Constructability of Zero Lot Lines Foundations with Shotcrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Constructability of Zero Lot Lines Foundations with Shotcrete

Author(s): Hanskat

Publication: Web Session

Volume: ws_2021_Hanskat_ZeroLotLines.pdf

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 4/1/2021

Abstract:
Zero-lot-line building foundations have been widely used for supporting new structures in close proximity to existing buildings in congested metropolitan areas. This presentation from the American Shotcrete Association will cover design and construction aspects of these walls and highlight how shotcrete placement provides superior strength, flexibility, efficiency, and durability.