ACI PRC-214.4-21: Obtaining Cores and Interpreting Core Compressive Strength Results—Guide

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: ACI PRC-214.4-21: Obtaining Cores and Interpreting Core Compressive Strength Results—Guide

Author(s): ACI Committee 214

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 20

Keywords: compressive strength; core; hardened concrete; sampling; test.

DOI:

Date: 6/7/2021

Abstract:
Core testing is the most direct method to determine the compressive strength of concrete in a structure. Generally, cores may be obtained to assess whether concrete in a new structure complies with strength-based acceptance criteria or to evaluate structural capacity of an existing structure based on in-place concrete strength. In either case, the process of obtaining core specimens and interpreting strength test results is often confounded by various factors affecting in-place concrete strength or the measured strength of a test specimen. The scatter in strength test data, which is unavoidable given the inherent randomness of in-place concrete strengths and the uncertainty attributable to preparation and testing of the specimen, may further complicate compliance and evaluation decisions. This guide summarizes practices for obtaining cores and interpreting core compressive strength test results. Factors that affect in-place concrete strength are reviewed so sampling locations that are consistent with objectives of the investigation can be selected. Strength correction factors are presented for converting measured strength of nonstandard core-test specimens to strength of equivalent specimens with standard diameters, length-to-diameter ratios, and moisture conditioning that have been derived using data for normalweight concrete with strengths between 2000 and 13,400 psi (14 and 92 MPa). This guide also provides direction for checking strength compliance of concrete in a structure under construction and methods for determining equivalent specified strength to assess existing structure capacity.