Pumping of Flowable Concrete: Analytical Prediction and Experimental Validation

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Pumping of Flowable Concrete: Analytical Prediction and Experimental Validation

Author(s): Rami Khatib and Kamal H. Khayat

Publication: Materials Journal

Volume: 118

Issue: 5

Appears on pages(s): 3-16

Keywords: analytical model; lubricating layer; pressure loss; pumping; viscosity; yield stress

DOI: 10.14359/51732928

Date: 9/1/2021

Abstract:
An analytical model was established to predict the pumping pressure of flowable concrete as a function of flow rate, pipe diameter, and rheological properties of the concrete and the lubricating layer (LL). The flow behaviors of the different flow zones across the pipe section during pumping were analytically defined for Bingham materials. The prediction model was validated using a pumping circuit involving 14 high-strength flowable concrete mixtures with slump flow values of 500 to 765 mm. The rheological properties of the concrete and the yield stress, viscosity, and thickness of the LL (the latter determined through reverse regression analysis) were considered as input parameters in the prediction model involving 113 data points in the comparison. The analysis revealed that the thickness of the LL can vary between 2 and 5 mm, and that the predicted pressure loss agrees well with experimental measurements within the range of the tested mixtures.

Related References:

1. Kaplan, D., “Pumping of Concretes,” PhD dissertation, Laboratoire Central des Ponts et Chaussées, Paris, France, 2001, 225 pp.

2. Chapdelaine, F., “Étude fondamentale et pratique sur le pompage du béton,” Faculté des Études Supérieures de l’Université Laval, Université Laval, Québec City, QC, Canada, 2007, 154 pp.

3. Ngo, T. T., “Influence of Concrete Compositions on the Pumpability Parameters,” PhD dissertation, Université de Cergy-Pontoise, Cergy, France, 2009.

4. Feys, D., “Interactions between Rheological Properties and Pumping of Self-Compacting Concrete,” PhD dissertation, Ghent University, Ghent, Belgium, 2009, 398 pp.

5. Khatib, R., “Analysis and Prediction of Pumping Characteristics of High-Strength Self-Consolidating Concrete,” PhD dissertation, Université de Sherbrooke, Sherbrooke, QC, Canada, 2013, 276 pp.

6. Choi, M. S.; Kim, J. Y.; and Kim, J. K., “Prediction of Concrete Pumping Using Various Rheological Models,” International Journal of Concrete Structures and Materials, V. 8, No. 4, 2014, pp. 269-278. doi: 10.1007/s40069-014-0084-1

7. Le, H. D.; Kadri, E. H.; Aggoun, S.; Vierendeels, J.; Troch, P.; and De Schutter, G., “Effect of Lubrication Layer on Velocity Profile of Concrete in a Pumping Pipe,” Materials and Structures, V. 48, No. 12, 2015, pp. 3991-4003. doi: 10.1617/s11527-014-0458-5

8. Feys, D.; Khayat, K. H.; Perez-Schell, A.; and Khatib, R., “Development of a Tribometer to Characterize Lubrication Layer Properties of Self-Consolidating Concrete,” Cement and Concrete Composites, V. 54, 2014, pp. 40-52. doi: 10.1016/j.cemconcomp.2014.05.008

9. Feys, D.; Khayat, K. H.; and Khatib, R., “How do Concrete Rheology, Tribology, Flow Rate and Pipe Radius Influence Pumping Pressure?” Cement and Concrete Composites, V. 66, 2016, pp. 38-46. doi: 10.1016/j.cemconcomp.2015.11.002

10. Feys, D.; Khayat, K. H.; Perez-Schell, A.; and Khatib, R., “Prediction of Pumping Pressure by Means of New Tribometer for Highly-Workable Concrete,” Cement and Concrete Composites, V. 57, 2015, pp. 102-115. doi: 10.1016/j.cemconcomp.2014.12.007

11. Gray, J., “Laboratory Procedure for Comparing Pumpability of Concrete Mixtures,” The Sixty-Fifth Annual Meeting of the Society, National Crushed Stone Association, Washington, DC, June 24-29, 1962, pp. 964-971.

12. Parker, H. W.; Deere, D. U.; Peck, R. B.; Birkemoe, P. C.; and Semple, R. M., “Testing and Evaluation of Prototype Tunnel Support Systems,” Report No. FRA-ORDD 74-11, Federal Railroad Administration, Department of Transportation, Washington, DC, 1973, 338 pp.

13. Browne, R. D., and Bamforth, P. B., “Tests to Establish Concrete Pumpability,” ACI Journal Proceedings, V. 74, No. 5, May 1977, pp. 193-203.

14. Best, J. F., and Lane, R. O., “Testing for Optimum Pumpability of Concrete,” Concrete International, V. 2, No. 10, Oct. 1980, pp. 9-17.

15. Secrieru, E., “Pumping Behaviour of Modern Concretes - Characterisation and Prediction,” PhD dissertation, TU Dresden, Dresden, Germany, 2018, 169 pp.

16. Ingber, M. S.; Graham, A. L.; Mondy, L. A.; and Fang, Z., “An Improved Constitutive Model for Concentrated Suspensions Accounting for Shear-Induced Particle Migration Rate Dependence on Particle Radius,” International Journal of Multiphase Flow, V. 35, No. 3, 2009, pp. 270-276. doi: 10.1016/j.ijmultiphaseflow.2008.11.003

17. Phillips, R. J.; Armstrong, R. C.; Brown, R. A.; Graham, A. L.; and Abbott, J. R., “A Constitutive Equation for Concentrated Suspensions that Accounts for Shear-Induced Particle Migration,” Physics of Fluids A: Fluid Dynamics, V. 4, No. 1, 1992, pp. 30-40. doi: 10.1063/1.858498

18. Nott, P. R., and Brady, J. F., “Pressure-Driven Flow of Suspensions: Simulation and Theory,” Journal of Fluid Mechanics, V. 275, 1994, pp. 157-199. doi: 10.1017/S0022112094002326

19. Choi, M. S.; Roussel, N.; Kim, Y. J.; and Kim, J. K., “Lubrication Layer Properties During Concrete Pumping,” Cement and Concrete Research, V. 45, 2013, pp. 69-78. doi: 10.1016/j.cemconres.2012.11.001

20. Jo, S. D.; Park, C. K.; Jeong, J. H.; Lee, S. H.; and Kwon, S. H., “A Computational Approach to Estimating a Lubricating Layer in Concrete Pumping,” Computers, Materials and Continua, V. 27, No. 3, 2012, pp. 189-210.

21. Wallevik, J. E., “Minimizing End-Effects in the Coaxial Cylinders Viscometer: Viscoplastic Flow Inside the ConTec BML Viscometer 3,” Journal of Non-Newtonian Fluid Mechanics, V. 155, No. 3, 2008, pp. 116-123. doi: 10.1016/j.jnnfm.2008.05.006

22. Koehler, E. P.; Fowler, D. W.; Ferraris, C. F.; and Amziane, S., “A New, Portable Rheometer for Fresh Self-Consolidating Concrete, ” Workability of SCC: Roles of Its Constituents and Measurement Techniques, SP-233, American Concrete Institute, Farmington Hills, MI, 2006, pp. 97-116.

23. Ede, A. N., “The Resistance of Concrete Pumped Through Pipelines,” Magazine of Concrete Research, V. 9, No. 27, 1957, pp. 129-140. doi: 10.1680/macr.1957.9.27.129

24. Chailmo, T.; Touloupov, N.; and Markovskiy, M., “Peculiarities of Concrete Pumping,” Stroikniga, Minsk, Belarus, 1989. (in Russian)

25. Tanigawa, Y.; Mori, H.; and Noda, Y., “Theoretical Study on Pumping of Fresh Concrete,” Transaction of the Japan Concrete Institute, V. 13, 1991.

26. Alekseev, S. N., “On the Calculation of Resistance in Pipe of Concrete Pumps (“Mechanization of Construction” translated from Russian) (Translated as Library Communication No. 450),” Building Research Station, V. 9, No. 1, 1953, pp. 8-13.

27. Weber, R., The Transport of Concrete by Pipeline, Cement and Concrete Association, London, UK, 1968.

28. Morinaga, S., “Pumpability of Concrete and Pumping Pressure in Pipelines,” Proceedings of RILEM Seminar, Leeds, UK, V. 3, 1973, pp. 1-39.

29. Sakuta, M.; Kasanu, I.; Yamane, S.; and Sakamoto, A., “Pumpability of Fresh Concrete,” Takenaka Technical Research Laboratory, Tokyo, Japan, 1989.

30. Jacobsen, S.; Haugan, L.; Hammer, T. A.; and Kalogiannidis, E., “Flow Conditions of Fresh Mortar and Concrete in Different Pipes,” Cement and Concrete Research, V. 39, No. 11, 2009, pp. 997-1006. doi: 10.1016/j.cemconres.2009.07.005

31. Kwon, S. H.; Park, C. K.; Jeong, J. H.; Jo, S. D.; and Lee, S. H., “Prediction of Concrete Pumping: Part II—Analytical Prediction and Experimental Verification,” ACI Materials Journal, V. 110, No. 6, Nov.-Dec. 2013, pp. 657-668.

32. Salinas, A., and Feys, D., “Estimation of Lubrication Layer Thickness and Composition through Reverse Engineering of Interface Rheometry Tests,” Materials (Basel), V. 13, No. 8, 2020, p. 1799. doi: 10.3390/ma13081799

33. Ngo, T. T.; Kadri, E. H.; Bennacer, R.; and Cussigh, F., “Use of Tribometer to Estimate Interface Friction and Concrete Boundary Layer Composition During the Fluid Concrete Pumping,” Construction and Building Materials, V. 24, No. 7, 2010, pp. 1253-1261. doi: 10.1016/j.conbuildmat.2009.12.010

34. Roussel, N.; Lemaître, A.; Flatt, R. J.; and Coussot, P., “Steady State Flow of Cement Suspensions: A Micromechanical State of the Art,” Cement and Concrete Research, V. 40, No. 1, 2010, pp. 77-84. doi: 10.1016/j.cemconres.2009.08.026

35. Feys, D.; Verhoeven, R.; and De Schutter, G., “Evaluation of Time Independent Rheological Models Applicable to Fresh Self-Compacting Concrete,” Applied Rheology (Lappersdorf, Germany), V. 17, No. 5, 2007, pp. 1-10. doi: 10.1515/arh-2007-0018

36. Ngo, T.-T.; Kadri, E.-H.; Cussigh, F.; and Bennacer, R., “Relationships between Concrete Composition and Boundary Layer Composition to Optimise Concrete Pumpability,” European Journal of Environmental and Civil Engineering, V. 16, No. 2, 2012, pp. 157-177. doi: 10.1080/19648189.2012.666910

37. Feys, D., and Khayat, K. H., “Comparing Rheological Properties of SCC Obtained with the ConTec and ICAR Rheometers,” Proceedings of the Fifth North American Conference on the Design and Use of Self-Consolidating Concrete, Chicago, IL, May 12-15, 2013.

38. Zhu, H.; Martys, N. S.; Ferraris, C. F.; and Kee, D. D., “A Numerical Study of the Flow of Bingham-Like Fluids in Two-Dimensional Vane and Cylinder Rheometers Using a Smoothed Particle Hydrodynamics (SPH) Based Method,” Journal of Non-Newtonian Fluid Mechanics, V. 165, No. 7-8, 2010, pp. 362-375. doi: 10.1016/j.jnnfm.2010.01.012

39. Wallevik, J. E., “Rheology of Particle Suspensions: Fresh Concrete, Mortar and Cement Paste with Various Types of Lignosulfonates,” PhD dissertation, Norwegian University of Science and Technology, Trondheim, Norway, 2003, 413 pp.

40. Reiner, M., Deformation and Flow: An Elementary Introduction to Theoretical Rheology, H.K. Lewis & Co. Ltd., London, UK, 1949, 348 pp.

41. Nehdi, M., and Rahman, M.-A., “Effect of Geometry and Surface Friction of Test Accessory on Oscillatory Rheological Properties of Cement Pastes,” ACI Materials Journal, V. 101, No. 5, Sept.-Oct. 2004, pp. 416-424.

42. Kim, H.-R.; Cho, H.-K.; Kim, J.-C.; and Lee, K.-C., “Prediction of Pumping Friction Resistance Coefficient in Pipe Influenced by Concrete Rheology Properties,” Journal of the Korea Institute of Building Construction, V. 14, No. 2, 2014, pp. 118-126. doi: 10.5345/JKIBC.2014.14.2.118