi: 10.1016/j.conbuildmat.2011.07.015

34. Khaloo, A. R., and Kim, N., “Influence of Concrete and Fiber Characteristics on Behavior of Steel Fiber Reinforced Concrete under Direct Shear,” ACI Materials Journal, V. 94, No. 6, Nov.-Dec. 1997, pp. 592-601.

35. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19),” American Concrete Institute, Farmington Hills, MI, 2019, 624 pp.

36. CSA A23.3-14, “Design of Concrete Structures,” Canadian Standards Association, Rexdale, ON, Canada, 2014.

37. Rombach, G. A.; Kohl, M.; and Nghiep, V. H., “Shear Design of Concrete Members without Shear Reinforcement—A Solved Problem?” Procedia Engineering, V. 14, 2011, pp. 134-140. doi: 10.1016/j.proeng.2011.07.015

38. Al-Sahawneh, E., “A New Approach for the Determination of Tensile and Shear Strengths of Normal Weight Concrete,” Journal of Engineering (Stevenage, England), V. 5, No. 8, 2015, pp. 38-48.

39. Banthia, N.; Majdzadeh, F.; Wu, J.; and Bindiganavile, V., “Fiber Synergy in Hybrid Fiber Reinforced Concrete (HyFRC) in Flexure and Direct Shear,” Cement and Concrete Composites, V. 48, 2014, pp. 91-97. doi: 10.1016/j.cemconcomp.2013.10.018

40. Gao, K.; Lin, K. L.; Wang, D.; Hwang, C. L.; Anh Tuan, B. L.; Shiu, H. S.; and Cheng, T. W., “Effect of Nano-SiO2 on the Alkali-Activated Characteristics of Metakaolin-Based Geopolymers,” Construction and Building Materials, V. 48, 2013, pp. 441-447. doi: 10.1016/j.conbuildmat.2013.07.027


ALSO AVAILABLE IN: