Elastic Modulus of Concrete: Influence of Steam Curing

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Elastic Modulus of Concrete: Influence of Steam Curing

Author(s): R. Girardi, D. C. Dal Molin, F. A. P. Recena, and F. Tiecher

Publication: Materials Journal

Volume: 118

Issue: 5

Appears on pages(s): 107-114

Keywords: elastic modulus; humid curing; thermal steam curing

DOI: 10.14359/51732936

Date: 9/1/2021

Abstract:
To dimension the structural systems of reinforced or prestressed concrete, it is necessary to know at least the elastic modulus and the compressive strength of the concrete. This is because several factors directly influence these two properties, from the dosage to the procedure adopted for curing the concrete. Therefore, this study aims to present the influence of two different types of curing (humid and thermal steam) over the elastic modulus of the concrete. The results demonstrate that a significant reduction occurs on the modulus when the concrete is submitted to thermal steam curing. Additionally, the increase in the volume of the paste in the mixture reduces the stiffness of the compound.

Related References:

1. Aguilar, M. T. P; Silva, A. P.; Corrêa, E. C. S.; and Cetlin, P. R., “Análise da Capacidade de Deformação do Concreto: Módulo de Young × Módulo de Deformação,” Proceedings, 17º CBECIMat—Congresso Brasileiro de Engenharia e Ciência dos Materiais, Foz do Iguaçu, Paraná, Brazil, 2006, pp. 3672-3684.

2. de Melo Neto, A. A., and do Lago Helene, P. R., “Módulo de Elasticidade e Avaliação de Modelos de Previsão do Módulo de Elasticidade de Concretos,” Proceedings, Anais do 44º Congresso Brasileiro do Concreto (IBRACON), Belo Horizonte, Minas Gerais, Brazil, 2002, 17 pp.

3. Montija, F. C., “Aspectos da Variabilidade Experimental do Ensaio de Módulo de Deformação do Concreto,” master’s dissertation, Polytechnic School of the University of São Paulo, SP, Brazil, 2007, 260 pp.

4. Alsalman, A.; Dang, C. N.; Prinz, G. S.; and Hale, W. M., “Evaluation of Modulus of Elasticity of Ultra-High Performance Concrete,” Construction and Building Materials, V. 153, Oct. 2017, pp. 918-928. doi: 10.1016/j.conbuildmat.2017.07.158

5. Tibbetts, C. M.; Perry, M. C.; Ferraro, C. C.; and Hamilton, H. R., “Aggregate Correction Factors for Concrete Elastic Modulus Prediction,” ACI Structural Journal, V. 115, No. 4, July 2018, pp. 931-941. doi: 10.14359/51701914

6. Davraz, M.; Ceylan, H.; Topçu, İ. B.; and Uygunoğlu, T., “Pozzolanic Effect of Andesite Waste Powder on Mechanical Properties of High Strength Concrete,” Construction and Building Materials, V. 165, Mar. 2018, pp. 494-503. doi: 10.1016/j.conbuildmat.2018.01.043

7. Neville, A. M., and Brooks, J. J., Tecnologia do Concreto, second edition, Tradução Ruy Alberto Cremonini, Bookman, Porto Alegre, RS, Brazil, 2013, 468 pp.

8. de Arruda, A. M., “Módulo de Elasticidade de Concretos Produzidos com Formações Rochosas do Triângulo Mineiro,” master’s dissertation, graduate program in civil engineering, the Federal University of Uberlândia, Uberlândia, MG, Brazil, 2013, 166 pp.

9. Oliveira, T. S., and Cardoso, A. C. S., “Deformação Lenta das Estruturas de Concreto Armado e Suas Manifestações Patológicas,” Revista de Engenharia e Tecnologia, V. 10, No. 3, 2018, pp. 195-206.

10. EN 1992-1-1:2004, “Eurocode 2: Design of Concrete Structures—Part 1-1: General Rules and Rules for Buildings,” European Committee for Standardization, Brussels, Belgium, 2004, 227 pp.

11. Fédération internationale du béton, “fib Model Code for Concrete Structures 2010,” Lausanne, Switzerland, 2010, 434 pp.

12. Leal, A. C. F. S., “Investigação Experimental do Módulo de Elasticidade nos Concretos Produzidos em Brasília,” master’s dissertation, Department of Civil and Environmental Engineering, the University of Brasília, FD, Brazil, 2012, 151 pp.

13. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 520 pp.

14. ABNT NBR 6118, “Projeto de Estruturas de Concreto—Procedimento,” Associação Brasileira de Normas Técnicas, Rio de Janeiro, Brazil, 2014, 238 pp.

15. Bilesky, P. C., “Contribuição aos Estudos do Módulo de Elasticidade do Concreto,” Master’s dissertation, graduate program in civil engineering, Instituto de Pesquisas Tecnológicas (IPT) do Estado de São Paulo, SP, Brazil, 2016, 137 pp.

16. Girardi, R.; Dal Molin, D. C. C.; and Recena, F. A. P., “Portland Cement Concrete Deformation Modulus: Influence of Paste Volume,” ACI Materials Journal, V. 117, No. 1, Jan. 2020, pp. 39-46. doi: 10.14359/51719068

17. Aïtcin, P.-C., and Mehta, P. K., “Effect of Coarse Aggregate Characteristics on Mechanical Properties of High-Strength Concrete,” ACI Materials Journal, V. 87, No. 2, Mar.-Apr. 1990, pp. 103-107.

18. Baalbaki, W.; Benmokrane, B.; Chaallal, O.; and Aïtcin, P.-C., “Influence of Coarse Aggregate on Elastic Properties of High-Performance Concrete,” ACI Materials Journal, V. 88, No. 5, Sept.-Oct. 1991, pp. 499-503.

19. Li, G.; Zhao, Y.; Pang, S.-S.; and Li, Y., “Effective Young’s Modulus Estimation of Concrete,” Cement and Concrete Research, V. 29, No. 9, Sept. 1999, pp. 1455-1462. doi: 10.1016/S0008-8846(99)00119-2

20. Wu, K.-R.; Chen, B.; Yao, W.; and Zhang, D., “Effect of Coarse Aggregate Type on Mechanical Properties of High-Performance Concrete,” Cement and Concrete Research, V. 31, No. 10, Oct. 2001, pp. 1421-1425. doi: 10.1016/S0008-8846(01)00588-9

21. Nadeau, J. C., “A Multiscale Model for Effective Moduli of Concrete Incorporating ITZ Water-Cement Ratio Gradients, Aggregate Size Distributions, and Entrapped Voids,” Cement and Concrete Research, V. 33, No. 1, Jan. 2003, pp. 103-113. doi: 10.1016/S0008-8846(02)00931-6

22. Al-Oraimi, S. K.; Taha, R.; and Hassan, H. F., “The Effect of the Mineralogy of Coarse Aggregate on the Mechanical Properties of High-Strength Concrete,” Construction and Building Materials, V. 20, No. 7, Sept. 2006, pp. 499-503. doi: 10.1016/j.conbuildmat.2004.12.005

23. Gidrão, G. M. S., “Propriedades Dinâmicas do Concreto e Relações com sua Microestrutura,” master’s dissertation, Polytechnic School of the University of São Paulo, SP, Brazil, 2015, 132 pp.

24. Wang, H., and Li, Q., “Prediction of Elastic Modulus and Poisson’s Ratio for Unsaturated Concrete,” International Journal of Solids and Structures, V. 44, No. 5, Mar. 2007, pp. 1370-1379. doi: 10.1016/j.ijsolstr.2006.06.028

25. Sáez del Bosque, I. F.; Zhu, W.; Howind, T.; Matías, A.; Sánchez de Rojas, M. I.; and Medina, C., “Properties of Interfacial Transition Zones (ITZs) in Concrete Containing Recycled Mixed Aggregate,” Cement and Concrete Composites, V. 81, Aug. 2017, pp. 25-34. doi: 10.1016/j.cemconcomp.2017.04.011

26. Jia, Z., Han, YZhang, Y., and Qiu, C., “Quantitative Characterization and Elastic Properties of Interfacial Transition Zone around Coarse Aggregate in Concrete,” Journal of Wuhan University of Technology-Materials Science Edition, V. 32, No. 4, Aug. 2017, pp. 838-844. doi: 10.1007/s11595-017-1677-8

27. Lutz, M. P.; Monteiro, P. J. M.; and Zimmerman, R. W., “Inhomogeneous Interfacial Transition Zone Model for the Bulk Modulus of Mortar,” Cement and Concrete Research, V. 27, No. 7, July 1997, pp. 1113-1122. doi: 10.1016/S0008-8846(97)00086-0

28. Vieira, G. L., “Influência da Microfissuração Causada por Carregamento Precoce nas Propriedades Mecânicas de Concretos Produzidos com Diferentes Tipos de Cimento,” PhD thesis, the Federal University of Rio Grande do Sul, Porto Alegre, RS, Brazil, 2008, 189 pp.

29. Ghebrab, T. T., and Soroushian, P., “Development of Structure-Property Relationships for Concrete,” Journal of Advanced Concrete Technology—Japan Concrete Institute, V. 9, No. 1, Feb. 2011, pp. 5-14.

30. Zhou, Y.; Gao, J.; Sun, Z.; and Qu, W., “A Fundamental Study on Compressive Strength, Static and Dynamic Elastic Moduli of Young Concrete,” Construction and Building Materials, V. 98, Nov. 2015, pp. 137-145. doi: 10.1016/j.conbuildmat.2015.08.110

31. Mehta, P. K., and Monteiro, P. J. M., Concreto: Microestrutura, Propriedades e Materiais, second edition, IBRACON, São Paulo, SP, Brazil, 2014, 751 pp.

32. Taylor, H. F. W., Cement Chemistry, second edition, Thomas Telford Ltd., London, UK, 1997, 459 pp.

33. Xie, Y.; Corr, D. J.; Jin, F.; Zhou, H.; and Shah, S. P., “Experimental Study of the Interfacial Transition Zone (ITZ) of Model Rock-Filled Concrete (RFC),” Cement and Concrete Composites, V. 55, Jan. 2015, pp. 223-231. doi: 10.1016/j.cemconcomp.2014.09.002

34. Kocáb, D.; Kucharczykova, B.; Misak, P.; Zitt, P.; and Kralikova, M., “Development of the Elastic Modulus of Concrete under Different Curing Conditions,” Procedia Engineering, V. 195, 2017, pp. 96-101. doi: 10.1016/j.proeng.2017.04.529

35. Prado, L. D. A., “Módulo de Deformação Estático do Concreto de Baixa e Alta Relação A/C Pelo Método Ultra-Sônico,” master’s dissertation, the Federal University of Goiás, GO, Brazil, 2006, 226 pp.

36. Barbosa, A. H.; Lopez-Yanez, P. A.; and Carneiro, A. M. P., “Contribuição à Obtenção do Módulo de Elasticidade do Concreto Utilizando Modelagem Micromecânica,” Revista IBRACON Structures and Materials Journal, V. 4, No. 5, Dec. 2011, pp. 845-862.

37. L’Hermite, R., Ao Pé do Muro, Concrebras sa, Taguatinga, FD, Brazil, 1970, 171 pp.

38. Kallel, H.; Carré, H.; La Borderie, C.; Masson, B.; and Tran, N. C., “Effect of Temperature and Moisture on the Instantaneous Behaviour of Concrete,” Cement and Concrete Composites, V. 80, July 2017, pp. 326-332. doi: 10.1016/j.cemconcomp.2017.03.021

39. ABNT NBR 12826:2014, “Cimento Portland e Outros Materiais em Pó—Determinação do Índice de Finura por Meio de Peneirador Aerodinâmico,” Associação Brasileira de Normas Técnicas, Rio de Janeiro, Brazil, 2014, 5 pp.

40. ABNT NBR 16606:2017, “Cimento Portland—Determinação da Pasta de Consistência Normal,” Associação Brasileira de Normas Técnicas, Rio de Janeiro, Brazil, 2017, 8 pp.

41. ABNT NBR 16607:2017, “Cimento Portland—Determinação dos Tempos de Pega,” Associação Brasileira de Normas Técnicas, Rio de Janeiro, Brazil, 2017, 4 pp.

42. ABNT NBR 16372:2015, “Cimento Portland e Outros Materiais em Pó—Determinação da Finura Pelo Método de Permeabilidade ao Ar (Método de Blaine),” Associação Brasileira de Normas Técnicas, Rio de Janeiro, Brazil, 2015, 11 pp.

43. ABNT NBR 16605:2017, “Cimento Portland e Outros Materiais em Pó—Determinação da Massa Específica,” Associação Brasileira de Normas Técnicas, Rio de Janeiro, Brazil, 2017, 4 pp.

44. ABNT NBR 7215:2019, “Cimento Portland—Determinação da Resistência à Compressão de Corpos de Prova Cilíndricos,” Associação Brasileira de Normas Técnicas, Rio de Janeiro, Brazil, 2019, 12 pp.

45. ABNT NBR NM 248:2003, “Agregados—Determinação da Composição Granulométrica,” Associação Brasileira de Normas Técnicas, Rio de Janeiro, Brazil, 2003, 6 pp.

46. ABNT NBR NM 45:2006, “Agregados—Determinação da Massa Unitária e do Volume de Vazios,” Associação Brasileira de Normas Técnicas, Rio de Janeiro, Brazil, 2006, 8 pp.

47. ABNT NBR NM 46:2003, “Agregados—Determinação do Material Fino que Passa Através da Peneira 75µm, por Lavagem,” Associação Brasileira de Normas Técnicas, Rio de Janeiro, Brazil, 2003, 6 pp.

48. ABNT NBR 10341:2006, “Agregado Graúdo para Concreto—Determinação do Módulo de Deformação Estático e do Diagrama Tensão-Deformação em Rocha Matriz—Método de Ensaio,” Associação Brasileira de Normas Técnicas, Rio de Janeiro, Brazil, 2006, 5 pp.

49. ABNT NBR 5738:2015, “Concreto—Procedimento para Moldagem e Cura de Corpos de Prova,” Associação Brasileira de Normas Técnicas, Rio de Janeiro, Brazil, 2015, 9 pp.

50. ABNT NBR 9479:2006, “Argamassa e Concreto—Câmaras Úmidas e Tanques para Cura de Corpos-de-Prova,” Associação Brasileira de Normas Técnicas, Rio de Janeiro, Brazil, 2006, 2 pp.

51. ABNT NBR 8522:2017, “Concreto—Determinação dos Módulos Estáticos de Elasticidade e de Deformação à Compressão,” Associação Brasileira de Normas Técnicas, Rio de Janeiro, Brazil, 2017, 20 pp.

52. ABNT NBR ISO 7500-1:2016, “Materiais Metálicos—Calibração e Verificação de Máquinas de Ensaio Estático Uniaxial—Parte 1: Máquinas de Ensaio de Tração/Compressão—Calibração e Verificação do Sistema de Medição da Força,” Associação Brasileira de Normas Técnicas, Rio de Janeiro, Brazil, 2016, 19 pp.

53. Abid, M.; Hou, X.; Zheng, W.; and Hussain, R. R., “High Temperature and Residual Properties of Reactive Powder Concrete—A Review,” Construction and Building Materials, V. 147, Aug. 2017, pp. 339-351. doi: 10.1016/j.conbuildmat.2017.04.083

54. Lenz, L. A., “Avaliação da Influência do Empacotamento do Esqueleto Granular no Módulo de Elasticidade de Concretos Convencionais,” Master’s dissertation, postgraduate program in civil engineering, the Federal University of Paraná, Curitiba, PR, Brazil, 2016, 158 pp.

55. Kummer, L. M., “Resistência à Compressão e Módulo de Elasticidade dos Concretos de Uma Central Dosadora de Concreto de Lajeado/RS,” the University of Taquari Valley (UNIVATES), Lajeado, RS, Brazil, 2016, 67 pp.

56. Santos, A. C.; Arruda, A. M.; Silva, T. J.; and Vitor, P. C. P., “Estudo Comparativo entre Valores Teóricos e Resultados Experimentais de Módulo de Elasticidade de Concretos Produzidos com Diferentes Tipos de Agregado Graúdo,” Ambiente Construído, V. 17, No. 3, 2017, pp. 281-294. doi: 10.1590/s1678-86212017000300176


ALSO AVAILABLE IN:

Electronic Materials Journal