Influence of Shear Span-to-Effective Depth Ratio on Behavior of High-Strength Reinforced Concrete Beams

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Influence of Shear Span-to-Effective Depth Ratio on Behavior of High-Strength Reinforced Concrete Beams

Author(s): Olaniyi Arowojolu, Ahmed Ibrahim, Abdullah Almakrab, Nicholas Saras, Richard Nielsen

Publication: IJCSM

Volume: 15

Issue:

Appears on pages(s):

Keywords: high-strength concrete, shear span-to-effective depth ratio, aggregate interlock, shear strength, moment capacity

DOI: 10.1186/s40069-020-00444-7

Date: 5/31/2021

Abstract:
The shear span-to-effective depth ratio (a/d) is one of the factors governing the shear behavior of reinforced concrete (RC) beams, with or without shear reinforcement. In high-strength concrete (HSC), cracks may propagate between the aggregate particles and result in a brittle failure which is against the philosophy of most design guidelines. The experimental results of six HSC beams, with and without shear reinforcement, tested under four-point bending with a/d ranged from 2.0 to 3.0 are presented and compared with different model equations in design codes. The a/d ratio has higher influence on the shear strength of reinforced HSC beams without shear reinforcement than beams with shear reinforcement. Most of the shear resistance prediction models underestimate the concrete shear strength of the beams but overpredict shear resistance of beams with shear reinforcement. However, the fib Model code 2010 accurately predicted the shear resistance for all the beams within an appropriate level of approximation (LoA).